Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Izod Impact, Notched | 0.460 J/cm | 0.862 ft-lb/in | ASTM D256-93a |
Multibase Multi-Pro® 0505 RC Black 5.2% Glass Filled Polypropylene This product was specially designed for one customer's glass filled polypropylene application.Data provided by Multibase. |
|||
Izod Impact, Notched | 0.460 J/cm | 0.862 ft-lb/in | ASTM D256 |
NYCOA 512 PA 6 UL and NSF rated nucleated general purpose molding gradeInformation provided by NYCOA, Inc. |
|||
Izod Impact, Notched | 0.460 J/cm @Temperature 23.0 °C |
0.862 ft-lb/in @Temperature 73.4 °F |
ASTM D 256 |
SABIC Innovative Plastics Cycolac® INP572 ABS High molecular weight SAN, functions as a carrier resin for color concentrates. Can be used as compounding additives for polymer blends. Can be blended with high rubber graft modifier resins to pro.. |
|||
Izod Impact, Notched | 0.460 J/cm | 0.862 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics Cycolac® INP572 ABS+SAN High molecular weight SAN, functions as a carrier resin for color concentrates. Can be used as compounding additives for polymer blends. Can be blended with high rubber graft modifier resins to pro.. |
|||
Izod Impact, Notched | 0.460 J/cm @Thickness 3.18 mm, Temperature 23.0 °C |
0.862 ft-lb/in @Thickness 0.125 in, Temperature 73.4 °F |
Compression Molded; ASTM D256 |
PolyOne Geon™ L4605 Ivory 3098 Polyvinyl Chloride, Semi-Rigid (PVC, Semi-Rigid) Information provided by PolyOne |
|||
Izod Impact, Notched | 0.460 J/cm | 0.862 ft-lb/in | ASTM D256 |
North Wood Plastics Polypropylene with 20% Wood Fiber, Extrusion Grade Data provided by North Wood Plastics, Inc. |
|||
Izod Impact, Notched | 0.460 J/cm @Thickness 6.35 mm |
0.862 ft-lb/in @Thickness 0.250 in |
ASTM D256 |
PolyOne Stat-Tech™ PI-05CF/000 Polyetherimide - 5% Carbon Fibers - ESD Applications
(discontinued **) Data provided by PolyOne. |
|||
Izod Impact, Notched | 0.460 J/cm | 0.862 ft-lb/in | ASTM D256A |
LyondellBasell Pro-fax 6331NW Polypropylene Homopolymer, Nucleated/Antistat Key Features: antistatic and nucleated polypropylene homopolymer resin, short cycle time, resists dust pickup, low odorApplications: lightweight containers, closures, hospital and institutional ware.. |
|||
Izod Impact, Notched | 0.460 J/cm | 0.862 ft-lb/in | ASTM D256/A |
Iran Petrochemical (PCC) 60505 High Density Polyethylene 60505 is a HDPE injection molding grade which combines high stiffness with good physical properties. This resin is well suited for crates and toys applications.Application: crates, injection molding.. |
|||
Izod Impact, Notched | 0.460 J/cm | 0.862 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics LNP LUBRICOMP RAL23 PA 66 LNP LUBRICOMP* RAL23 is a compound based on Nylon 66 resin containing 15% PTFE, 10% Aramid Fiber. Added features of this material include: Wear Resistant. |
|||
Izod Impact, Notched | 0.460 J/cm | 0.862 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics LNP LUBRICOMP RAL23 PA 66 (Asia Pacific) LNP LUBRICOMP* RAL23 is a compound based on Nylon 66 resin containing Aramid Fiber, PTFE. Added features of this material include: Internally Lubricated. |
|||
Izod Impact, Notched | 0.460 J/cm | 0.862 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics LNP LUBRICOMP RAL23 PA 66 (Europe-Africa-Middle East) LNP LUBRICOMP* RAL23 is a compound based on Nylon 66 resin containing PTFE, Aramid Fiber. Added features of this material include: Internally Lubricated. |
|||
Izod Impact, Notched | 0.460 J/cm | 0.862 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics LNP LUBRICOMP RAL23S PA 66 LNP LUBRICOMP* RAL23S is a compound based on Nylon 66 resin containing 10% PTFE, 15% Aramid. Added features of this material include: Heat Stabilized, Wear Resistant. |
|||
Izod Impact, Notched | 0.460 J/cm | 0.862 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics LNP LUBRICOMP RAL23S PA 66 (Asia Pacific) LNP LUBRICOMP* RAL23S is a compound based on Nylon 66 resin containing Aramid Fiber, PTFE. Added features of this material include: Heat Stabilized. |
|||
Izod Impact, Notched | 0.460 J/cm | 0.862 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics LNP LUBRICOMP RAL23S PA 66 (Europe-Africa-Middle East) LNP LUBRICOMP* RAL23S is a compound based on Nylon 66 resin containing PTFE, Aramid Fiber. Added features of this material include: Heat Stabilized. |
|||
