Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Izod Impact, Notched | 0.800 J/cm | 1.50 ft-lb/in | ASTM D256-93a |
Multibase Multi-Pro® 4008 RC Medium Impact 40% Glass Filled Polypropylene Multi-Pro 4008 RC is a chemically coupled glass reinforced polypropylene compound exhibiting highest flexural modulus, flex strength and high impact resistance. Heat resistance is high due to highl.. |
|||
Izod Impact, Notched | 0.800 J/cm @Thickness 6.35 mm, Temperature 23.0 °C |
1.50 ft-lb/in @Thickness 0.250 in, Temperature 73.4 °F |
Injection Molded; ASTM D256A |
PolyOne Gravi-Tech™ GRV-NJ-110-W Polyamide 12 (Nylon 12) Information provided by PolyOne |
|||
Izod Impact, Notched | 0.800 J/cm @Thickness 3.18 mm, Temperature 23.0 °C |
1.50 ft-lb/in @Thickness 0.125 in, Temperature 73.4 °F |
Injection Molded; ASTM D256A |
PolyOne Stat-Tech™ NN-30CF/000 Black Polyamide 66 (Nylon 66) Stat-Tech™ Electrically Conductive Compounds are specifically engineered to provide anti-static, ESD and RFI/EMI shielding performance for critical electronic equipment applications. These compound.. |
|||
Izod Impact, Notched | 0.800 J/cm @Thickness 3.17 mm |
1.50 ft-lb/in @Thickness 0.125 in |
ASTM D256 |
PTS PBT-30GF 30% Glass Fiber Reinforced PBT Information provided by Polymer Technology and Services, LLC (PTS). |
|||
Izod Impact, Notched | 0.800 J/cm | 1.50 ft-lb/in | ASTM D256 |
Solvay Specialty Polymers Primef® 7002 Polyphenylene Sulfide (PPS), 65% GlassMineral
(discontinued **) Primef 7002 is a 65% mineral/glass fiber reinforced polyphenylene sulfide (PPS). This grade offers higher fluidity than Primef 7010 (also 65% mineral/glass fiber), but with somewhat lower mechanical.. |
|||
Izod Impact, Notched | 0.800 J/cm | 1.50 ft-lb/in | ASTM D256 |
Solvay Specialty Polymers Amodel® A-1133 HS Polyphthalamide (PPA)
(Unverified Data**) Amodel A-1133 HS is a 33% glass reinforced, heat stabilized polyphthalamide (PPA) with a high heat deflection temperature, high flexural modulus and high tensile strength. Excellent creep resistance.. |
|||
Izod Impact, Notched | 0.800 J/cm | 1.50 ft-lb/in | ASTM D256 |
Solvay Specialty Polymers Amodel® AS-4133 HS Polyphthalamide (PPA)
(Unverified Data**) Amodel AS-4133 HS is a 33% glass reinforced, lubricated, heat stabilized grade of polyphthalamide (PPA) that offers fast cycle times and moldability in hot water molds. Typical applications include .. |
|||
Izod Impact, Notched | 0.800 J/cm @Temperature 23.0 °C |
1.50 ft-lb/in @Temperature 73.4 °F |
ASTM-D256 |
Polyram PE322G22 PET, 22% Glass Fiber
(discontinued **) 22% Glass fiber reinforced, flame retardant PET for injection molding applications.Information provided by Polyram Ram On Ind. |
|||
Izod Impact, Notched | 0.800 J/cm | 1.50 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics LNP LUBRICOMP ABL12 ABS LNP* Lubricomp* ABL12 is a compound based on Acrylonitrile Butadiene Styrene resin containing 10% Glass Bead and 5% PTFE. Added features of this material include: Internally Lubricated. |
|||
Izod Impact, Notched | 0.800 J/cm | 1.50 ft-lb/in | ASTM D256 |
Mitsui Arlen™ C230 30% Glass Fiber-Reinforced Modified Nylon 6T (DAM) ARLEN™ is a heat resistant, modified polyamide 6T developed by Mitsui Chemicals, Inc. With a high melting point (320°C) and a rigidity level comparable to super engineering plastics, it poss.. |
|||
Izod Impact, Notched | 0.800 J/cm | 1.50 ft-lb/in | ASTM D 256 |
MRC Polymers NAXALOY™ 793MF6 PC + Polyester Blend, 6% Mineral Filled • Available in natural and custom colors• Can be UV Stabilized• Internal and external lubricants can be addedInformation provided by MRC Polymers Inc. |
|||
Izod Impact, Notched | 0.800 J/cm | 1.50 ft-lb/in | ASTM D256-93a |
Multibase Multi-ABS 802 Utility Grade White Data provided by Multibase. |
|||
Izod Impact, Notched | 0.800 J/cm | 1.50 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics NORYL V095 PPE+HIPS (Asia Pacific) 83dc HDT, V0@1.5mm,Higher flow version of PX1007 |
|||
Izod Impact, Notched | 0.800 J/cm | 1.50 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics Valox® 412 PBT (Europe-Africa-Middle East) VALOX 412 is 20% glass reinforced PBT injection moulding resin. Applications: Spotlights, appliance housings and handles. |
|||
Izod Impact, Notched | 0.800 J/cm | 1.50 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics LNP THERMOCOMP DF00A1P PC (Asia Pacific) LNP* Thermocomp* DF00AIP is a compound based on Polycarbonate resin containing Glass Fiber, Flame Retardant. Added features of this material include: High Modulus, low warpage, Non-Brominated & Non.. |
