Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Izod Impact, Notched | 0.480 J/cm | 0.899 ft-lb/in | ASTM D256-93a |
Multibase Multi-Pro® 4005 M I Medium Impact 40% Filler Content Polypropylene Multi-Pro 4005 M I is a chemically coupled reinforced polypropylene compound featuring high flex modulus and high impact under retention of the heat resistance properties. The product is designed f.. |
|||
Izod Impact, Notched | 0.480 J/cm @Thickness 3.18 mm, Temperature 23.0 °C |
0.899 ft-lb/in @Thickness 0.125 in, Temperature 73.4 °F |
Injection Molded; ASTM D256A |
PolyOne LubriOne™ AT-000/10T 2S Acetal (POM) Copolymer LubriOne™ Lubricated and Wear-Resistant Compounds have been specifically formulated to be self-lubricating materials, offering low coefficient of friction and improved wear resistance properties. L.. |
|||
Izod Impact, Notched | 0.480 J/cm @Temperature -30.0 °C |
0.899 ft-lb/in @Temperature -22.0 °F |
ASTM D256 |
SABIC Innovative Plastics Cycoloy® NX07353 PC+ABS (Asia Pacific) Cycoloy* C7230P resin is a mineral filled, flame retardant PC/ABS. Good stiffness combined with balanced flow and impact performance, makes it a good candidate for various applications. |
|||
Izod Impact, Notched | 0.480 J/cm @Thickness 3.18 mm |
0.899 ft-lb/in @Thickness 0.125 in |
ASTM D256 |
LNP Stat-Kon® OC-1006 Polyphenylene Sulfide, Carbon Fiber Reinforcement
(discontinued **) Features: Electrically ConductiveForms: PelletsProcessing Method: Injection MoldingInformation provided by LNP, a GE Plastics Company.This data sheet is labeled Discontinued; however many LNP grades.. |
|||
Izod Impact, Notched | 0.480 J/cm @Thickness 6.35 mm |
0.899 ft-lb/in @Thickness 0.250 in |
ASTM D256 |
PolyOne Lubri-Tech™ PS-000/15T-2S Polyester (PBT) - 15% PTFE Lubricated - 2% Silicone Lubricated
(discontinue Data provided by PolyOne. |
|||
Izod Impact, Notched | 0.480 - 4.00 J/cm @Temperature -40.0 - 0.000 °C |
0.899 - 7.49 ft-lb/in @Temperature -40.0 - 32.0 °F |
Average value: 1.28 J/cm Grade Count:13 |
Overview of materials for Acrylonitrile Butadiene Styrene (ABS), Extruded This property data is a summary of similar materials in the MatWeb database for the category "Acrylonitrile Butadiene Styrene (ABS), Extruded". Each property range of values reported is minimum and .. |
|||
Izod Impact, Notched | 0.480 J/cm | 0.899 ft-lb/in | ASTM D256 |
Ineos H00G-00 Polypropylene Homopolymer A polypropylene homopolymer produced by Ineos utilizing catalyst technology. This material meets the Food and Drug Administration requirements of 21CFR 177.1520. Homopolymer H00G-00 meets certain .. |
|||
Izod Impact, Notched | 0.480 J/cm | 0.899 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics LNP LUBRICOMP OX97635 PPS LNP LUBRICOMP* OX97635 is a compound based on Polyphenylene Sulfide resin containing Proprietary Filler(s). Added features of this material include: Electrically Conductive, Wear Resistant. |
|||
Izod Impact, Notched | 0.480 J/cm | 0.899 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics LNP STAT-KON CD000I PS (Asia Pacific) LNP* Stat-kon* CD000I is a compound based on Polystyrene resin containing Carbon Powder. Added features of this material include: Electrically Conductive, High Impact. |
|||
Izod Impact, Notched | 0.480 J/cm | 0.899 ft-lb/in | ASTM D256 |
