Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Izod Impact, Notched | 0.780 J/cm | 1.46 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics Cycoloy® MC5220 PC+ABS (Asia Pacific) |
|||
Izod Impact, Notched | 0.780 J/cm | 1.46 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics Lexan® BFL2015 PC (Asia Pacific) Non-brominated, non-chlorinated flame retardant, glass reinforced PC. Opaque colors only |
|||
Izod Impact, Notched | 0.780 J/cm | 1.46 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics Lexan® BFL2015 PC (Europe-Africa-Middle East) Non-brominated, non-chlorinated flame retardant, glass reinforced PC. Opaque colors only |
|||
Izod Impact, Notched | 0.780 J/cm | 1.46 ft-lb/in | ASTM D256 |
Asahi Kasei Tenac® 5012 Acetal Homopolymer
(discontinued **) Standard-flow grade, with reduced stiffness and increased elongation through addition of special polymers.Applications: Clips, fasteners, press-fit parts.This product is not a part of the standard p.. |
|||
Izod Impact, Notched | 0.780 J/cm @Temperature 23.0 °C |
1.46 ft-lb/in @Temperature 73.4 °F |
ASTM D 256 |
SABIC Innovative Plastics Lexan® SP7604 PC (Asia Pacific) This data was supplied by SABIC-IP for the Asia Pacific region. |
|||
Izod Impact, Notched | 0.780 J/cm | 1.46 ft-lb/in | ASTM D256 |
Kolon KOPA® KN333HFBL General Purpose Nylon 66 Middle viscosity, flexibleApplications Band cables for vehiclesInformation provided by API-Kolon. |
|||
Izod Impact, Notched | 0.780 J/cm | 1.46 ft-lb/in | ASTM D256 |
Kolon SPESIN® KP212G30V0NB G/F Reinforced & Flame Retardant PBT Compound Resin Flame retardant, high flowApplications: A variety of cases and connectorsInformation provided by API-Kolon. Information provided by API-Kolon. |
|||
Izod Impact, Notched | 0.780 J/cm @Temperature 23.0 °C |
1.46 ft-lb/in @Temperature 73.4 °F |
V-Notched 1/8"; ASTM D256 |
Kotec Carbotex KG-15MRA Polycarbonate, 15% Glass Fiber Reinforced Features: Glass fiber 15% reinforced, Mold release, Translucent, Dimensional stability, Flame retardant, High rigidityApplications: OA equipment, Communications, Precision parts, Machineries, E & E .. |
|||
Izod Impact, Notched | 0.780 J/cm @Temperature 23.0 °C |
1.46 ft-lb/in @Temperature 73.4 °F |
V-Notched 1/8"; ASTM D256 |
Kotec Carbotex KG-20F10 Polycarbonate, Wear Resistant, 20% Glass Fiber Reinforced Features: Glass fiber 20% reinforced, Mold release, Translucent, Dimensional stability, Non-frictionApplications: OA equipment, Communications, Precision parts, Machineries, E & E partsInformation p.. |
|||
Izod Impact, Notched | 0.780 J/cm @Temperature 23.0 °C |
1.46 ft-lb/in @Temperature 73.4 °F |
V-Notched 1/8"; ASTM D256 |
Kotec Carbotex KGN-15MRA Polycarbonate, Flame Retardant, 15% Glass Fiber Reinforced Features: Glass fiber 15% reinforced, Mold release, Translucent, Dimensional stability, Flame retardant, High rigidityApplications: OA equipment, Communications, Precision parts, Machineries, E & E .. |
|||
Izod Impact, Notched | 0.780 J/cm @Temperature 23.0 °C |
1.46 ft-lb/in @Temperature 73.4 °F |
ASTM D 256 |
SABIC Innovative Plastics Valox® AB9530 ABS+PBT (Asia Pacific) This data was supplied by SABIC-IP for the Asia Pacific region. |
|||
Izod Impact, Notched | 0.780 J/cm @Temperature -30.0 °C |
1.46 ft-lb/in @Temperature -22.0 °F |
ASTM D256 |
SABIC Innovative Plastics Valox® IQ8280SF PBT+PET Valox iQ8280SF resin is an environmentally responsible, low carbon footprint, and sustainable resin. Valox iQ8280SF resin offer Super High Flow characteristics combined with high modulus and excell.. |
|||
Izod Impact, Notched | 0.780 J/cm @Temperature -30.0 °C |
1.46 ft-lb/in @Temperature -22.0 °F |
ASTM D256 |
SABIC Innovative Plastics Valox® IQ8280SF PBT+PET (Europe-Africa-Middle East) Valox iQ8280SF resin is an environmentally responsible, low carbon footprint, and sustainable resin. Valox iQ8280SF resin offer Super High Flow characteristics combined with high modulus and excell.. |
|||
Izod Impact, Notched | 0.780 J/cm | 1.46 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics LNP THERMOCOMP Lexan_SP7604 PC (Asia Pacific) |
|||
