Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Izod Impact, Notched | 0.540 J/cm | 1.01 ft-lb/in | ASTM D256 |
NCMT NanoPAC™ G3000 High Performance Polypropylene Nanocomposite Applications: Automobile Construction MaterialInformation provided by Nano Composite Materials Technology Limited |
|||
Izod Impact, Notched | 0.540 J/cm | 1.01 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics LNP FARADEX NX96302 PC+ABS LNP* FARADEX* NX96302 is a compound based on PC+ABS resin containing Stainless Steel Fibers. |
|||
Izod Impact, Notched | 0.540 - 1.90 J/cm @Temperature -40.0 - -20.0 °C |
1.01 - 3.56 ft-lb/in @Temperature -40.0 - -4.00 °F |
Average value: 1.21 J/cm Grade Count:12 |
Overview of materials for Polyphenylene Ether, Molded This property data is a summary of similar materials in the MatWeb database for the category "Polyphenylene Ether, Molded". Each property range of values reported is minimum and maximum values of ap.. |
|||
Izod Impact, Notched | 0.540 J/cm @Temperature -30.0 °C |
1.01 ft-lb/in @Temperature -22.0 °F |
|
Asahi Kasei Tenac®-C 4510 Acetal Copolymer, General Purpose
(discontinued **) General-purpose grade, characterized by balanced flowability and mechanical properties.Applications: Gears, cams, hose joints, clips, switches, mechanical parts of audio and video equipment.This pro.. |
|||
Izod Impact, Notched | 0.540 J/cm | 1.01 ft-lb/in | ASTM D256 |
Firestone C200-001 Nylon 6 Natural color. Not heat stabilized, modified, or lubricated. Chip size is 2 x 3.5 mm.Information provided by Firestone |
|||
Izod Impact, Notched | 0.540 J/cm | 1.01 ft-lb/in | ASTM D256 |
Firestone CL200-001 Nylon 6 Natural color. Not heat stabilized or modified. Lubricated. Chip size is 2 x 3.5 mm.Information provided by Firestone |
|||
Izod Impact, Notched | 0.540 J/cm | 1.01 ft-lb/in | ASTM D256 |
LG Chemical HI855HS PMMA, Impact Resistant Grade Molding granule designed for greater impact strength combined with the outstanding properties of conventional acrylic materialsFeatures: Excellent transparency and eleganceWeather resistance and che.. |
|||
Izod Impact, Notched | 0.540 J/cm | 1.01 ft-lb/in | ASTM D256 |
Kolon KOCETAL® LW301 Wear Modified Acetal Resin Special polymer added, improved wear property. Applications: Products for low noise and precision gear. Information provided by API-Kolon. |
|||
Izod Impact, Notched | 0.540 J/cm | 1.01 ft-lb/in | ASTM D256 |
Kolon KOPA® KN333HB40HFBL Hybrid Nylon 66 High flow, dimensionally stableApplications Fans & ShroudsInformation provided by API-Kolon. |
|||
Izod Impact, Notched | 0.540 J/cm | 1.01 ft-lb/in | ASTM D256 |
Kolon SPESIN® KP515FLBL High Impact PBT Alloy Resin High elastic, whether resistantApplications: WipersInformation provided by API-Kolon. |
|||
Izod Impact, Notched | >= 0.540 J/cm | >= 1.01 ft-lb/in | Reversed Notch (Method E); ASTM D 256 |
Karina E 854-35/1-A-ERYB Ivory PVC Compound Heavy metal free PVC compound recommended for extrusion of furniture profiles.Information provided by Karina Indústria e Comércio de Plásticos Ltda. |
|||
Izod Impact, Notched | >= 0.540 J/cm | >= 1.01 ft-lb/in | Reversed Notch (Method E); ASTM D 256 |
Karina E 854-35/1-Y-ERYB Ivory PVC Compound Information provided by Karina Indústria e Comércio de Plásticos Ltda. |
|||
Izod Impact, Notched | 0.540 J/cm | 1.01 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics LNP LUBRICOMP KAL22 Acetal Copolymer LNP* LUBRICOMP* KAL22 is a compound based on Acetal Copolymer resin containing 10% PTFE, 10% Aramid Fiber. Added feature of this material is: Wear Resistant. |
|||
Izod Impact, Notched | 0.540 J/cm | 1.01 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics LNP STAT-KON DX05301C PC LNP* STAT-KON* DX05301C is a compound based on Polycarbonate containing Proprietary Filler(s). Added features of this material include: Clean Compounding System, Electrically Conductive, Low Ionic.. |
|||