Solvay Specialty Polymers Udel® GF-110 Polysulfone (PSU), Glass Fiber Udel® GF-110, resin is a 10% glass fiber reinforced polysulfone (PSU). Glass fiber substantially increases the rigidity, tensile strength, creep resistance, dimensional stability and chemical res.. |
|||
Izod Impact, Notched | 0.480 J/cm @Temperature -30.0 °C |
0.899 ft-lb/in @Temperature -22.0 °F |
ASTM D256 |
SABIC Innovative Plastics Valox® 8032UX PBT+PET (Asia Pacific) VALOX 8032UX is a 30% glass fibre reinforced, UV stabilized PBT+PET blend with excellent surface finish. This grade is VALOX 8032U with improved weathering resistance. Applications: appliance housin.. |
|||
Izod Impact, Notched | 0.480 J/cm | 0.899 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics LNP STAT-KON EX11318C PEI (Asia Pacific) LNP* Stat-Kon* EX11318C is a polyetherimide compound reinforced with carbon fiber for good stiffness, dimension stability and has extremely high level of cleanliness for the most demanding applicati.. |
|||
Izod Impact, Notched | 0.480 J/cm | 0.899 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics LNP STAT-KON KE004 Acetal Copoly LNP* STAT-KON* KE004 is a compound based on Acetal Copolymer resin containing 20% Carbon Fiber. Added features of this material include: Electrically Conductive. |
|||
Izod Impact, Notched | 0.480 J/cm @Temperature 23.0 °C |
0.899 ft-lb/in @Temperature 73.4 °F |
ASTM D 256 |
SABIC Innovative Plastics LNP Thermocomp OF003A PPS LNP* Thermocomp* OF003A is a compound based on Polyphenylene Sulfide resin containing Glass Fiber.This data was supplied by SABIC-IP for the Americas region. |
|||
Izod Impact, Notched | 0.480 J/cm | 0.899 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics LNP THERMOCOMP PH1000A PA 6 LNP THERMOCOMP* PH1000A is a compound based on Nylon 6 resin. Added features of this material include: High Specific Gravity. |
|||
Izod Impact, Notched | 0.480 J/cm @Temperature 23.0 °C |
0.899 ft-lb/in @Temperature 73.4 °F |
ASTM D 256 |
SABIC Innovative Plastics LNP Thermocomp RF0059 PA 66 (Asia Pacific) LNP STARFLAM* RF0059 is a compound based on Nylon 66 resin containing Flame Retardant, Glass Fiber. Added features of this material include: Flame Retardant.This data was supplied by SABIC-IP for t.. |
|||
Izod Impact, Notched | 0.480 J/cm | 0.899 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics LNP STAT-KON AE002 ABS LNP* STAT-KON* AE002 is a compound based on ABS resin containing 10% Carbon Fiber. Added feature of this material is: Electrically Conductive. |
|||
Izod Impact, Notched | 0.480 J/cm @Temperature 23.0 °C |
0.899 ft-lb/in @Temperature 73.4 °F |
ASTM D 256 |
SABIC Innovative Plastics Ultem 2110N PEI (Asia Pacific) 10% Glass fiber filled, enhanced flow Polyetherimide (Tg 217C). ECO Conforming.This data was supplied by SABIC-IP for the Asia Pacific region. |
|||
Izod Impact, Notched | 0.480 J/cm | 0.899 ft-lb/in | ASTM D256 |
A. Schulman POLYFORT™ FPP 3454F Talc Filled Copolymer DescriptionPolyfort® FPP 3454F is a 20% talc filled copolymer.Information provided by A. Schulman. |
|||
Izod Impact, Notched | 0.480 J/cm | 0.899 ft-lb/in | ASTM D256 |
