Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Izod Impact, Notched | 1.47 J/cm | 2.76 ft-lb/in | ASTM D256 |
PolyMirae Moplen EP340K Sheet and Thermoforming Grade Polypropylene Moplen RP340K is the polypropylene random copolymer polymer manufactured by PMC under the license of BASELL using the Spheripol process. Moplen RP340K is a random copolymer particularly suitable for.. |
|||
Izod Impact, Notched | 1.47 J/cm | 2.75 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics Lexan® LF1520 PC (Asia Pacific) |
|||
Izod Impact, Notched | 1.47 J/cm | 2.76 ft-lb/in | DIN 53453; ASTM D256 |
Kolon SPESIN® KP213G15HI Multi Reinforced PBT Resin
(discontinued **) SPESIN® is a thermoplastic PBT resin with excellent thermal, mechanical and electrical properties. SPESIN® is widely used in industrial parts and especially in electrical-electronic parts.High hea.. |
|||
Izod Impact, Notched | 1.47 J/cm @Thickness 6.40 mm, Temperature 23.0 °C |
2.76 ft-lb/in @Thickness 0.252 in, Temperature 73.4 °F |
ASTM D256 |
LG Chemical KEYFLEX BT GN7155F Ester Type TPE Description: Extrusion Molding, TPC-ET, Halogen Free Flame Retardant, Medium ModulusApplication: Cable & Wire Jackets, Hose & Tubing, SheetInformation provided by LG Chemical |
|||
Izod Impact, Notched | 1.47 J/cm @Thickness 3.20 mm, Temperature 23.0 °C |
2.76 ft-lb/in @Thickness 0.126 in, Temperature 73.4 °F |
ASTM D256 |
LG Chemical LUMAX GN5006FC PBT+ABS, Heat Resistance Description: Injection Molding, PBT+ABS, Halogen Free Flame RetardantApplication: E&E (Connector)CAS: 9003-56-9, 9003-54-7 and 24968-12-5Information provided by LG Chemical |
|||
Izod Impact, Notched | 1.47 J/cm | 2.75 ft-lb/in | ASTM D256 |
Kolon Kopa® KN153G30 Nylon 6 Resin KOPA is widely used in the automobile and industrial parts.General KOPA N-6 Features: Good mechanical properties, Extreme toughness, Outstanding self-lubrication and abrasion resistance, Excellent c.. |
|||
Izod Impact, Notched | >= 1.47 J/cm @Thickness 6.40 mm, Temperature 23.0 °C |
>= 2.76 ft-lb/in @Thickness 0.252 in, Temperature 73.4 °F |
ASTM D256 |
LG Chemical LUPOL HI2202B PP+GF20%, High Impact Description: Injection Molding, PP+GF20%, General Purpose, High ImpactApplication: Electrical & Electronic, Automotive PartsCAS: 9003-07-0, 65997-17-3 and 9010-79-1Information provided by LG Chemica.. |
|||
Izod Impact, Notched | >= 1.47 J/cm @Thickness 6.40 mm, Temperature 23.0 °C |
>= 2.76 ft-lb/in @Thickness 0.252 in, Temperature 73.4 °F |
ASTM D256 |
LG Chemical LUPOL HI5302RB PP+MF25%, High Impact Description: Injection Molding, PP+MF25%, High Impact, Good WeatherabilityApplication: Automotive Interior PartsCAS: 9003-07-0, 9010-79-1 and 14807-96-6Information provided by LG Chemical |
|||
Izod Impact, Notched | 1.47 J/cm | 2.76 ft-lb/in | DIN 53453; ASTM D256 |
Kolon KOPA® KN135HB30HI Multi Reinforced Nylon 6 KOPA® is a thermoplastic resin with excellent mechanical, thermal and electrical properties and is widely used in automobile and industrial parts.Good mechanical properties, outstanding self-lubr.. |
|||
Izod Impact, Notched | 1.47 J/cm | 2.76 ft-lb/in | |
Shinil Chemical SHINSTAT ABS Electrostatic Control Polymer Injection Grade SHINSTAT is an Inherently Dissipative Polymer (IDP) compound which can discharge the electrostatic charge (ESD) effectively. Shinil has designed SHINSTAT using Shinil's patented IDP technology for .. |
|||
Izod Impact, Notched | 1.47 J/cm @Thickness 3.17 mm |
2.75 ft-lb/in @Thickness 0.125 in |
ASTM D256 |
Samsung Cheil Industries TRANEX® TX-0520T Transparent Grade ABS Information provided by Polymer Technology and Services, LLC (PTS). |
|||
Izod Impact, Notched | 1.47 J/cm @Thickness 3.17 mm |
2.76 ft-lb/in @Thickness 0.125 in |
ASTM D256 |
Samsung Cheil Industries Starex® TX-0520T TRABS, Unreinforced Information provided by Samsung Cheil Industries. |
|||
Izod Impact, Notched | 1.47 J/cm @Thickness 6.35 mm |
2.76 ft-lb/in @Thickness 0.250 in |
ASTM D256 |
Samsung Cheil Industries Starex® VE-0812 ABS, Unreinforced FR Information provided by Samsung Cheil Industries. |
|||
Izod Impact, Notched | 1.47 J/cm @Thickness 3.17 mm |
2.76 ft-lb/in @Thickness 0.125 in |
ASTM D256 |
Samsung Cheil Industries Starex® WR-9130 ASA, Unreinforced Information provided by Samsung Cheil Industries. |
|||
Izod Impact, Notched | 1.47 J/cm @Thickness 3.17 mm |
2.75 ft-lb/in @Thickness 0.125 in |
