Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Izod Impact, Notched | 1.44 J/cm | 2.70 ft-lb/in | ASTM D256-93a |
Multibase Multi-Pro® 0001 Black Polypropylene This product was specially designed for one customer's extrusion application needs. Data is taken from sample material only.Data provided by Multibase. |
|||
Izod Impact, Notched | 1.44 J/cm @Temperature -30.0 °C |
2.70 ft-lb/in @Temperature -22.0 °F |
ASTM D256 |
SABIC Innovative Plastics Lexan® 4504 PPC High heat resistant polycarbonate copolymer, provides DTUL of 290F at 264 psi. FDA food contact compliant in limited colors. Effective January 15th, 2008 this grade will no longer be supported with .. |
|||
Izod Impact, Notched | 1.44 J/cm @Temperature 22.8 °C |
2.70 ft-lb/in @Temperature 73.0 °F |
ASTM D256 |
Polymer Resources PC/TP-GP3-G30 PC/Polyester Alloy, 30% Glass Reinforced Superior Chemical Resistance, 30% Glass ReinforcedProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Information pr.. |
|||
Izod Impact, Notched | 1.44 J/cm | 2.70 ft-lb/in | 73°F; ASTM D256 |
Ravago Manufacturing Americas Hylon® N1013THL Nylon 6/6 (Cond) Information provided by Ravago. |
|||
Izod Impact, Notched | 1.44 J/cm | 2.70 ft-lb/in | 73°F; ASTM D256 |
Ravago Manufacturing Americas Hylon® N1033THL Nylon 6/6 (Cond) Information provided by Ravago. |
|||
Izod Impact, Notched | 1.44 J/cm @Temperature -30.0 °C |
2.70 ft-lb/in @Temperature -22.0 °F |
ASTM D256 |
SABIC Innovative Plastics Lexan® HPH4504 PPC (Asia Pacific) High heat specialty polycarbonate. For medical devices and pharmaceutical applications. Healthcare management of change, biocompatible (ISO10993 of USP Class VI). EtO, steam, gamma and e-beam steril.. |
|||
Izod Impact, Notched | 1.44 J/cm @Temperature -30.0 °C |
2.70 ft-lb/in @Temperature -22.0 °F |
ASTM D256 |
SABIC Innovative Plastics Lexan® HPH4504H PPC (Asia Pacific) High heat specialty polycarbonate with enhanced autoclavability. For medical devices and pharmaceutical applications. Healthcare management of change, biocompatible (ISO10993 of USP Class VI). EtO, .. |
|||
Izod Impact, Notched | 1.44 J/cm | 2.70 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics LNP LUBRICOMP DFL22 PC LNP* Lubricomp* DFL22 is a compound based on Polycarbonate resin containing 10% Glass Fiber and 10% PTFE. Added features include: Internally Lubricated. |
|||
Izod Impact, Notched | 1.44 J/cm @Thickness 3.17 mm, Temperature 22.8 °C |
2.70 ft-lb/in @Thickness 0.125 in, Temperature 73.0 °F |
ASTM D-256 |
Chevron Phillips EC6755 HIPS - High Impact Polystyrene
(discontinued **) Rubber modified high impact polystyrene.Applications:Containers and lidsPackaging for foods such as yot, sour cream, delicatessen salads and gravyCold temperature packagingPortion dairy containersFe.. |
|||
Izod Impact, Notched | 1.44 J/cm | 2.70 ft-lb/in | 73°F; ASTM D256 |
Ravago Manufacturing Americas Hylon® N1033TL Nylon 6/6 (Cond)
(discontinued **) Information provided by Ravago. |
|||
Izod Impact, Notched | 1.44 J/cm @Thickness 6.35 mm, Temperature 23.0 °C |
2.70 ft-lb/in @Thickness 0.250 in, Temperature 73.4 °F |
Method A, Injection Molded; ASTM D256 |
PolyOne Edgetek® NL-43GF/000 Nylon 6/12, Glass Filled
(discontinued **) Description/Features:Glass Fiber ReinforcedPolyOne First ChoiceInformation provided by PolyOne Corporation. |
|||
Izod Impact, Notched | 1.44 J/cm @Thickness 3.17 mm |
2.70 ft-lb/in @Thickness 0.125 in |
ASTM D256 |
Techmer ES HiFill® PA6 GF50 L BN047 LE 50% Glass Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 50% Filler by WeightAdditive: LubricantFeatures: Low Extractables and LubricatedAppearance: BeigeInformation.. |
|||
Izod Impact, Notched | 1.44 J/cm @Thickness 3.17 mm |
2.70 ft-lb/in @Thickness 0.125 in |
ASTM D256 |
Techmer ES Luriblend® PA6 GF40 ML5 HS 12 mm 40% Glass Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber, 40% Filler by WeightAdditive: Heat Stabilized and Molybdenum Disulfide LubricantFeatures: Lubricated and Heat StabilizerAp.. |
