Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Izod Impact, Notched | 0.900 J/cm | 1.69 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics Lexan® 505RU PC (Europe-Africa-Middle East) Lexan* 505RU is a 10% glass reinforced,flame retardant(FR)grade with non brominated and non chlorinated FR systems and UV stablization packages. This product is intended for applications to meet WEE.. |
|||
Izod Impact, Notched | 0.900 J/cm @Temperature -30.0 °C |
1.69 ft-lb/in @Temperature -22.0 °F |
ASTM D256 |
SABIC Innovative Plastics Lexan® FST3403 PC Copolymer (Asia Pacific) Lexan* FST3403 resin is a high flow PC Copolymer Resin, suitable for injection molding. This halogen-free flame retardant resin is EN45545 R6 HL3 compliant and an ideal candidate for train interior .. |
|||
Izod Impact, Notched | 0.900 J/cm | 1.69 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics LNP LUBRICOMP DFL32 PC LNP LUBRICOMP* DFL32 is a compound based on Polycarbonate resin containing 10% Glass Fiber and 15% PTFE. Added features of this material include: Internally Lubricated. |
|||
Izod Impact, Notched | 0.900 J/cm | 1.69 ft-lb/in | ASTM D256 |
Solvay Specialty Polymers Veradel® A-100, A-200, A-300 Polyethersulfone
(discontinued **) For superior long-term performance at high temperatures in severe service environments. It offers especially good toughness, hydrolytic stability, chemical resistance, plus FDA and USDA compliance.N.. |
|||
Izod Impact, Notched | 0.900 J/cm @Thickness 3.17 mm, Temperature -40.0 °C |
1.69 ft-lb/in @Thickness 0.125 in, Temperature -40.0 °F |
ASTM D256 |
Ineos ABS Lustran® 456 Extrusion, Matte-Gloss
(discontinued **) Properties tested in transverse direction (worst case) on 125-mil (3.2 mm) extruded sheets specimens with |
|||
Izod Impact, Notched | 0.900 - 5.34 J/cm @Temperature -40.0 - 0.000 °C |
1.69 - 10.0 ft-lb/in @Temperature -40.0 - 32.0 °F |
Average value: 4.02 J/cm Grade Count:18 |
Overview of materials for Polycarbonate, Impact Modified This property data is a summary of similar materials in the MatWeb database for the category "Polycarbonate, Impact Modified". Each property range of values reported is minimum and maximum values of.. |
|||
Izod Impact, Notched | 0.900 - 1.08 J/cm @Thickness 3.20 - 3.20 mm |
1.69 - 2.02 ft-lb/in @Thickness 0.126 - 0.126 in |
Average value: 0.960 J/cm Grade Count:4 |
Overview of materials for Polycarbonate, Glass Fiber Filled, Flame Retardant This property data is a summary of similar materials in the MatWeb database for the category "Polycarbonate, Glass Fiber Filled, Flame Retardant". Each property range of values reported is minimum a.. |
|||
Izod Impact, Notched | 0.900 J/cm @Temperature 23.0 °C |
1.69 ft-lb/in @Temperature 73.4 °F |
V-Notched 1/8"; ASTM D256 |
Kotec Carbotex KGN-20MRA Polycarbonate, Flame Retardant, 20% Glass Fiber Reinforced Features: Glass fiber 20% reinforced, Mold release, Translucent, Dimensional stability, Flame retardant, High rigidityApplications: OA equipment, Communications, Precision parts, Machineries, E & E .. |
|||
Izod Impact, Notched | 0.900 J/cm @Temperature -30.0 °C |
1.69 ft-lb/in @Temperature -22.0 °F |
ASTM D256 |
SABIC Innovative Plastics NORYL SE100HX PPE+PS Improved productivity and reliability. Nonchlorinated, nonbrominated FR. |
|||
Izod Impact, Notched | 0.900 J/cm | 1.69 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics Valox® HR426 PBT AUTOMOTIVE. 30% GR, hydrolytically stable PBT. Excellent strength, stiffness and dimensional stability. |
|||
Izod Impact, Notched | 0.900 J/cm | 1.69 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics Valox® HR426 PBT (Asia Pacific) AUTOMOTIVE. 30% GR, hydrolytically stable PBT. Excellent strength, stiffness and dimensional stability. |
|||
Izod Impact, Notched | 0.900 J/cm @Temperature -30.0 °C |
1.69 ft-lb/in @Temperature -22.0 °F |
ASTM D256 |
SABIC Innovative Plastics Xenoy® IQ4840 PBT+PC (Asia Pacific) Xenoy iQ4840 (PBT+PC) resin is an environmental responsible, sustainable, and low carbon footprint resin. It is a 10% mineral filled resin with high modulus and ductile (HMD) characteristics. Xen.. |
|||
Izod Impact, Notched | 0.900 J/cm | 1.69 ft-lb/in | ASTM D256 |
SPS Guang Zhou POBUXâ„¢ 3001G30 Flame-retarded/GF30%-PBT Characteristic: Good flame retardance, high mechanical properties, high rigidity, superior heat resistance, good dimensional stabilityApplications: E/E partsInformation Provided by SPS (Guang Zhou) .. |
|||