A. Schulman POLYFORT™ FPP 1697HU High Flow Fortified Polypropylene DescriptionPolyfort® FPP 1697HU is a high flow fortified polypropylene with high temperature dimensioned stability. It is stabilized for UV exposure and available in matched automotive color.Infor.. |
|||
Izod Impact, Notched | 0.480 J/cm | 0.899 ft-lb/in | ASTM D256 |
A. Schulman POLYFORT™ FPP 1477 Mineral Filled, General-Purpose Polypropylene DescriptionPolyfort® FPP 1477 is a 20% mineral filled, general-purpose polypropylene.Information provided by A. Schulman. |
|||
Izod Impact, Notched | 0.480 J/cm | 0.899 ft-lb/in | ASTM D256 |
A. Schulman POLYFORT™ FPP 1697HU High Flow Fortified Polypropylene DescriptionPolyfort® FPP 1697HU is a high flow fortified polypropylene with high temperature dimensioned stability. It is stabilized for UV exposure and available in matched automotive color.Infor.. |
|||
Izod Impact, Notched | 0.480 J/cm | 0.899 ft-lb/in | ASTM D256 |
A. Schulman POLYFORT™ FPP 3711 High Impact Polypropylene DescriptionPolyfort® FPP 3711 is a 26% calcium carbonate filled high impact polypropylene.Information provided by A. Schulman. |
|||
Izod Impact, Notched | 0.480 J/cm | 0.899 ft-lb/in | ASTM D256A |
Dow DS6D21 Polypropylene Random Copolymer Resin OverviewConsistent processabilityHigh clarity and glossComplies with U.S. FDA 21 CFR 177.1520 (c)3.1aDOW DS6D21 Polypropylene Resin is intended for use in case film processes. It is particularly su.. |
|||
Izod Impact, Notched | 0.480 J/cm @Temperature -40.0 °C |
0.899 ft-lb/in @Temperature -40.0 °F |
ASTM Test |
BASF Ultramid® 8270 HS PA6 (Conditioned) Ultramid 8270 HS is a thermally modified PA6 blow molding compound exhibiting exceptional toughness and melt strength ideally suited for blow molding, profile extrusion, and other applications requi.. |
|||
Izod Impact, Notched | 0.480 J/cm | 0.899 ft-lb/in | ASTM D256 |
A. Schulman ComAlloy Hiloy® 431 Glass Reinforced, PBT Alloy Data provided by the manufacturer, ComAlloy International Company.15% Glass Reinforced.The ComAlloy product line has been integrated into the A Schulman product line. |
|||
Izod Impact, Notched | 0.480 J/cm | 0.899 ft-lb/in | ASTM D256 |
A. Schulman ComAlloy Voloy® 415 Polyester - PBT, Glass/Mineral Reinforced, Flame Retardant, UL Data provided by the manufacturer, ComAlloy International Company.30% Glass/Mineral Reinforced.The ComAlloy product line has been integrated into the A Schulman product line. |
|||
Izod Impact, Notched | 0.480 J/cm | 0.899 ft-lb/in | ASTM D256 |
A. Schulman ComAlloy Voloy® 612 Nylon 6, Glass Fiber/Bead Reinforced, Flame Retardant, UL Data provided by the manufacturer, ComAlloy International Company.30% Glass Fiber/Bead Reinforced.The ComAlloy product line has been integrated into the A Schulman product line. |
|||
Izod Impact, Notched | 0.480 J/cm | 0.899 ft-lb/in | ASTM D256 |
Ashley Polymers Ashlene® 61M Nylon 66, 40% Mineral reinforced A 40% mineral reinforced general purpose Nylon 66 resin with superior stiffness and dimensional stability.Data provided by the manufacturer |
|||
Izod Impact, Notched | 0.480 J/cm | 0.899 ft-lb/in | ASTM D256 |
A. Schulman ComAlloy Lubrilon® 606 Nylon 6/6, PTFE Filled, Flow Enhanced Data provided by the manufacturer, ComAlloy International Company. High performance and excellent lubricity with minimal surface wear.The ComAlloy product line has been integrated into the A Schulma.. |