Polymer Property : Izod Impact, Notched = 0.52 J/cm Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Izod Impact, Notched 0.52 J/cm
0.97 ft-lb/in
ASTM D256
Sumitomo Bakelite North America 52-40-40-P Long-Glass Reinforced Diallyl Phthalate
Ortho Resin Isomer (DAP). Used for critical, high-performance military and commercial electrical components where long-term reliability is demanded.Meets the requirements of ASTM D5948 Type GDI-30F..