Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Izod Impact, Notched | 0.420 J/cm @Thickness 3.18 mm, Temperature 23.0 °C |
0.787 ft-lb/in @Thickness 0.125 in, Temperature 73.4 °F |
Injection Molded; ASTM D256A |
PolyOne Stat-Tech™ CTX-1125 Natural Acrylonitrile Butadiene Styrene (ABS) Stat-Tech™ Electrically Conductive Compounds are specifically engineered to provide anti-static, ESD and RFI/EMI shielding performance for critical electronic equipment applications. These compound.. |
|||
Izod Impact, Notched | 0.420 - 1.28 J/cm | 0.787 - 2.40 ft-lb/in | Average value: 0.679 J/cm Grade Count:53 |
Overview of materials for Acetal Homopolymer, Unreinforced This property data is a summary of similar materials in the MatWeb database for the category "Acetal Homopolymer, Unreinforced". Each property range of values reported is minimum and maximum values .. |
|||
Izod Impact, Notched | 0.420 J/cm @Thickness 4.00 mm, Temperature 23.0 °C |
0.787 ft-lb/in @Thickness 0.157 in, Temperature 73.4 °F |
ISO 180 |
Premix Thermoplastics PRE-ELEC® 12-033
(discontinued **) PRE-ELEC 12-033 is a conductive thermoplastic compound based on a polyacetal copolymer with 30% carbon fiber. PRE-ELEC 12-033 exhibits excellent mechanical properties and electrical conductivity. Te.. |
|||
Izod Impact, Notched | 0.420 - 0.480 J/cm | 0.787 - 0.899 ft-lb/in | ASTM D256 |
Huntsman RenShape® SL 7820 Stereolithography Plastic RenShape® SL 7820 stereolithography material is a white, low viscosity and stable liquid that produces strong black models and prototypes with good surface fi nish and detail, and ABS-like appear.. |
|||
Izod Impact, Notched | >= 0.420 J/cm | >= 0.787 ft-lb/in | Method A; ASTM D 256 |
Karina E 835-10/155-C-ERYB White PVC Compound Information provided by Karina Indústria e Comércio de Plásticos Ltda. |
|||
Izod Impact, Notched | 0.420 J/cm | 0.787 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics LNP LUBRICOMP ECL36 PEI LNP* Lubricomp* ECL36 is a compound based on Polyetherimide resin containing 30% Carbon Fiber, 15% PTFE. Added features of this material include: Internally Lubricated. |
|||
Izod Impact, Notched | 0.420 J/cm | 0.787 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics LNP LUBRICOMP IAL12 PA 6/12 (Asia Pacific) LNP* Lubricomp* IAL12 is a compound based on Nylon 6/12 resin containing PTFE, Aramid Fiber. Added features of this material include: Internally Lubricated. |
|||
Izod Impact, Notched | 0.420 J/cm | 0.787 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics LNP LUBRICOMP KFL32R Acetal Copolymer LNP LUBRICOMP* KFL32R is a compound based on Acetal Copolymer resin containing 10% Glass Fiber, 15% PTFE. Added feature of this material is: Easy Release, Wear Resistant. |
|||
Izod Impact, Notched | 0.420 J/cm @Temperature 23.0 °C |
0.787 ft-lb/in @Temperature 73.4 °F |
ASTM D 256 |
SABIC Innovative Plastics LNP Lubricomp KFL34 Acetal Copolymer (Asia Pacific) LNP* Lubricomp* KFL34 is a compound based on Acetal Copolymer resin containing Glass Fiber, PTFE. Added features of this material include: Internally Lubricated.This data was supplied by SABIC-IP f.. |
|||
Izod Impact, Notched | 0.420 J/cm | 0.787 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics LNP LUBRICOMP KL004L Acetal Copoly (Asia Pacific) LNP* Lubricomp* KL004L is a compound based on Acetal Copolymer resin containing PTFE. Added features of this material include: Internally Lubricated, Low Extractible. |
|||
Izod Impact, Notched | 0.420 J/cm | 0.787 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics LNP LUBRICOMP KL004U Acetal Copolymer LNP LUBRICOMP* KL004U is a compound based on Acetal Copolymer resin containing 20% PTFE. Added features of this material include: Wear Resistant, UV Stabilized. |
|||
Izod Impact, Notched | 0.420 J/cm | 0.787 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics LNP STAT-KON AX00756 ABS LNP STAT-KON* AX00756 is a compound based on ABS resin containing Stainless Steel. Added feature of this material is: Electrically Conductive. |
|||
Izod Impact, Notched | 0.420 J/cm | 0.787 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics Valox® 4521 PBT VALOX 4521 is a high flow, 20% glass reinforced flame retardant PBT injection moulding resin. Applications: electrical applications |
|||
Izod Impact, Notched | 0.420 J/cm @Temperature 23.0 °C |
0.787 ft-lb/in @Temperature 73.4 °F |
ASTM D 256 |
SABIC Innovative Plastics LNP Stat-kon EE006EM PEI (Asia Pacific) LNP* Stat-kon* EE006EM is a compound based on Polyetherimide resin containing Carbon Fiber. Added features of this material include: Electrically Conductive, Easy Molding.This data was supplied by .. |
