Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Izod Impact, Notched | 0.750 J/cm @Thickness 3.18 mm, Temperature 23.0 °C |
1.41 ft-lb/in @Thickness 0.125 in, Temperature 73.4 °F |
Injection Molded; ASTM D256A |
PolyOne Maxxam™ PPC-40C Nat Polypropylene Copolymer (PP Copolymer) PolyOne's Maxxam™ family of polypropylene- and polyethylene-based products covers a wide range of applications, markets and performance requirements. Standard grades are compounded with calcium car.. |
|||
Izod Impact, Notched | 0.750 J/cm | 1.41 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics Cycoloy® CX7010 PC+ABS (Europe-Africa-Middle East) Cycoloy* CX7010 resin is an injection moldable PC/ABS blend. It contains non-brominated and non-chlorinated flame retardant systems to meet UL-94 V0. Excellent flow combined with good balance of pro.. |
|||
Izod Impact, Notched | 0.750 J/cm | 1.41 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics EXTEM UH1006 TPI Blend High Heat Amorphous TPI Blend, Excellent Chemical Resistance, High Continuous Use Temperature (CUT), Best-in-class FR, OSU and LOI. Material is UL-listed. This material is RoHS compliant and also ha.. |
|||
Izod Impact, Notched | >= 0.750 J/cm @Temperature 23.0 °C |
>= 1.41 ft-lb/in @Temperature 73.4 °F |
ASTM D256 |
NIZHNEKAMSKNEFTEKHIM PP 7445L (EPC57MA) Propylene and Ethylene Block Polymer Product obtained by copolymerization of propylene with ethylene in presence of complex metalorganic catalysts. It incorporates increased long-term thermal stability, thermal-oxidative degradation r.. |
|||
Izod Impact, Notched | 0.750 J/cm @Thickness 3.18 mm, Temperature 23.0 °C |
1.41 ft-lb/in @Thickness 0.125 in, Temperature 73.4 °F |
Injection Molded; ASTM D256A |
PolyOne Edgetek® X TR2-20TA/000 NATURAL Copolyester The Edgetek™ engineering thermoplastics compounds made with Eastman Tritan™ copolyester offer a wide range of performance and properties with the addition of reinforcing additives. By utilizing Ea.. |
|||
Izod Impact, Notched | 0.750 J/cm @Temperature -30.0 °C |
1.41 ft-lb/in @Temperature -22.0 °F |
ASTM D256 |
SABIC Innovative Plastics Lexan® XHT2143 PC Copolymer (Europe-Africa-Middle East) XHT2143 is a high flow, UV stabilized, high heat polycarbonate copolymer with an HDT/Af of 142 C. It is available in a range of opaque and limited transparent colors. |
|||
Izod Impact, Notched | 0.750 J/cm | 1.41 ft-lb/in | ASTM D256 |
Plenco 50125 PET, Pellet, Injection Molded, White
(discontinued **) PLENCO 50125 is an engineering grade glass reinforced UL flame rated polyethylene terephthalate resin designed for excellent dimensional stability. It is UL listed and available in white only.Inform.. |
|||
Izod Impact, Notched | 0.750 J/cm | 1.41 ft-lb/in | ASTM D256 |
Solvay Specialty Polymers AvaSpire® AV-848 Polyaryletherketone (PAEK)
(Unverified Data**) AvaSpire® AV-848 is a high-temperature, polyaryletherketone (PAEK) that offers several key performance advantages over comparable grades of PEEK above 150°C, including better dimensional stability.. |
|||
Izod Impact, Notched | 0.750 J/cm | 1.41 ft-lb/in | ASTM D256 |
Ineos Nova 271 High Performance Styrenic Enhanced Polystyrene
(discontinued **) Excellent balance of stiffness, heat resistance, and impact properties, Custom colorsApplications: Injection molding and extrusion, Applications requiring strength and durability where custom colori.. |
|||
Izod Impact, Notched | 0.750 J/cm @Temperature -30.0 °C |