Izod Impact, Notched | 0.900 J/cm | 1.69 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics LNP STAT-KON RX05488 PA 66 LNP STAT-KON* RX05488 is a compound based on Nylon 66 resin containing Carbon Fiber, Flame Retardant, Glass Fiber, PTFE. Added features of this material include: Electrically Conductive. |
|||
Izod Impact, Notched | 0.900 J/cm | 1.69 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics LNP THERMOCOMP DF0049E PC (Asia Pacific) LNP* Thermocomp* DF0049E is a compound based on Polycarbonate resin containing Glass Fiber, Flame Retardant. Added features of this material include: Easy Molding, Flame Retardant. |
|||
Izod Impact, Notched | 0.900 J/cm | 1.69 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics LNP THERMOCOMP EF006ER PEI (Asia Pacific) LNP* Thermocomp* EF006ER is a compound based on Polyetherimide resin containing Glass Fiber. Added features of this material include: Easy Molding, Mold Release. |
|||
Izod Impact, Notched | 0.900 J/cm | 1.69 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics LNP THERMOCOMP LF005 PEEK (Asia Pacific) LNP* Thermocomp* LF005 is a compound based on Polyetheretherketone resin containing Glass Fiber. |
|||
Izod Impact, Notched | 0.900 J/cm @Temperature 23.0 °C |
1.69 ft-lb/in @Temperature 73.4 °F |
ASTM D 256 |
SABIC Innovative Plastics LNP Thermocomp RF0069RS PA 66 LNP THERMOCOMP* RF0069RS is a compound based on Nylon 66 resin containing Glass Fiber, Mold Release, Flame Retardant. Added features of this material include: Easy Release.This data was supplied by.. |
|||
Izod Impact, Notched | 0.900 J/cm @Temperature -30.0 °C |
1.69 ft-lb/in @Temperature -22.0 °F |
ASTM D256 |
SABIC Innovative Plastics NORYL GFN1740V PPE+PS (Europe-Africa-Middle East) Noryl* GFN1740V Polyphenylene Oxide (PPO) + Polystyrene (PS) resin is a 40 % Glass Reinforced, injection moldable grade with improved hydrolytic stability and with a Tensile Modulus > 11000 MPa; thi.. |
|||
Izod Impact, Notched | 0.900 J/cm | 1.69 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics NORYL LTA1350 PPE+PS Noryl* LTA1350 is an unfilled, injection moldable grade. Designed for improved long term heat aging, this resin also uses non-chlorinated, non-brominated FR additives to achieve a V0 UL94 rating. No.. |
|||
Izod Impact, Notched | 0.900 J/cm | 1.69 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics NORYL PX138H PPE+HIPS (Asia Pacific) Modified PPO Resin with 20% Glass Fibre Reinforced |
|||
Izod Impact, Notched | 0.900 J/cm | 1.69 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics Valox® 830 PBT (Europe-Africa-Middle East) VALOX 830 is a 30% glass fibre reinforced PBT+PET blend with excellent surface finish. Applications: hot air gun housing assemblies, industrial glue guns, appliance housings and handles. |
|||
Izod Impact, Notched | 0.900 J/cm | 1.69 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics LNP THERMOCOMP Noryl_HM3020 PPE+PS LNP* Thermocomp* Noryl_HM3020 compound is a 30% Glass/Mineral filled, high modulus grade. DTUL 248F (120C). UL94 V-1/5VA rated in black and gray. |
|||
Izod Impact, Notched | 0.900 J/cm @Thickness 3.20 mm |
1.69 ft-lb/in @Thickness 0.126 in |
ASTM D256 |
Supreme Petrochem SP 6410 0003 Abrasion Resistant Polystyrene Characteristics Self lubricating, abrasion resistant Low specific Gravity Suitable for multicavity thin wall parts Excellent thermal stability and easy to color Processing Injection moldingApplic.. |
|||
Izod Impact, Notched | 0.900 J/cm @Thickness 3.20 mm |
1.69 ft-lb/in @Thickness 0.126 in |
ASTM D256 |
Supreme Petrochem SP 6425 9885 Abrasion Resistant Polystyrene Characteristics Low friction, impact polystyrene to provide wear resistance and static charge dissipation Excellent gloss & molded appearance and weld line miscibility Easy flowing grade with good.. |
|||
Izod Impact, Notched | 0.900 J/cm @Temperature 23.0 °C |
1.69 ft-lb/in @Temperature 73.4 °F |
ASTM D 256 |
Cossa Polimeri ESTAPROP KUR 4000 CH/TD Polypropylene Copolymer Polypropylene copolymer, elastomer modifiedInformation provided by Cossa Polimeri S.r.l. |
|||
Izod Impact, Notched | 0.900 J/cm @Thickness 3.17 mm |
1.69 ft-lb/in @Thickness 0.125 in |
ASTM Test |
BASF Petra® 330 FR BK-112 30% Glass Filled PET Petra 330 FR BK-112 is a 30% glass reinforced, flame retardant PET, pigmented black injection molding compound rated UL94 V-0 in a 1/64 inch thickness. The product is designed for injection molding.. |
|||
Izod Impact, Notched | 0.900 J/cm | 1.69 ft-lb/in | ASTM D256 |
E-Polymers TEKAMID® TA210G15 , 15% Glass Fiber Reinforced PA66, DAM Beautiful surface, strength propertyInformation provided by E-Polymers Co. Ltd. |