|||
Izod Impact, Notched | 0.800 J/cm | 1.50 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics NORYL GTX GTX820 PPE+PS+PA (Asia Pacific) GR 20%. Higher stiffness of 800000 psi (4000 MPa) flexural modulus. Excellent chemical and high heat resistance. Application: valves. |
|||
Izod Impact, Notched | 0.800 J/cm @Temperature -30.0 °C |
1.50 ft-lb/in @Temperature -22.0 °F |
ASTM D256 |
SABIC Innovative Plastics NORYL IGN5531 PPE+PS (Asia Pacific) Noryl* IGN5531 is an 20% glass fiber reinforced, injection moldable grade. This modified polyphenylene ether resin is designed to deliver a balance of heat, strength and electrical properties. Nor.. |
|||
Izod Impact, Notched | 0.800 J/cm @Temperature 23.0 °C |
1.50 ft-lb/in @Temperature 73.4 °F |
ASTM D 256 |
SABIC Innovative Plastics Ultem ATX152R PEI+PCE 20% Glass fiber filled, high flow Polyetherimide blend with internal mold release. ECO Conforming, UL94 V0 and 5VA listing.This data was supplied by SABIC-IP for the Americas region. |
|||
Izod Impact, Notched | 0.800 J/cm @Temperature -30.0 °C |
1.50 ft-lb/in @Temperature -22.0 °F |
ASTM D256 |
SABIC Innovative Plastics Valox® 508 PBT+PC (Asia Pacific) 30% GR PBT+PC. Excellent mechanical and thermal performance. Non-flame retardant. Reduced warpage characteristics. Applications same as VALOX 420. |
|||
Izod Impact, Notched | 0.800 J/cm | 1.50 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics Valox® SHF4960 PBT (Europe-Africa-Middle East) Valox Super high flow grade, 30% glass filled Flame retardant, High CTI, heat stabilized with mold release. |
|||
Izod Impact, Notched | 0.800 J/cm | 1.50 ft-lb/in | 40 min.; ASTM D256 |
A. Schulman PP 1329 Polypropylene Stabilized Copolymer Polypropylene DescriptionPolypropylene PP 1329 is a stabilized copolymer polypropylene. Information provided by A. Schulman. |
|||
Izod Impact, Notched | 0.800 J/cm | 1.50 ft-lb/in | ASTM D256 |
E-Polymers Tekaster® F615GFR , Flame Retardant, 30% Glass Reinforced PET 30% Glass Fiber Reinforced, Flame RetardantInformation provided by E-Polymers Co. Ltd. |
|||
Izod Impact, Notched | 0.800 J/cm | 1.50 ft-lb/in | ASTM D256 |
Adell RQ-14 Copolymer Polypropylene, 20% Mica Reinforced Data provided by Adell Plastics, Inc. |
|||
Izod Impact, Notched | 0.800 J/cm | 1.50 ft-lb/in | ASTM D256 |
Ashley Polymers Ashlene® E126 PET Polyester, 30% Glass Reinforced PET Polyester, economy grade with 30% glass reinforcement.Data provided by the manufacturer |
|||
Izod Impact, Notched | 0.800 - 1.30 J/cm @Thickness 6.35 mm |
1.50 - 2.44 ft-lb/in @Thickness 0.250 in |
ASTM D256 |
Chang Chun Plastic PBT3030 30% Glass Fiber Enforced PBT Information provided by Dowell Trading Company Ltd. |
|||
Izod Impact, Notched | 0.800 J/cm | 1.50 ft-lb/in | ASTM D256 |
Chem Polymer Chemlon 214 G Nylon 6, 14% Glass Fiber Reinforced A 14% glass fiber reinforced nylon 6 offering improved creep resistance, stiffness, tensile and dimensional stability over unmodified nylon 6 materials.Data provided by the manufacturer, Chem Polyme.. |
|||
Izod Impact, Notched | 0.800 J/cm | 1.50 ft-lb/in | ASTM D256 |
A. Schulman ComAlloy Hiloy® 441 Glass Reinforced, PET Alloy Data provided by the manufacturer, ComAlloy International Company.33% Glass Reinforced.The ComAlloy product line has been integrated into the A Schulman product line. |
|||
Izod Impact, Notched | 0.800 J/cm | 1.50 ft-lb/in | ASTM D256 |
A. Schulman ComAlloy Hiloy® 640 Nylon 6/12, Glass/Mineral Reinforced Data provided by the manufacturer, ComAlloy International Company.45% Glass/Mineral Reinforced.The ComAlloy product line has been integrated into the A Schulman product line. |
|||
Izod Impact, Notched | 0.800 J/cm @Temperature 23.0 °C |
1.50 ft-lb/in @Temperature 73.4 °F |
DAM; ASTM D256 |
DuPont Performance Polymers Zytel® FR70G25V0 NC010 Nylon 66
(Unverified Data**) Zytel® FR70G25V0 NC010 is a 25% glass fiber reinforced, heat stabilized, flame retardant polyamide 66 resin for injection molding.Information provided by DuPont Performance Polymers |
|||
Izod Impact, Notched | 0.800 J/cm @Temperature 23.0 °C |
1.50 ft-lb/in @Temperature 73.4 °F |
ASTM D256 |
LATI LAESTRA G/40-V0CT1 40% Glass Fiber Reinforced, Elastomer Modified, Flame Retardant Syndiotactic Polystyrene (SPS) Description: Laestra compounds are syndiotactic polystyrene (SPS) products. SPS is a polymer offering a combination of properties unavailable with other materials. It exhibits a melting point of 270.. |