1.41 ft-lb/in @Temperature -22.0 °F |
ASTM D256 |
SABIC Innovative Plastics Lexan® XHT2146 PC Copolymer (Asia Pacific) XHT2146 resin is a high flow, high heat polycarbonate copolymer with improved release performance compared to Lexan* XHT2141 resin. It is available in a range of opaque and limited transparent colo.. |
|||
Izod Impact, Notched | 0.750 J/cm | 1.41 ft-lb/in | ASTM D256 |
Solvay Specialty Polymers Ryton® R-4-200BL Polyphenylene Sulfide Compound
(Unverified Data**) Black Polyphenylene Sulfide CompoundRyton® R-4-200BL is an advanced 40% fiberglass reinforced polyphenylene sulfide compound developed to provide high strength, fast cycles, and low maintenance mol.. |
|||
Izod Impact, Notched | 0.750 J/cm @Thickness 3.20 mm, Temperature 23.0 °C |
1.41 ft-lb/in @Thickness 0.126 in, Temperature 73.4 °F |
ASTM D256 |
Kingfa JH-R2G10 P60 10% Glass Fiber Reinforced PC/ABS Alloy Features:UL HB @ 1.6-3.2mmExcellent balance propertiesHigh stiffnessGood size stabilityGood surface adhesionExcellent processing properties, large partsApplications:Injection moldingAutomobile instr.. |
|||
Izod Impact, Notched | 0.750 J/cm @Temperature 23.0 °C |
1.41 ft-lb/in @Temperature 73.4 °F |
ASTM D256 |
Lavergne VYPET VNT 835 PET 35% Glass-Mineral Reinforced Vypet VNT 835 is a 35% mineral and fiberglass reinforced PET injection molding compound designed for structural applications.Features: High temperature performance; Low warp; Excellent dimensional s.. |
|||
Izod Impact, Notched | 0.750 J/cm @Thickness 3.20 mm, Temperature 23.0 °C |
1.41 ft-lb/in @Thickness 0.126 in, Temperature 73.4 °F |
ASTM D256 |
Kingfa PBT-RG15 Flame Retardant, 15% Glass Fiber Reinforced PBT Features:Flame retardantHigh strengthHigh temperature propertiesOutstanding electrical propertiesGood heat resistanceApplications:Injection moldingConnectorsRelayBobbins, plugsE & E partsInformation.. |
|||
Izod Impact, Notched | 0.750 J/cm @Thickness 3.20 mm, Temperature 23.0 °C |
1.41 ft-lb/in @Thickness 0.126 in, Temperature 73.4 °F |
ASTM D256 |
Kingfa PET-G15 15% Glass Fiber Reinforced PET Features:High strengthGood heat resistanceApplications:Injection moldingApplication partsAuto partsInformation Provided by Kingfa Sci. & Tech. Co., Ltd. |
|||
Izod Impact, Notched | 0.750 J/cm @Temperature 23.0 °C |
1.41 ft-lb/in @Temperature 73.4 °F |
ASTM D 256 |
SABIC Innovative Plastics Ultem ATX202R PEI+PCE (Europe-Africa-Middle East) 20% Glass fiber filled, high flow Polyetherimide blend with internal mold release. ECO Conforming, UL94 V0 and 5VA listing.This data was supplied by SABIC-IP for the Europe-Africa-Middle East regio.. |
|||
Izod Impact, Notched | 0.750 J/cm @Thickness 3.18 mm |
1.41 ft-lb/in @Thickness 0.125 in |
ASTM D256 |
Solvay Specialty Polymers Ryton® BR111 Polyphenylene Sulfide (PPS), GlassMineral Filled Ryton® BR111 is a natural-colored glass fiber and mineral filled polyphenylene sulfide compound that provides enhanced mechanical strength with good electrical properties and outstanding chemical.. |
|||
Izod Impact, Notched | 0.750 J/cm @Temperature -30.0 °C |
1.41 ft-lb/in @Temperature -22.0 °F |
ASTM D256 |
SABIC Innovative Plastics Valox® IQ4860HR PBT Valox iQ* Resin iQ4860HR: Environmentally responsible iQ* PBT resin with 30% Glass reinforcement + UL94 V-0. Hydrolytically stable and impact modified. |
|||
