Mechanical Properties Metric English Comments
Izod Impact, Notched 0.550 - 0.550 J/cm

@Temperature -30.0 - -30.0 °C
1.03 - 1.03 ft-lb/in

@Temperature -22.0 - -22.0 °F
Average value: 0.550 J/cm Grade Count:1
Overview of materials for Thermoplastic Olefinic Elastomer (TPO), Extrusion Grade
This property data is a summary of similar materials in the MatWeb database for the category "Thermoplastic Olefinic Elastomer (TPO), Extrusion Grade". Each property range of values reported is mini..
Izod Impact, Notched 0.37373 - 0.550 J/cm

@Temperature -40.0 - 82.2 °C
0.70015 - 1.03 ft-lb/in

@Temperature -40.0 - 180 °F
Average value: 0.459 J/cm Grade Count:3
Overview of materials for Acetal Copolymer, 30% Glass Fiber Reinforced
This property data is a summary of similar materials in the MatWeb database for the category "Acetal Copolymer, 30% Glass Fiber Reinforced". Specific grades with glass content between 25% and 34% ar..
Izod Impact, Notched 0.500 - 0.550 J/cm

@Temperature -40.0 - -20.0 °C
0.937 - 1.03 ft-lb/in

@Temperature -40.0 - -4.00 °F
Average value: 0.642 J/cm Grade Count:1
Overview of materials for Polycarbonate, 20% Glass Filled
This property data is a summary of similar materials in the MatWeb database for the category "Polycarbonate, 20% Glass Filled". Specific grades with glass content between 15% and 24% are included. E..
Izod Impact, Notched 0.500 - 0.550 J/cm
0.937 - 1.03 ft-lb/in
ASTM D256
Loxim 230 01V0 Polybutylene Terephthalate
Information provided by Loxim Industries
Izod Impact, Notched 0.150 - 0.550 J/cm

@Temperature -20.0 - 0.000 °C
0.281 - 1.03 ft-lb/in

@Temperature -4.00 - 32.0 °F
Average value: 0.329 J/cm Grade Count:17
Overview of materials for Polypropylene, Flame Retardant
This property data is a summary of similar materials in the MatWeb database for the category "Polypropylene, Flame Retardant". Each property range of values reported is minimum and maximum values of..