Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Izod Impact, Notched = 0.525 ft-lb/in Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Izod Impact, Notched 0.280 J/cm
0.525 ft-lb/in
ASTM D256
North Wood Plastics HDPE with 20% Wood Fiber
Data provided by North Wood Plastics, Inc.
Izod Impact, Notched 0.280 J/cm
0.525 ft-lb/in
ASTM D256
SABIC M300054 High Density Polyethylene for Injection Molding
Product Description: M300054 is a high density polyethylene grade with a narrow molecular weight distribution suitable for injection molding applications. It has been designed to provide good flow..
Izod Impact, Notched 0.280 - 1.80 J/cm
0.525 - 3.37 ft-lb/in
Average value: 0.941 J/cm Grade Count:45
Overview of materials for Nylon 6, Glass Fiber Filled, Flame Retardant
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 6, Glass Fiber Filled, Flame Retardant". Each property range of values reported is minimum and max..
Izod Impact, Notched 0.280 - 0.700 J/cm

@Temperature -40.0 - -20.0 °C
0.525 - 1.31 ft-lb/in

@Temperature -40.0 - -4.00 °F
Average value: 0.321 J/cm Grade Count:4
Overview of materials for Nylon 6, Glass/Mineral Reinforced
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 6, Glass/Mineral Reinforced". Each property range of values reported is minimum and maximum values..
Izod Impact, Notched 0.280 J/cm
0.525 ft-lb/in
ASTM D256
SABIC Innovative Plastics LNP LUBRICOMP IBP34 PA6.12
LNP* LUBRICOMP* IBP34 is a compound based on Nylon 6/12 containing 20% Glass Bead, 15% PTFE/Silicone. Added features include: Wear Resistant.
Izod Impact, Notched 0.280 J/cm