Izod Impact, Notched | 0.460 J/cm | 0.862 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics LNP LUBRICOMP RFL32 PA 66 LNP* Lubricomp* RFL32 is a compound based on Nylon 66 containing 10% Glass Fiber, 15% PTFE. Added feature of this material includes: Wear Resistant. |
|||
Izod Impact, Notched | 0.460 J/cm | 0.862 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics LNP LUBRICOMP RP004S PA 66 LNP* LUBRICOMP* RP004S is a compound based on Nylon 66 containing PTFE/Silicone. Added features of this grade include: Heat Stabilized, Wear Resistant. |
|||
Izod Impact, Notched | 0.460 J/cm | 0.862 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics LNP STAT-KON DD0001I PC LNP* STAT-KON* DD0001I is a compound based on Polycarbonate resin containing Carbon Powder. Added features include: ECO FR rating of 94V-0 @ 3.0mm and 94V-1 @ 1.5mm, High Impact. |
|||
Izod Impact, Notched | 0.460 J/cm | 0.862 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics LNP STAT-KON DX99620C PC (Asia Pacific) LNP STAT-KON* DX99620C is a compound based on Polycarbonate resin containing Carbon Powder. Added features of this material include: Clean Compounding System. |
|||
Izod Impact, Notched | 0.460 J/cm @Temperature -30.0 °C |
0.862 ft-lb/in @Temperature -22.0 °F |
ASTM D256 |
SABIC Innovative Plastics Valox® IQ325 PBT (Asia Pacific) PBT resin, using chemically recycled post consumer PET Bottles. |
|||
Izod Impact, Notched | 0.460 J/cm @Temperature -30.0 °C |
0.862 ft-lb/in @Temperature -22.0 °F |
ASTM D256 |
SABIC Innovative Plastics Valox® IQ325HP PBT (Asia Pacific) FDA compliant PBT resin, using chemically recycled post consumer PET Bottles. Fit to food contact applications. |
|||
Izod Impact, Notched | 0.460 J/cm @Temperature -30.0 °C |
0.862 ft-lb/in @Temperature -22.0 °F |
ASTM D256 |
SABIC Innovative Plastics Valox® IQNH4550 PBT (Asia Pacific) Valox* iQNH4550 resin is a non-brominated/non-chlorinated flame retardant product based on an environmentally sustainable Valox iQ* PBT resin. Post-consumer recycle (PCR) usage is 31% based on EPEAT.. |
|||
Izod Impact, Notched | 0.460 J/cm | 0.862 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics Valox® V2000DM PBT (Asia Pacific) Unreinforced, directly metallizable PBT injection molding resin with high flow better release characteristics. |
|||
Izod Impact, Notched | 0.460 J/cm | 0.862 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics Valox® V2000DM PBT (Europe-Africa-Middle East) Unreinforced, directly metallizable PBT injection molding resin with high flow better release characteristics. |
|||
Izod Impact, Notched | 0.460 J/cm | 0.862 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics LNP STAT-KON ZX08301 PPE (Asia Pacific) Stat-Kon* ZX08301 compound is a high heat compounds with ESD safe and low warpage performance suitable for use in Semiconductor Packaging Applications. |
|||
Izod Impact, Notched | 0.460 J/cm @Temperature 23.0 °C |
0.862 ft-lb/in @Temperature 73.4 °F |
ASTM D 256 |
SABIC Innovative Plastics LNP Thermocomp 9X06477 SPS LNP* Thermocomp* 9X06477 is a compound based on Syndiotactic Polystyrene resin containing Glass Fiber. Characteristics of this grade is Heat Stabilized.This data was supplied by SABIC-IP for the Am.. |
|||
Izod Impact, Notched | 0.460 J/cm | 0.862 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics LNP THERMOCOMP ZX06323 PPE+HIPS (Asia Pacific) This material is mineral filled PPO grade with high dielectric constant and low loss tangent |
|||
Izod Impact, Notched | 0.460 J/cm | 0.862 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics LNP STAT-KON EX08318C PEI (Asia Pacific) LNP* Stat-Kon* EX08318C is a polyetherimide compound reinforced with carbon fiber for good stiffness, dimension stability and has extremely high level of cleanliness for the most demanding applicati.. |
|||
Izod Impact, Notched | 0.460 J/cm | 0.862 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics Valox® V2000DM PBT Unreinforced, directly metallizable PBT injection molding resin with high flow better release characteristics. |
|||
Izod Impact, Notched | 0.460 J/cm @Thickness 3.20 mm |
0.862 ft-lb/in @Thickness 0.126 in |
ASTM D256 |
Beijing Chemical Industry KAIFA® GL5200 ABS Extrusion Grade Non-toxic, Superior impact strength at low temp., High gloss, Uniform sheet thickness for vacuum moldingInformation provided by Beijing Chemical Industry Research Institute (Group) |