Izod Impact, Notched | 0.780 J/cm | 1.46 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics LNP THERMOCOMP RF007H PA 66 LNP* Thermocomp* RF007H is a compound based on Nylon 66 containing glass fiber. Added feature includes: Healthcare. |
|||
Izod Impact, Notched | 0.780 J/cm | 1.46 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics LNP THERMOCOMP RF007SXP PA 66 LNP* THERMOCOMP* RF007SXP is a compound based on Nylon 66 containing 35% Glass Fiber. Added feature of this material includes: Heat Stabilized. |
|||
Izod Impact, Notched | 0.780 J/cm | 1.46 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics LNP THERMOCOMP WF007 PBT LNP THERMOCOMP WF007 is a compound based on PBT resin containing 35% Glass Fiber. |
|||
Izod Impact, Notched | 0.780 J/cm @Temperature 23.0 °C |
1.46 ft-lb/in @Temperature 73.4 °F |
ASTM D 256 |
SABIC Innovative Plastics LNP Thermocomp WF007 PET/PBT LNP Thermocomp WF-1007 BK8-114 is a compound based on PET/PBT resin containing glass fiber.This data was supplied by SABIC-IP for the Americas region. |
|||
Izod Impact, Notched | 0.780 J/cm | 1.46 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics NORYL INT1001 PPE+HIPS (Asia Pacific) PPE / HIPS unfilled, high flow for auto interior |
|||
Izod Impact, Notched | 0.780 J/cm | 1.46 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics NORYL LEN2211 PPE+HIPS (Asia Pacific) PPE / HIPS unfilled, FR for LED application |
|||
Izod Impact, Notched | 0.780 J/cm | 1.46 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics ULTEM JD4901 PEI (Asia Pacific) |
|||
Izod Impact, Notched | 0.780 J/cm | 1.46 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics NORYL GTX APS430 PPE+PPS (Asia Pacific) PPE + PPS GF 30%, FR V-0 |
|||
Izod Impact, Notched | 0.780 J/cm @Thickness 3.17 mm |
1.46 ft-lb/in @Thickness 0.125 in |
ASTM D256 |
Unitika AX-1500 Dry AX series resins are opaque polymer alloys with a high deflection temperature under load without reinforcement and a chemical resistance as high as those of crystalline resins. They are excellent in.. |
|||
Izod Impact, Notched | 0.780 J/cm | 1.46 ft-lb/in | ASTM D256 |
Toyobo VYLOPET® EMC132-02 Injection Molding Polyester Resin, Flame Resistant Applications: Relay partsFeatures: Excellent arc resistanceFlame resistanceInformation provided by Toyobo. |
|||
Izod Impact, Notched | 0.780 J/cm | 1.46 ft-lb/in | ASTM D256 |
UBE UBESTA® 3035UF Rigid Piping Grade Nylon 12 Description: UBESTA contributes to the field of Utilities such as plastic pipe system evolutionary developed for gas industry. It is used for both burial and for rehabilitation of existing cast iron.. |
|||
Izod Impact, Notched | 0.780 J/cm @Thickness 3.17 mm |
1.46 ft-lb/in @Thickness 0.125 in |
ASTM D256 |
Unitika L-8005 Chemical resistance, and excellent lubricant propertyInformation provided by Unitika Ltd. |
|||
Izod Impact, Notched | 0.780 J/cm @Temperature 23.0 °C |
1.46 ft-lb/in @Temperature 73.4 °F |
ASTM D256 |
DuPont Performance Polymers VESPEL TP-8395 Polyimide DuPont Vespel TP-8395 parts are specified for high-temperature and high-wear applications. TP-8395 parts offer an excellent balance of mechanical and thermal properties for superior performance in a.. |
|||
Izod Impact, Notched | 0.780 J/cm | 1.46 ft-lb/in | ASTM D256 |
Asahi Kasei Tenac®-C EX351 Acetal Copolymer, Extrusion Grade
(discontinued **) High-viscosity grade amenable to extrusion.Applications: Extruded rods and sheets.This product is not a part of the standard product line dated 2003. |
|||
Izod Impact, Notched | 0.780 J/cm | 1.46 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics NORYL PX2060 PPE+PS (Asia Pacific) Noryl* PX2060 is an unfilled, injection moldable modified polyphenylene ether resin. Designed for good dimensional stability and high flow , this resin also uses non-chlorinated, non-brominated FR .. |
|||
Izod Impact, Notched | 0.780 J/cm | 1.46 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics NORYL PX2060 PPE+PS Noryl* PX2060 is an unfilled, injection moldable modified polyphenylene ether resin. Designed for good dimensional stability and high flow , this resin also uses non-chlorinated, non-brominated FR .. |