@Temperature 23.0 °C
0.525 ft-lb/in

@Temperature 73.4 °F
ASTM D 256
SABIC Innovative Plastics Valox® 175 PBT
Unreinforced, neat PBT resin for compounding only. Natural Color Only, Not intended for injection molding.This data was supplied by SABIC-IP for the Americas region.
Izod Impact, Notched 0.280 J/cm
0.525 ft-lb/in
ASTM D256
SABIC Innovative Plastics Valox® 175 PBT (Europe-Africa-Middle East)
Unreinforced, neat PBT resin for compounding only. Natural Color Only, Not intended for injection molding.
Izod Impact, Notched 0.280 J/cm
0.525 ft-lb/in
ASTM D256
SABIC Innovative Plastics Valox® 176 PBT
Unreinforced, neat PBT resin for fibers. Natural Color Only, Not intended for injection molding.
Izod Impact, Notched 0.280 J/cm
0.525 ft-lb/in
ASTM D256
SABIC Innovative Plastics Valox® 176HP PBT
Unreinforced, FDA compliant neat PBT resin for fibers. Natural Color Only, Not intended for injection molding.
Izod Impact, Notched 0.280 J/cm
0.525 ft-lb/in
ASTM D256
SABIC Innovative Plastics Valox® IQ3001 PBT (Asia Pacific)
Valox IQ3001 is an unfilled environmentally responsible iQ-PBT resin modified with elastomer. Targeted for flexible hinge applications.
Izod Impact, Notched 0.280 J/cm
0.525 ft-lb/in
ASTM D256
SABIC Innovative Plastics Valox® IQ3001 PBT (Europe-Africa-Middle East)
Valox IQ3001 is an unfilled environmentally responsible iQ-PBT resin modified with elastomer. Targeted for flexible hinge applications.
Izod Impact, Notched 0.280 J/cm
0.525 ft-lb/in
ASTM D256
Sumitomo Bakelite Durez® 31735 Phenolic, Compression Grade
Durez 31735 is a special purpose phenolic molding compound developed for automotive and industrial pulleys. This material is designed to optimize pulley performance relating to belt life, dimension..
Izod Impact, Notched 0.280 J/cm
0.525 ft-lb/in
ASTM D256
SABIC Innovative Plastics Valox® IQ3001 PBT
Valox IQ3001 is an unfilled environmentally responsible iQ-PBT resin modified with elastomer. Targeted for flexible hinge applications.
Izod Impact, Notched 0.280 J/cm
0.525 ft-lb/in
ASTM D256
SABIC Innovative Plastics LNP THERMOCOMP M7002XXH PP
LNP* THERMOCOMP* M7002XXH is a compound based on Polypropylene resin containing proprietary antimicrobial additives. Designed for touch surfaces in healthcare applications. Added features include:..
Izod Impact, Notched 0.280 J/cm
0.525 ft-lb/in
ASTM D256
SABIC Innovative Plastics LNP THERMOCOMP RB004 PA 66
LNP* THERMOCOMP* RB004 is a compound based on Nylon 66 containing Glass Beads.
Izod Impact, Notched 0.280 J/cm
0.525 ft-lb/in
ASTM D256
Goodfellow TPX® MX002O Polymethylpentene
This grade is highly recommended for injection molding, film and mandrel extrusion; also for fiber extrusion and blow molding.TPX® is semi-crystalline, transparent, very light and - for a polyolefi..
Izod Impact, Notched 0.280 J/cm
0.525 ft-lb/in
ASTM D256
Cresset Powers Cress-Alon™ NF3020 2% Nano Clay Loaded, 3.0 r.v. Film Grade Nylon 6, 50% RH
Low density, high rigidity, high heat distortion temperature, high retention of mechanical properties under humid conditions, flame retardant, recyclable and environmentally friendly, less glass fib..
Izod Impact, Notched 0.280 J/cm
0.525 ft-lb/in
ASTM D-256
Axiall ProTherm® 4303 Rigid PVC, Extrusion
Georgia Gulf 4303 is a CPVC powder formulation designed for the processing of pipe products with an O.D. range of 1/2" to 8 inches requiring high heat deflection temperatures. Processing and stabil..
Izod Impact, Notched 0.280 J/cm
0.525 ft-lb/in
ASTM-D256
Braskem IB58 HDPE Injection Molding Polyethylene Copolymer
IB58 is a high-density polyethylene, narrow molecular weight butene-1 copolymer produced by the solution process for injection molding applications. It offers good processability combined with good ..
Izod Impact, Notched 0.280 - 0.420 J/cm
0.525 - 0.787 ft-lb/in
IS 13411-1992
Amity Thermosets ATM 122 Phenolic Molding Organic Filler, Compression Molded
Characteristics:Good mouldability Good mechanical strengthGood electrical insulationGood surface finishMedium thermal stabilityColor- black, brownSoft/medium flow Applications: Electric control pane..
Izod Impact, Notched 0.280 - 0.420 J/cm
0.525 - 0.787 ft-lb/in
IS 13411-1992
Amity Thermosets ATM 144 Phenolic Molding Organic Filler, Compression Molded
Characteristics:Good mouldability Good mechanical strengthGood electrical insulationGood surface finishMedium thermal stabilityColor- black, brownSoft/medium flow Applications: Electric control pane..
Izod Impact, Notched 0.280 J/cm

@Thickness 3.20 mm
0.525 ft-lb/in

@Thickness 0.126 in
ASTM D256
Beijing Chemical Industry KAIFA® HN301-G30 PA6 Resin
30% glass fiber reinforced, flame retardantInformation provided by Beijing Chemical Industry Research Institute (Group)
Izod Impact, Notched 0.280 J/cm
0.525 ft-lb/in
ASTM-D256
Braskem IG58 HDPE Injection Molding Polyethylene Copolymer
IG58 is a high-density polyethylene, narrow molecular weight butene-1 copolymer produced by the solution process for injection molding applications. It offers high stiffness, impact strength and out..
Izod Impact, Notched 0.280 - 0.370 J/cm
0.525 - 0.693 ft-lb/in
IS 13411-1992
Amity Thermosets ATG 112 Phenolic Molding Organic Filler, Compression Molded
Characteristics:Medium mechanical strength Medium electrical insulationGeneral purposeColor- Black, BrownSoft/medium flow Applications: Electrical accessories & fittings ( medium quality ) Domestic ..
Izod Impact, Notched 0.280 J/cm

@Thickness 3.20 mm
0.525 ft-lb/in

@Thickness 0.126 in
ASTM D256
Beijing Chemical Industry KAIFA® 302-G0 PBT Resin
Flame retardant, low bleedingInformation provided by Beijing Chemical Industry Research Institute (Group)
Copyright © lookpolymers.com All Rights Reserved