Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Izod Impact, Notched | 0.450 J/cm | 0.843 ft-lb/in | ASTM D256-93a |
Multibase Multi-Pro® 3018 CU Dark Green 30% Filler Content Polypropylene Data provided by Multibase. |
|||
Izod Impact, Notched | 0.450 J/cm | 0.843 ft-lb/in | ISO 180/A |
Polimeri Europa Eraclene® MR 80 High Density Polyethylene - Injection Molding Eraclene MR 80 is a high density polyethylene resin (HDPE) with antioxidants, suitable for injection molding application. Eraclene MR 80 shows a good balance between processability and mechanical p.. |
|||
Izod Impact, Notched | 0.450 J/cm | 0.843 ft-lb/in | ASTM D256 |
NCMT NanoPAC™ HS403 High Performance Polypropylene Nanocomposite Applications: Electrical AppliancesInformation provided by Nano Composite Materials Technology Limited |
|||
Izod Impact, Notched | 0.450 J/cm | 0.843 ft-lb/in | ASTM D256 |
Premix Premi-Glas® 8101 Glass Reinforced Polyester BMC Description: Premi-Glas® 8101 is a glass reinforced thermoset polyester Bulk Molding Compound designed for injection molding of automotive forward lighting reflectors. Key features and benefits: Ex.. |
|||
Izod Impact, Notched | 0.450 J/cm @Temperature -30.0 °C |
0.843 ft-lb/in @Temperature -22.0 °F |
ASTM D256 |
SABIC Innovative Plastics Lexan® ML7686E PC (Europe-Africa-Middle East) Transparent Polycarbonate in natural color. Excellent processability, super high flow. UL compliant 94V-2 at 1.5mm. |
|||
Izod Impact, Notched | 0.450 J/cm @Thickness 3.18 mm, Temperature 23.0 °C |
0.843 ft-lb/in @Thickness 0.125 in, Temperature 73.4 °F |
Compression Molded; ASTM D256A |
PolyOne Geon™ Vinyl Cellular E2519 Polyvinyl Chloride, Rigid (PVC, Rigid) Note: Physical properties were measured on non-foamed profiles. Measured density of an extruded 1 thick free foamed part was 0.70 gms/cc at a 360 deg.F melt temperature.Information provided by PolyO.. |
|||
Izod Impact, Notched | 0.450 J/cm | 0.843 ft-lb/in | ASTM D256 |
Solvay Specialty Polymers Amodel® A-1340 HS Polyphthalamide (PPA) Resin, 40% Mineral/Glass Reinforced, at 50% RH
&n AMODEL® A-1340 HS is a 40% mineral/glass reinforced, heat stabilized polyphthalamide (PPA) which exhibits a high deflection temperature, high flexural modulus, high tensile strength and low warpage.. |
|||
Izod Impact, Notched | 0.450 J/cm @Temperature 23.0 °C |
0.843 ft-lb/in @Temperature 73.4 °F |
ASTM D256 |
LATI LAPEX A G/10 10% Glass Fiber Reinforced Polyethersulfone (PES) (UL94 V-0)
(Unverified Data**) Description: Lapex A compounds are polyethersulfone (PES) products. They are high temperature compounds offering an interesting combination of properties. Lapex A provides outstanding thermal resist.. |
|||
Izod Impact, Notched | 0.450 J/cm @Temperature -30.0 °C |
0.843 ft-lb/in @Temperature -22.0 °F |
ASTM D256 |
SABIC Innovative Plastics Lexan® EXRL1061 PC (Asia Pacific) Transparent Polycarbonate in natural color. Excellent processability, super high flow. |
|||
Izod Impact, Notched | 0.450 J/cm @Temperature 23.0 °C |
0.843 ft-lb/in @Temperature 73.4 °F |
ASTM D256 |
LATI LATILUB 73/13-10ST Polyoxymethylene Base (POM), 10% Mixed PTFE/Silicone Self Lubricating Plastic
(Un Description: Latilub self-lubricating plastic materials are more and more often designed to replace metals in applications such as gears, bushings, cams, slides, etc), for which, besides their intri.. |
|||
Izod Impact, Notched | 0.450 J/cm | 0.843 ft-lb/in | ASTM D256A |
DSM Somos® WaterClear® 10110 Epoxy Resin for Stereolithography
(discontinued **) DescriptionDSM Somos® 10110 is a high-speed liquid photopolymer that produces strong, rigid, and durable parts with optical clarity using stereolithography machines. This material is especially us.. |
|||
Izod Impact, Notched | 0.450 J/cm | 0.843 ft-lb/in | ASTM D256 |
LG Chemical LUCEL WK-320 Wear Resistant POM, 20% Mineral Filled, High Modulus LUCEL semi-crystalline acetal copolymer resins are produced by gas phase polymerization. LUCEL resins can be widely accepted as the replacement of thermosets, aluminum and zinc die-casts or other m.. |
|||
Izod Impact, Notched | 0.450 J/cm | 0.843 ft-lb/in | ASTM D256 |
Kolon KOCETAL® LF301 Wear Modified Acetal Resin Special polymer added, improved wear property. Applications: Products for low noise and precision gear. Information provided by API-Kolon. |
|||
Izod Impact, Notched | 0.450 J/cm | 0.843 ft-lb/in | ASTM D256-03 |
Ipiranga Petrochem PH 0952 Polypropylene The production of polypropylene (PP) employs Spheripol technology from Montell / Italy. This technology has been acclaimed all over the world and is known as clean technology, because it does not pr.. |
|||