ASTM D256 |
Samsung Cheil Industries TRANEX® TX-0520T Transparent Grade ABS Information provided by Polymer Technology and Services, LLC (PTS). |
|||
Izod Impact, Notched | 1.47 J/cm @Thickness 3.17 mm, Temperature 23.0 °C |
2.76 ft-lb/in @Thickness 0.125 in, Temperature 73.4 °F |
ASTM D256 |
Shinkong Synthetic Fibers Shinite® C501G40 Nylon 6, 40% Glass Filled Information from Shinkong Synthetic Fibers Corp. |
|||
Izod Impact, Notched | 1.47 J/cm @Thickness 3.17 mm |
2.76 ft-lb/in @Thickness 0.125 in |
ASTM D256 |
Samsung Cheil Industries Infino® LS-3302A PC, Glass Filled High Impact Information provided by Samsung Cheil Industries. |
|||
Izod Impact, Notched | 1.47 J/cm @Temperature 23.0 °C |
2.76 ft-lb/in @Temperature 73.4 °F |
ASTM D256 |
SCG Chemicals EL-Leneâ„¢ H6670B High Density Polyethylene Film Key Characteristics:High flowExcellent processabilityHigh stiffnessOdorlessSafe for food contactGood printabilityRecommended Applications: Bottles for drinking water, fruit juice, soft drink, milkI.. |
|||
Izod Impact, Notched | 1.47 J/cm | 2.76 ft-lb/in | |
Zylog Hipolyene® 8025 HC Thermoplastic Polyolefin & PP Compound Information provided by Zylog Plastalloys Pvt. Ltd. |
|||
Izod Impact, Notched | 1.47 J/cm | 2.75 ft-lb/in | ASTM D256 |
Ecomass® 1080ZD93 Tungsten Powder Filled Polyamide Alloy, Injection Molding Grade High Specific Gravity, Tungsten Powder Filled Polyamide (PA) Alloy, Excellent Toughness, Product Form - PelletsProcessing Method: Injection MoldingNontoxic alternative to Lead, weighting, balancing.. |
|||
Izod Impact, Notched | 1.47 J/cm | 2.76 ft-lb/in | ASTM D256 |
E-Polymers TEKASTER® F10G30H 30% Glass Fiber Reinforced Impact Modified PBT Polyester Resin: TEKASTER is thermoplastic polyester resins (PBT, PET) mostly injection molding. PBT has excellent mechanical properties and well balanced engineering plastics with an electrical pe.. |
|||
Izod Impact, Notched | 1.47 J/cm @Thickness 6.40 mm, Temperature 23.0 °C |
2.75 ft-lb/in @Thickness 0.252 in, Temperature 73.4 °F |
ASTM D256 |
Asahi Kasei Xyron® 340Z Modified Polyphenylene Ether Flame RetardantInformation provided by Asahi Kasei |
|||
Izod Impact, Notched | 1.47 J/cm @Thickness 6.40 mm, Temperature 23.0 °C |
2.75 ft-lb/in @Thickness 0.252 in, Temperature 73.4 °F |
ASTM D256 |
Asahi Kasei Xyron® 640V Modified Polyphenylene Ether Flame RetardantInformation provided by Asahi Kasei |
|||
Izod Impact, Notched | 1.47 J/cm @Thickness 6.40 mm, Temperature 23.0 °C |
2.75 ft-lb/in @Thickness 0.252 in, Temperature 73.4 °F |
ASTM D256 |
Asahi Kasei Xyron® 640Z Modified Polyphenylene Ether Flame RetardantInformation provided by Asahi Kasei |
|||
Izod Impact, Notched | 1.47 J/cm | 2.75 ft-lb/in | Dry; ASTM D256 |
Asahi Kasei Leona® 54G43 43% Glass Filled Nylon 66 Enhanced strength, stiffness, and impact resistance; with 43% GF. Excellent appearance. Applications:Fans, railroad tie insulators, office furniture Information provided by Asahi Kasei |
|||
Izod Impact, Notched | 1.47 J/cm @Thickness 6.35 mm, Temperature 23.0 °C |
2.75 ft-lb/in @Thickness 0.250 in, Temperature 73.4 °F |
ASTM D256 |
Asahi Kasei Xyron® 540V Modified Polyphenylene Ether Flame RetardantInformation provided by Asahi Kasei |
|||
Izod Impact, Notched | 1.47 J/cm @Thickness 6.35 mm, Temperature 23.0 °C |
2.75 ft-lb/in @Thickness 0.250 in, Temperature 73.4 °F |
ASTM D256 |
Asahi Kasei Xyron® 540Z Modified Polyphenylene Ether Flame RetardantInformation provided by Asahi Kasei |
|||
Izod Impact, Notched | 1.47 J/cm @Thickness 6.40 mm, Temperature 23.0 °C |
2.75 ft-lb/in @Thickness 0.252 in, Temperature 73.4 °F |
ASTM D256 |
Asahi Kasei Xyron® 740V Modified Polyphenylene Ether Flame RetardantInformation provided by Asahi Kasei |
|||
Izod Impact, Notched | 1.47 J/cm @Thickness 3.17 mm, Temperature 23.0 °C |
2.76 ft-lb/in @Thickness 0.125 in, Temperature 73.4 °F |
ASTM D256 |
Asia International Enterprise (Hong Kong) ST6010 Nylon 66 Information provided by Asia International Enterprise (Hong Kong) Ltd. |
|||
Izod Impact, Notched | 1.47 J/cm | 2.76 ft-lb/in | DIN 53453; ASTM D256 |
Kolon SPELLOY® KB133G30 PC + PBT Alloy Resin
(discontinued **) SPELLOY® is a new technology of thermoplastic Polymer alloys developed to provide unique combination of excellent mechanical properties.High impact resistance (at low temperature), good dimensional.. |