Polymer Property : Izod Impact, Notched = 1.42 ft-lb/in Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Izod Impact, Notched 0.760 J/cm

@Thickness 6.35 mm,
Temperature 23.0 °C
1.42 ft-lb/in

@Thickness 0.250 in,
Temperature 73.4 °F
Injection Molded; ASTM D256A
PolyOne LubriOne™ AS-000/15T Acrylonitrile Butadiene Styrene (ABS)
LubriOne™ Lubricated and Wear-Resistant Compounds have been specifically formulated to be self-lubricating materials, offering low coefficient of friction and improved wear resistance properties. L..
Izod Impact, Notched 0.760 J/cm

@Thickness 6.35 mm,
Temperature 23.0 °C
1.42 ft-lb/in

@Thickness 0.250 in,
Temperature 73.4 °F
Injection Molded; ASTM D256A
PolyOne Stat-Tech™ AS-15CF/000 Acrylonitrile Butadiene Styrene (ABS)
Stat-Tech™ Electrically Conductive Compounds are specifically engineered to provide anti-static, ESD and RFI/EMI shielding performance for critical electronic equipment applications. These compound..
Izod Impact, Notched 0.760 J/cm

@Temperature -30.0 °C
1.42 ft-lb/in

@Temperature -22.0 °F
ASTM D256
SABIC Innovative Plastics Lexan® XHT4141 PC Copolymer
XHT4141 is a high flow, high heat polycarbonate copolymer. It is available in a range of opaque and limited transparent colors.
Izod Impact, Notched 0.760 J/cm

@Temperature -30.0 °C
1.42 ft-lb/in

@Temperature -22.0 °F
ASTM D256
SABIC Innovative Plastics Lexan® XHT4141 PC Copolymer (Europe-Africa-Middle East)
XHT4141 is a high flow, high heat polycarbonate copolymer. It is available in a range of opaque and limited transparent colors.
Izod Impact, Notched 0.760 J/cm

@Temperature -30.0 °C
1.42 ft-lb/in

@Temperature -22.0 °F
ASTM D256
SABIC Innovative Plastics Lexan® XHT4143 PC Copolymer
XHT4143 is a high flow, UV stabilized, high heat polycarbonate copolymer blend with an HDT/Af of 162C. It is available in a range of opaque and limited transparent colors.
Izod Impact, Notched 0.760 J/cm

@Temperature -30.0 °C
1.42 ft-lb/in

@Temperature -22.0 °F
ASTM D256
SABIC Innovative Plastics Lexan® XHT4143 PC Copolymer (Asia Pacific)
XHT4143 is a high flow, UV stabilized, high heat polycarbonate copolymer blend with an HDT/Af of 162C. It is available in a range of opaque and limited transparent colors.
Izod Impact, Notched 0.760 J/cm

@Temperature -30.0 °C
1.42 ft-lb/in

@Temperature -22.0 °F
ASTM D256
SABIC Innovative Plastics Lexan® XHT4143T PC Copolymer (Asia Pacific)
XHT4143 is a high flow, UV stabilized, high heat polycarbonate copolymer blend with an HDT/Af of 162C.
Izod Impact, Notched 0.760 J/cm

@Temperature -30.0 °C
1.42 ft-lb/in

@Temperature -22.0 °F
ASTM D256
SABIC Innovative Plastics Lexan® XHT4141 PC Copolymer (Asia Pacific)
XHT4141 is a high flow, high heat polycarbonate copolymer. It is available in a range of opaque and limited transparent colors.
Izod Impact, Notched 0.760 J/cm

@Temperature -30.0 °C
1.42 ft-lb/in

@Temperature -22.0 °F
ASTM D256
SABIC Innovative Plastics Lexan® XHT4143 PC Copolymer (Europe-Africa-Middle East)
XHT4143 is a high flow, UV stabilized, high heat polycarbonate copolymer blend with an HDT/Af of 162C. It is available in a range of opaque and limited transparent colors.
Izod Impact, Notched 0.758 - 0.800 J/cm
1.42 - 1.50 ft-lb/in
Average value: 0.786 J/cm Grade Count:3
Overview of materials for Polychlorotrifluoroethylene; Molded
This property data is a summary of similar materials in the MatWeb database for the category "Polychlorotrifluoroethylene; Molded". Each property range of values reported is minimum and maximum valu..
Izod Impact, Notched 0.760 J/cm
1.42 ft-lb/in
ASTM D256
Kolon KOCETAL® K200 Standard Grade Acetal Resin
Suitable for both injection and extrusion.Applications: Injection and extruded use such as rod and sheetInformation provided by API Kolon.
Izod Impact, Notched >= 0.760 J/cm
>= 1.42 ft-lb/in
Method A; ASTM D 256
Karina 804-48/1-CRM Black PVC Compound
Information provided by Karina Indústria e Comércio de Plásticos Ltda.
Izod Impact, Notched 0.760 J/cm

@Temperature 23.0 °C
1.42 ft-lb/in

@Temperature 73.4 °F
ASTM D 256
SABIC Innovative Plastics LNP Lubricomp EFP36G PEI
LNP* EFP36G is a Polyetherimide base resin containing a Mixed Glass Fiber and PTFE/Silicone.This data was supplied by SABIC-IP for the Americas region.
Izod Impact, Notched 0.760 J/cm
1.42 ft-lb/in
ASTM D256
SABIC Innovative Plastics LNP LUBRICOMP KFI15 ACETAL
LNP* LUBRICOMP* KFI15 is a compound based on Acetal containing 25% Glass Fiber, 2% Silicone. Added feature of this grade is: Wear Resistant.
Izod Impact, Notched 0.760 J/cm

@Temperature 23.0 °C
1.42 ft-lb/in

@Temperature 73.4 °F
ASTM D 256
SABIC Innovative Plastics Valox® VC130 PBT (Asia Pacific)
This data was supplied by SABIC-IP for the Asia Pacific region.
Izod Impact, Notched 0.760 J/cm
1.42 ft-lb/in
ASTM D256
SABIC Innovative Plastics LNP STAT-KON RE0069S PA 66
LNP* STAT-KON* RE0069S is a compound based on Nylon 66 resin containing 30% Carbon Fiber. Added features of this material include: Electrically Conductive, Flame Retardant, Heat Stabilized.
Izod Impact, Notched 0.760 J/cm
1.42 ft-lb/in
UBE UBEPOL BR15HB HIPS (n-DM =0.03 wt %)
Description: UBEPOL-BR15HB is characterized by the highest branching of these 3 grades and is adapted by many PS manufacturers.Information provided by UBE.
Izod Impact, Notched 0.760 J/cm

@Thickness 3.17 mm
1.42 ft-lb/in

@Thickness 0.125 in
ASTM D256
Unitika AXG-1500-300 Dry
Characteristics: Glass-reinforced grades of the AX1500 resin, excellent in heat and chemical resistancesFavorable rigidity and dimensional accuracyInformation provided by Unitika Ltd.
Izod Impact, Notched 0.758 J/cm
1.42 ft-lb/in
ASTM D256
Ensinger XP-46 Compression Molded Unfilled PCTFE
PCTFE is a high performance crystalline polymer with excellent chemical resistance. Because of its low moisture absorption, PCTFE can operate in a continuous service temperature of -250°F to 300°F..
Izod Impact, Notched 0.760 J/cm
1.42 ft-lb/in
ASTM D256
SABIC Innovative Plastics NORYL PX2944 PPE+HIPS (Asia Pacific)
PPE/PS, GF20%, high heat, non-FR