Izod Impact, Notched | 0.450 - 0.500 J/cm | 0.843 - 0.937 ft-lb/in | ASTM D256 |
Loxim 330 12V0 Nylon 6 Information provided by Loxim Industries |
|||
Izod Impact, Notched | 0.450 J/cm | 0.843 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics LNP STAT-KON DEL139P PC LNP* STAT-KON* DEL139P is a compound based on Polycarbonate containing 15% Carbon Fiber, 5% PTFE. Added features of this grade include: Electrically Conductive, Exceptional Processing, Flame Retar.. |
|||
Izod Impact, Notched | 0.450 J/cm @Temperature 0.000 °C |
0.843 ft-lb/in @Temperature 32.0 °F |
ASTM D256 |
SABIC Innovative Plastics Valox® DR48 PBT (Europe-Africa-Middle East) VALOX DR48 is a 17% glass reinforced, flame retardant injection moulding PBT resin. Applications: lamp sockets, connectors, switches, electrical housings and bases, bobbins, trimmers and electromoto.. |
|||
Izod Impact, Notched | 0.450 J/cm | 0.843 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics Valox® ENH8530 PBT+PET (Europe-Africa-Middle East) Non-Brominated & Non-Chlorinated Flame Retardant, 15% Glass fiber reinforced PBT/PET blend |
|||
Izod Impact, Notched | 0.450 J/cm | 0.843 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics LNP STAT-KON MD000A PP LNP* STAT-KON* MD000A is a compound based on Polypropylene resin containing Carbon. Added feature of this grade is: Electrically Conductive. |
|||
Izod Impact, Notched | 0.450 J/cm @Temperature 23.0 °C |
0.843 ft-lb/in @Temperature 73.4 °F |
ASTM D 256 |
SABIC Innovative Plastics LNP Thermocomp FF008L PE LNP* Thermocomp* FF008L is a compounding based on Polyethylene containing glass fiber. Added characteristics include Low Extractible.This data was supplied by SABIC-IP for the Americas region. |
|||
Izod Impact, Notched | 0.450 J/cm | 0.843 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics LNP THERMOCOMP MF741XXH PP LNP* THERMOCOMP* MF741XXH is a compound based on Polypropylene reain containing Glass Fiber and proprietay antimicrobial additives. Designed for touch surfaces in patient critical healthcare applic.. |
|||
Izod Impact, Notched | 0.450 J/cm @Temperature 23.0 °C |
0.843 ft-lb/in @Temperature 73.4 °F |
ASTM D 256 |
SABIC Innovative Plastics LNP Thermocomp OFJ66 PPS - Linear LNP* Thermocomp* OFJ66 is a compound based on PPS - Linear resin containing Glass Fiber, Mineral. Added features of this material include: Low Warpage.This data was supplied by SABIC-IP for the Ame.. |
|||
Izod Impact, Notched | 0.450 J/cm | 0.843 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics NORYL GTX GTX985 PPE+PA66 NORYL GTX985 is a 18% mineral filled material. This material combines high stiffness and excellent temperature resistance with conductivity for electrostatic painting. |
|||
Izod Impact, Notched | 0.450 J/cm @Temperature -30.0 °C |
0.843 ft-lb/in @Temperature -22.0 °F |
ASTM D256 |
SABIC Innovative Plastics Xenoy® X6320 PBT+PC (Asia Pacific) X6320 is a mineral filled PBT/PC resin developed for automotive painted doorhandles. Key advantages are excellent surface finish, easy processing and paint quality. |
|||
Izod Impact, Notched | 0.450 J/cm @Temperature -30.0 °C |
0.843 ft-lb/in @Temperature -22.0 °F |
ASTM D256 |
SABIC Innovative Plastics NORYL FE1520PW PPE+PS (Europe-Africa-Middle East) Noryl* FE1520PW resin is a blend of polyphenylene oxide (PPO) and polystyrene (PS) resin that contains 20% glass reinforcement. The resin is suitable for injection molding. Noryl FE1520PW resin has .. |
|||
Izod Impact, Notched | 0.450 J/cm | 0.843 ft-lb/in | |
Cosmic Plastics K31 Short Glass Fiber Filled Iso Diallyl Phthalate Molding Compound Data provided by the manufacturer. |
|||
Izod Impact, Notched | 0.450 J/cm @Temperature 23.0 °C |
0.843 ft-lb/in @Temperature 73.4 °F |
ASTM-D256 |
Polyram PlusTek PB351I6 Nylon 6, 30% Glass Fiber and Mineral 30% glass fiber and mineral reinforced polyamide 6 for injection molding applicationsInformation provided by Polyram Ram On Ind. |
|||
Izod Impact, Notched | 0.450 J/cm @Temperature 23.0 °C |
0.843 ft-lb/in @Temperature 73.4 °F |
ASTM-D256 |
Polyram PlusTek RA124 Nylon 6.6, Injection Molding Fast cycle polyamide 6.6 for injection molding applicationsInformation provided by Polyram Ram On Ind. |
|||
Izod Impact, Notched | 0.450 J/cm @Temperature 23.0 °C |
0.843 ft-lb/in @Temperature 73.4 °F |
ASTM D256A |
Braskem H 603 Blow Molding Polypropylene Description: H 603 is a low melt flow rate homopolymer used for general purposes. This resin is designed for blow moulding and extrusion applications. H 603 exhibits excellent processability, excell.. |
|||
Izod Impact, Notched | 0.450 J/cm | 0.843 ft-lb/in | ASTM D256 |
BASF Capron® B73MP Nylon 6 (DAM)