Izod Impact, Notched | 0.750 J/cm | 1.41 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics LNP THERMOCOMP LC006EXQ PEEK LNP* THERMOCOMP* LC006EXQ is a compound based on Polyetheretherketone containing 30% Carbon Fiber. Added features of this material include: Electrically Conductive, Easy Molding. |
|||
Izod Impact, Notched | 0.750 J/cm @Temperature -30.0 °C |
1.41 ft-lb/in @Temperature -22.0 °F |
ASTM D256 |
SABIC Innovative Plastics NORYL NH8006 PPE+HIPS (Asia Pacific) Noryl* NH8006 resin is a 30% glass reinforced, modified PPE-PS blend. The material uses non-halogenated flame retardants to achieve a UL94 V0 flame rating (color specific) while offering an exceptio.. |
|||
Izod Impact, Notched | 0.750 J/cm @Temperature -30.0 °C |
1.41 ft-lb/in @Temperature -22.0 °F |
ASTM D256 |
SABIC Innovative Plastics NORYL PX1007 PPE+PS Noryl* PX1007 is an unfilled non-chlorinated, non-brominated flame retardant PPE/HIPS grade. |
|||
Izod Impact, Notched | 0.750 J/cm @Temperature -20.0 °C |
1.41 ft-lb/in @Temperature -4.00 °F |
ASTM D256 |
SABIC Innovative Plastics Valox® K3501 PBT (Europe-Africa-Middle East) Unfilled PBT, Hydrollytically Stable, Heat Stabilized, Impact Modified. A hydrollytically stable grade designed for improved performance under heat/humidity environments. Targeted at automotive unde.. |
|||
Izod Impact, Notched | 0.750 J/cm | 1.41 ft-lb/in | ASTM D256 |
A. Schulman PP 2175 Polypropylene High Flow Copolymer Polypropylene DescriptionPolypropylene PP 2175 is a high flow copolymer polypropylene.Information provided by A. Schulman. |
|||
Izod Impact, Notched | 0.750 J/cm | 1.41 ft-lb/in | ASTM D256 |
A. Schulman PP 2175 Polypropylene High Flow Copolymer Polypropylene DescriptionPolypropylene PP 2175 is a high flow copolymer polypropylene.Information provided by A. Schulman. |
|||
Izod Impact, Notched | 0.750 J/cm | 1.41 ft-lb/in | ASTM D256 |
A. Schulman PP 2175 Polypropylene High Flow Copolymer Polypropylene DescriptionPolypropylene PP 2175 is a high flow copolymer polypropylene.Information provided by A. Schulman. |
|||
Izod Impact, Notched | 0.750 J/cm | 1.41 ft-lb/in | ASTM D256 |
A. Schulman POLYFORT™ FPP 4529 Mineral Filled Copolymer Polypropylene DescriptionPolyfort® FPP 4528 is a mineral filled copolymer polypropylene for applications requiring good impact and increased stiffness with long term heat stability.Information provided by A. Sch.. |
|||
Izod Impact, Notched | 0.750 J/cm | 1.41 ft-lb/in | ASTM D256 |
A. Schulman POLYFORT™ PP 2175HU Toyota High Flow Copolymer Polypropylene DescriptionPolyfort® PP 2175HU Toyota is a high flow copolymer polypropylene.Information provided by A. Schulman. |
|||
Izod Impact, Notched | 0.750 J/cm | 1.41 ft-lb/in | ASTM D256 |
A. Schulman PP 2175 Polypropylene High Flow Copolymer Polypropylene DescriptionPolypropylene PP 2175 is a high flow copolymer polypropylene.Information provided by A. Schulman. |
|||
Izod Impact, Notched | 0.750 J/cm @Temperature -40.0 °C |
1.41 ft-lb/in @Temperature -40.0 °F |
ASTM D256 |
Eastman Eastar AN004 Natural PCTA Copolyester EASTAR AN004 Copolyester contains a mold release. It has excellent appearance and is nearly water-clear. Its most outstanding features are its chemical resistance and processing capabilities. Exp.. |
|||
Izod Impact, Notched | 0.750 J/cm @Thickness 3.20 mm, Temperature 23.0 °C |
1.41 ft-lb/in @Thickness 0.126 in, Temperature 73.4 °F |
ASTM D256, ISO 180/4a |
EPICHEM Epiter PBT GF 30 Polybutylene Terephthalate, 30% Glass Characteristics: 30% glass fibre filled |