Izod Impact, Notched | 0.540 J/cm | 1.01 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics LNP STAT-KON DX05301C PC (Asia Pacific) Low Ionic, Low Outgassing, Low LPC and ESD safe Polycarbonate compound suitable for Semiconductor and Hard Disk Drive (HDD) application.Added features of this material include: Clean Compounding Sys.. |
|||
Izod Impact, Notched | 0.540 J/cm | 1.01 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics NORYL PCN2615H PPE+PS (Asia Pacific) PPE+PS, Noryl, Glass Fiber, Mica, Flame Retardant, UL Grade, Non-Halogen Flame Retaardant, High Flow, |
|||
Izod Impact, Notched | 0.540 J/cm | 1.01 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics LNP LUBRICOMP KFI12 Acetal Copolymer LNP LUBRICOMP* KFI12 is a compound based on Acetal Copolymer resin containing 10% Glass Fiber, 2% Silicone. Added feature of this grade is: Wear Resistant. |
|||
Izod Impact, Notched | 0.540 J/cm | 1.01 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics LNP THERMOCOMP MF742XXH PP LNP* THERMOCOMP* MF742XXH is a compound based on Polypropylene resin containing Glass Fiber and proprietary antimicrobial additives. This product is best suited for touch surfaces in healthcare app.. |
|||
Izod Impact, Notched | 0.540 J/cm | 1.01 ft-lb/in | ASTM D256 |
UBE UBESTA® 3020X15 Nylon 12 Thermister Description: UBESTA Nylon 12 ThermisterInformation provided by UBE. |
|||
Izod Impact, Notched | 0.540 J/cm | 1.01 ft-lb/in | ASTM D256 |
UBE UBESTA® 3020X8 Nylon 12 Thermister Description: UBESTA Nylon 12 ThermisterInformation provided by UBE. |
|||
Izod Impact, Notched | 0.540 J/cm @Thickness 3.17 mm |
1.01 ft-lb/in @Thickness 0.125 in |
ASTM D256 |
Unitika AXF-1500-05 Dry Characteristics: Lubricant grade of AX1500, excellent in heat and chemical resistancesInformation provided by Unitika Ltd. |
|||
Izod Impact, Notched | 0.540 J/cm @Thickness 3.17 mm |
1.01 ft-lb/in @Thickness 0.125 in |
ASTM D256 |
Entec Hypro™ PPC-T40 Copolymer Polypropylene, 40% Talc Reinforced Information provided by Entec |
|||
Izod Impact, Notched | 0.540 J/cm | 1.01 ft-lb/in | ASTM D256 |
Ashley Polymers Ashlene® P105 PBT Polyester A general purpose polyester with low shrinkage and good flow.Data provided by the manufacturer |
|||
Izod Impact, Notched | 0.540 J/cm | 1.01 ft-lb/in | Dry; ASTM D256 |
Asahi Kasei Leona® 9400S Nylon 66 Excellent impact resistance. Suitable for thick-wall parts.Applications:Railroad tie insulatorsInformation provided by Asahi Kasei |
|||
Izod Impact, Notched | 0.540 J/cm | 1.01 ft-lb/in | ASTM D256 |
Ashley Polymers Ashlene® 195-N2 Acetal A general purpose, medium viscosity natural.Data provided by the manufacturer |
|||
Izod Impact, Notched | 0.540 J/cm @Temperature -40.0 °C |
1.01 ft-lb/in @Temperature -40.0 °F |
ASTM D256 |
Ashley Polymers Ashlene® 279 PPO Alloy A general purpose, paintable injection molding grade with high chemical resistance and mechanical performance. Good heat resistance with dimensional stability in dark gray or black only.Data provid.. |
|||
Izod Impact, Notched | 0.540 J/cm | 1.01 ft-lb/in | ASTM D256 |
Ashley Polymers Ashlene® R195B Acetal A general purpose, low viscosity with excellent toughness, strength, stiffness, lubricity in black. Available in UV stabilized grades: R195-B2 (good weatherability); R195-HB2 (maximum weatherabili.. |
|||
Izod Impact, Notched | 0.540 J/cm | 1.01 ft-lb/in | ASTM D256 |
ALM PA 601-CF Filled Nylon 12 Prototyping Polymer Carbon fiber filled nylon 12 easy to process, strong light weight filled material.Low density, good dimensional stability while maintaining excellent mechanical properties.Fibers have been optimized.. |
|||
Izod Impact, Notched | 0.540 J/cm | 1.01 ft-lb/in | ASTM D256 |
Plenco 50335 PET, Pellet, Injection Molded, Natural Color
(discontinued **) PLENCO 50335 is an engineering grade glass reinforced polyethylene terephthalate resin designed for excellent dimensional stability. It is UL listed and available in white, natural, and black.Inform.. |