|||
Izod Impact, Notched | 0.420 J/cm | 0.787 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics LNP STAT-KON REL42 PA 66 LNP* STAT-KON* REL42 is a compound based on Nylon 66 resin containing 20% PTFE, 10% Carbon Fiber. Added features of this material include: Electrically Conductive, Internally Lubricated. |
|||
Izod Impact, Notched | 0.420 J/cm @Temperature 23.0 °C |
0.787 ft-lb/in @Temperature 73.4 °F |
ASTM D 256 |
SABIC Innovative Plastics LNP Stat-kon RX89129 PA 66 LNP* Stat-Kon RX89129 is a compound based on Nylon 6,6. Fillers are proprietary.This data was supplied by SABIC-IP for the Americas region. |
|||
Izod Impact, Notched | 0.420 J/cm | 0.787 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics LNP THERMOCOMP DX07350 PC (Asia Pacific) Lexan *DX07350 resin is a glass filled, Non-brominated & Non-chlorinated flame retardant polycarbonate. High stiffness and good flow. |
|||
Izod Impact, Notched | 0.420 J/cm | 0.787 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics LNP THERMOCOMP EC006 PEI (Asia Pacific) LNP THERMOCOMP* EC006 is a compound based on Polyetherimide resin containing Carbon Fiber. Added features of this material include: Electrically Conductive. |
|||
Izod Impact, Notched | 0.420 J/cm | 0.787 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics LNP THERMOCOMP MX95319 PP LNP* THERMOCOMP* MX95319 is a compound based on Polypropylene resin containing Proprietary Filler(s). |
|||
Izod Impact, Notched | 0.420 J/cm | 0.787 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics LNP THERMOCOMP PH0460A PA 6 LNP* THERMOCOMP* PH0460A is a compound based on Nylon 6. Added feature of this material is: High Specific Gravity. |
|||
Izod Impact, Notched | 0.420 J/cm @Temperature 23.0 °C |
0.787 ft-lb/in @Temperature 73.4 °F |
ASTM D 256 |
SABIC Innovative Plastics LNP Thermocomp WC006 Polyester, TP LNP* Thermocomp* WC006 is a compound based on Polyester, TP resin containing Carbon Fiber.This data was supplied by SABIC-IP for the Americas region. |
|||
Izod Impact, Notched | 0.420 J/cm | 0.787 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics LNP STAT-KON KE002 ACETAL LNP* STAT-KON* KE002 is a compound based on Acetal resin containing 10% Carbon Fiber. Added feature of this material is: Electrically Conductive. |
|||
Izod Impact, Notched | 0.420 J/cm | 0.787 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics LNP THERMOCOMP AH0400A ABS LNP* THERMOCOMP* AH0400A is a compound based on ABS resin. Added feature of this material is: High Specific Gravity. |
|||
Izod Impact, Notched | 0.420 J/cm | 0.787 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics LNP THERMOCOMP PF001S PA 6 LNP* THERMOCOMP* PF001S is a compound based on Nylon 6 resin containing 5% Glass Fiber. Added features of this material include: Heat Stabilized. |
|||
Izod Impact, Notched | 0.420 J/cm | 0.787 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics LNP THERMOCOMP RX93402 PA 66 LNP THERMOCOMP* RX93402 is a compound based on Nylon 66 resin containing Glass Fiber. Added features of this material include: Flame Retardant. |
|||
Izod Impact, Notched | 0.420 J/cm | 0.787 ft-lb/in | ASTM D256 |
A. Schulman POLYFORT™ FPP 3715 Glass Filled Homopolymer Polypropylene DescriptionPolyfort® FPP 3715 is a 15% glass filled homopolymer polypropylene product. Information provided by A. Schulman. |
|||
Izod Impact, Notched | 0.420 J/cm | 0.787 ft-lb/in | ASTM D256 |
A. Schulman POLYFORT™ FPP 3715 Glass Filled Homopolymer Polypropylene DescriptionPolyfort® FPP 3715 is a 15% glass filled homopolymer polypropylene product. Information provided by A. Schulman. |
|||
Izod Impact, Notched | 0.420 J/cm | 0.787 ft-lb/in | ASTM D256 |
A. Schulman POLYFORT™ FPP 3715 Glass Filled Homopolymer Polypropylene DescriptionPolyfort® FPP 3715 is a 15% glass filled homopolymer polypropylene product. Information provided by A. Schulman. |
|||
Izod Impact, Notched | 0.420 J/cm | 0.787 ft-lb/in | ASTM D256 |
ALM PA 614-GS Filled Nylon 12 Prototyping Polymer 40% glass sphere filled material for improved dimensional stability, increased stiffness, and higher temperature applications when compared to unfilled PA.Drop-in replacement for other commercially .. |
|||
Izod Impact, Notched | 0.420 J/cm | 0.787 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics LNP THERMOCOMP AX06472 ABS LNP* Thermocomp* AX06472 is a compound based on ABS containing a clay blend. |