Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Izod Impact, Notched | 0.534 J/cm | 1.00 ft-lb/in | 73°F; ASTM D256 |
Multibase Multi-Pro® 2514 XU Polypropylene Mineral Filled, 25% by weight.Features:Heat Resistance, HighForms:PelletsProcessing Methods:Injection MoldingUses:AppliancesFurnitureTable ProductsInformation provided by Multibase |
|||
Izod Impact, Notched | 0.534 J/cm @Temperature 22.8 °C |
1.00 ft-lb/in @Temperature 73.0 °F |
ASTM D256 |
Polymer Resources NY66-GP1-[color]-H General Purpose Nylon 66, Heat Stabilized General Purpose Nylon 66, Heat Stabilized, LubricatedProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples. Nylon grad.. |
|||
Izod Impact, Notched | 0.534 J/cm @Temperature 23.0 °C |
1.00 ft-lb/in @Temperature 73.4 °F |
Method A; ASTM D256 |
Phillips 66 COPYLENE® CR350CL Polypropylene, Random Copolymer, Clarified, Lubricated COPYLENE™ CR350CL is a clarified, easy molding high melt flow polypropylene random copolymer resin with good see-through and contact clarity in injection molding applications. Applications: Housewa.. |
|||
Izod Impact, Notched | 0.534 J/cm @Temperature 22.8 °C |
1.00 ft-lb/in @Temperature 73.0 °F |
ASTM D256 |
LTL Color Compounds ColorFast® PSU1700 Polysulfone General purpose polysulfone with excellent clarityAll information provided by LTL Color Compounders, Inc. |
|||
Izod Impact, Notched | 0.534 J/cm | 1.00 ft-lb/in | 73°F; ASTM D256 |
LyondellBasell Pro-faxâ„¢ SC973 Polypropylene Copolymer Description: Pro-faxâ„¢ Ultra SC973 fully formulated (antistatic, nucleated, slip modified), very high melt flow, impact polypropylene reactor copolymer resin is designed for injection molding ap.. |
|||
Izod Impact, Notched | 0.534 J/cm @Thickness 3.17 mm |
1.00 ft-lb/in @Thickness 0.125 in |
ASTM D256 |
Techmer ES HiFill® PA11 GB30 HS 30% Glass Bead Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Bead, 30% Filler by WeightAdditive: Heat Stabilizer and LubricantFeatures: Heat Stabilized and LubricatedInformation provided by .. |
|||
Izod Impact, Notched | 0.534 J/cm @Thickness 3.17 mm |
1.00 ft-lb/in @Thickness 0.125 in |
ASTM D256 |
Techmer ES Luriblend® PA6 TS18 Nylon 6 Availability: North AmericaForms: PelletsAdditive: PTFE+ Silicone Lubricant(18%)Features: LubricatedInformation provided by TP Composites, Inc. |
|||
Izod Impact, Notched | 0.534 J/cm @Thickness 3.17 mm |
1.00 ft-lb/in @Thickness 0.125 in |
ASTM D256 |
Techmer ES Luriblend® PA6 TSX10 Nylon 6 Availability: North AmericaForms: PelletsAdditive: PTFE Lubricant (10%)Features: Lubricated and Good Wear ResistanceInformation provided by TP Composites, Inc. |
|||
Izod Impact, Notched | 0.534 J/cm | 1.00 ft-lb/in | ASTM D256 |
Techmer ES Plaslube® NY-1/TF/20 NAT PA66 |
|||
Izod Impact, Notched | 0.534 J/cm @Thickness 3.17 mm |
1.00 ft-lb/in @Thickness 0.125 in |
ASTM D256 |
Techmer ES Luriblend® POM CO TL20 LE Acetal Availability: North AmericaForms: PelletsAdditive: PTFE Lubricant(20%) and Silicone LubricantFeatures: Lubricated, Good Wear Resistance, Low Friction, Low Extractables and CopolymerUL File Number: E.. |
|||
Izod Impact, Notched | 0.534 J/cm @Thickness 3.17 mm |
1.00 ft-lb/in @Thickness 0.125 in |
ASTM D256 |
Techmer ES Plastiblend® LDPE E FR V-2 Availability: North AmericaForms: PelletsFeatures: Flame RetardantProcessing Method: ExtrusionInformation provided by TP Composites, Inc. |
|||
Izod Impact, Notched | 0.534 J/cm | 1.00 ft-lb/in | ASTM D256-93a |
Lubrizol Stat-Rite® X-5111 Static Control Polypropylene Stat-Rite® X-5111 is a static dissipative Polypropylene alloy. Stat-Rite® X-5111 utilizes the patented Stat-Rite® inherently dissipative polymer (IDP) alloy system to provide clean, permanent ES.. |
|||
Izod Impact, Notched | 0.534 J/cm | 1.00 ft-lb/in | 0.125 in; ASTM D256 |
Chase Plastics CP Pryme® N100M2 (Dry) Nylon 6, Lubricated Features: DurableLubricatedForm: PelletsInformation provided by Chase Plastics. |
|||
Izod Impact, Notched | 0.534 J/cm | 1.00 ft-lb/in | ASTM D256 |
A. Schulman PP 1632-01 Polypropylene Random Copolymer DescriptionPolypropylene PP 1632-01 is a polypropylene random copolymer produced utilizing unique catalyst and processing technology. It was designed for injection molding and stretch blow molding .. |
|||
Izod Impact, Notched | >= 0.534 J/cm | >= 1.00 ft-lb/in | ASTM D256 |
A. Schulman LP390-01 Narrow Molecular Weight Copolymer DescriptionLP 390-01 natural is a narrow molecular weight copolymer, high density polyethylene combining excellent impact strength with good environmental stress crack resistance.ApplicationLP 390-0.. |
|||
Izod Impact, Notched | 0.534 J/cm @Temperature -40.0 °C |
1.00 ft-lb/in @Temperature -40.0 °F |
ASTM D256 |
ExxonMobil HDPE HD 6605.70 High Density Polyethylene Copolymer Resin Product Description: HD 6605.70 is a narrow molecular weight hexane copolymer designed for a wide range of injection molding applications, offering excellent ESCR with good stiffness-toughness balan.. |
|||
Izod Impact, Notched | 0.534 J/cm | 1.00 ft-lb/in | ASTM D256 |
Aclo Accutech Polypropylene Copolymer CP0436M40L Mica Reinforced |
|||
Izod Impact, Notched | 0.534 - 7.47 J/cm @Thickness 3.18 - 3.18 mm |
1.00 - 14.0 ft-lb/in @Thickness 0.125 - 0.125 in |
Average value: 3.11 J/cm Grade Count:4 |
Overview of materials for PVC, Molded This property data is a summary of similar materials in the MatWeb database for the category "PVC, Molded". Each property range of values reported is minimum and maximum values of appropriate MatWeb.. |