|||
Izod Impact, Notched | 1.44 J/cm | 2.70 ft-lb/in | ASTM D256 |
Techmer ES Plaslube® J-1/20/MS/5 NAT PA66 |
|||
Izod Impact, Notched | 1.44 J/cm | 2.70 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics LNP THERMOCOMP PF007 PA 6 LNP* THERMOCOMP* PF007 is a compound based on Nylon 6 resin containing 35% Glass Fiber. |
|||
Izod Impact, Notched | 1.44 J/cm @Temperature -30.0 °C |
2.70 ft-lb/in @Temperature -22.0 °F |
ASTM D256 |
SABIC Innovative Plastics NORYL HNA033 PPE+HIPS Noryl* HNA033 resin is an unfilled modified polyphenylene ether resin designed to withstand several cycles in an autoclave. This resin is suitable for multiple conversion routes and is available in.. |
|||
Izod Impact, Notched | 1.44 J/cm @Temperature -30.0 °C |
2.70 ft-lb/in @Temperature -22.0 °F |
ASTM D256 |
SABIC Innovative Plastics NORYL HNA033 PPE+HIPS (Europe-Africa-Middle East) Noryl* HNA033 resin is an unfilled modified polyphenylene ether resin designed to withstand several cycles in an autoclave. This resin is suitable for multiple conversion routes and is available in.. |
|||
Izod Impact, Notched | 1.44 J/cm | 2.70 ft-lb/in | ASTM D256 |
A. Schulman SCHULAMID® 6 GF50H 50% Glass Fiber Reinforced Nylon 6 Information provided by A. Schulman. |
|||
Izod Impact, Notched | 1.44 J/cm @Thickness 3.17 mm |
2.70 ft-lb/in @Thickness 0.125 in |
injection molded sample; ASTM D256 |
American Polymers API 650-21 Polystyrene API 650-21 has been developed for injection molding applications that need a higher degree of toughness and gloss than conventional polystyrene. This polymer approaches ABS type properties.Applicat.. |
|||
Izod Impact, Notched | 1.44 J/cm | 2.70 ft-lb/in | ASTM D256 |
Ecomass® 1080ZB92 Filled Polyamide Nontoxic alternative to Lead (Pb), radiation shielding applications.Moderate Specific GravityFilled Polyamide (PA) alloyExcellent ToughnessInformation provided by Technical Polymers |
|||
Izod Impact, Notched | 1.44 J/cm | 2.70 ft-lb/in | ASTM D256 |
Ashley Polymers Ashlene® 830L-50G Nylon 6, 50% Glass Reinforced Nylon 6, 50% glass reinforced resin.Data provided by the manufacturer |
|||
Izod Impact, Notched | 1.44 J/cm | 2.70 ft-lb/in | ASTM D256 |
Aclo Accutech Polypropylene Copolymer CP0436G25M5CL Glass/Mineral Reinforced Coupled |
|||
Izod Impact, Notched | 1.44 J/cm @Diameter 3.17 mm |
2.70 ft-lb/in @Diameter 0.125 in |
bar, 0.010" notch radius; ASTM D256 |
Ineos Nova 5120 High Impact Polystyrene
(discontinued **) Good balance of toughness and rigidity, Superior gloss, USP Class VIApplications: Refrigeration, Appliances, High gloss applicationsProperties were determined on injection molded specimens at 23°C .. |
|||
Izod Impact, Notched | 1.44 J/cm @Diameter 3.17 mm |
2.70 ft-lb/in @Diameter 0.125 in |
bar, 0.010" notch radius; ASTM D256 |
Ineos Nova 5124 High Impact Polystyrene
(discontinued **) Good balance of toughness and rigidity, Superior gloss, USP Class VIApplications: Refrigeration, Appliances, High gloss applicationsProperties were determined on injection molded specimens at 23°C .. |
|||
Izod Impact, Notched | 1.44 J/cm @Thickness 6.35 mm, Temperature 23.0 °C |
2.70 ft-lb/in @Thickness 0.250 in, Temperature 73.4 °F |
Method A, Injection Molded; ASTM D256 |
PolyOne Lubri-Tech™ AM-30CF/15T Polyphthalamide (PPA), Carbon Fiber Reinforced, PTFE Lubricated
(discontinued Description/Features:Carbon Fiber ReinforcedPTFE LubricatedPolyOne First ChoiceInformation provided by PolyOne Corporation. |
|||
Izod Impact, Notched | 1.44 J/cm @Temperature -30.0 °C |
2.70 ft-lb/in @Temperature -22.0 °F |
ASTM D256 |
SABIC Innovative Plastics Lexan® HPH4504H PPC High heat specialty polycarbonate with enhanced autoclavability. For medical devices and pharmaceutical applications. Healthcare management of change, biocompatible (ISO10993 of USP Class VI). EtO, .. |