Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Izod Impact, Notched | 0.961 J/cm @Temperature 23.0 °C |
1.80 ft-lb/in @Temperature 73.4 °F |
ASTM D256 |
RheTech Products GC40P100-00 40% Glass Fiber Reinforced Polypropylene, Chemically Coupled, Natural Applications: Consumer goodsBracketsInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Izod Impact, Notched | >= 0.960 J/cm | >= 1.80 ft-lb/in | ASTM D256 |
NIZHNEKAMSKNEFTEKHIM 825 High Impact Polystyrene Grade 825 is a high impact polystyrene for injection molding. The polymer's ability to be molded on fast cycles with minimal stresses results in outstanding impact retention. It is used in such ap.. |
|||
Izod Impact, Notched | 0.960 J/cm | 1.80 ft-lb/in | ASTM Data |
Dow Questra® WA202 High Heat Syndiotactic Polystyrene, 30% Glass Filled
(discontinued **) QUESTRA® Crystalline Polymers are semi-crystalline engineering thermoplastic resins produced from styrene monomer using a proprietary metallocene catalyst system. These syndiotactic polymers are ve.. |
|||
Izod Impact, Notched | 0.961 J/cm @Thickness 6.35 mm, Temperature 23.0 °C |
1.80 ft-lb/in @Thickness 0.250 in, Temperature 73.4 °F |
Method A, Injection Molded; ASTM D256 |
PolyOne Edgetek® BB-25GF/000 PC/ABS Blend, Glass Filled
(discontinued **) Description/Features:Glass Fiber ReinforcedPolyOne First ChoiceInformation provided by PolyOne Corporation. |
|||
Izod Impact, Notched | 0.961 J/cm | 1.80 ft-lb/in | ASTM D256 |
Solvay Specialty Polymers Mindel® B-430 Polysulfone, Modified (PSU, Modified)
(discontinued **) Mindel B-430 is a 30% glass reinforced thermoplastic with excellent dimensional stability, exceptional resistance to warp, good chemical resistance, and high stiffness. It was developed specifically.. |
|||
Izod Impact, Notched | 0.961 J/cm | 1.80 ft-lb/in | at 73°F; ASTM D256 |
M. Holland Company CP300 Polypropylene Copolymer Features: Medium Flow, High Impact Resistance, Good StiffnessUses: Appliances, Business, Equipment, Tool/Tote Box, ToysApprovals: FDA 21 CFR 177.1520 Processing Method: Injection MoldingInformatio.. |
|||
Izod Impact, Notched | 0.961 J/cm @Thickness 3.17 mm |
1.80 ft-lb/in @Thickness 0.125 in |
ASTM D256 |
Fiberfil® PP-61/V2 Polypropylene Copolymer, Flame Retardant, UL94 V2 Information provided by FIBERFIL Engineered Plastics |
|||
Izod Impact, Notched | 0.960 J/cm | 1.80 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics NORYL SE1GFN1 PPE+PS PPE+PS blend. 10% Glass reinforced. Non-brominated, non-chlorinated FR system. UL94 V1 listing. RTI 110/105/110. Dielectric strength. Dimensional stability. Suitable for E/E applications. |
|||
Izod Impact, Notched | 0.960 J/cm | 1.80 ft-lb/in | ASTM D256 |
Solvay Specialty Polymers AvaSpire® AV-650 GF30 Polyaryletherketone (PAEK), 30% Glass Fiber AvaSpire® AV-650 GF30 is a 30% glass fiber-reinforced polyaryletherketone (PAEK) that has been specifically formulated to provide a high degree of chemical resistance and higher mechanical streng.. |
|||
Izod Impact, Notched | 0.961 J/cm @Thickness 3.17 mm |
1.80 ft-lb/in @Thickness 0.125 in |
ASTM D256 |
Techmer ES HiFill® PA6/6 GF30 HR L 30% Glass Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 30% Filler by WeightAdditive: Heat Stabilizer and LubricantFeatures: Heat Stabilized, Lubricated and Hydroly.. |
|||
Izod Impact, Notched | 0.960 J/cm | 1.80 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics LNP STAT-KON WS002I PBT (Asia Pacific) LNP* Stat-kon* WS002I is a compound based on Polybutylene Terephalate resin containing Stainless Steel. Added features of this material include: Electrically Conductive, High Impact. |
|||
Izod Impact, Notched | 0.960 J/cm | 1.80 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics Valox® 508 PBT+PC (Asia Pacific) 30% GR PBT+PC. Excellent mechanical and thermal performance. Non-flame retardant. Reduced warpage characteristics. Applications same as VALOX 420. |
|||
Izod Impact, Notched | 0.961 J/cm | 1.80 ft-lb/in | 0.125 in; ASTM D256 |
Chase Plastics CP Pryme® PC120R Polycarbonate, 20% Glass Fiber Reinforced Features: Good mold releaseForm: PelletsInformation provided by Chase Plastics. |
|||
Izod Impact, Notched | 0.961 J/cm | 1.80 ft-lb/in | At 73°F; ASTM D256 |
Plastics Group Polifil® GFPC-40 40% Glass-Reinforced Polycarbonate Polifil® GFPC series compounds offer a combination of improved dimensional stability and decreased flammability. The excellent balance of physical properties make the Polifil® glass-filled polycar.. |
|||
Izod Impact, Notched | 0.961 J/cm | 1.80 ft-lb/in | ASTM D256 |
Cheng Yu Plastic N6G35 Nylon 6, 35% Glass Filled |
|||
Izod Impact, Notched | 0.960 J/cm @Temperature -40.0 °C |
1.80 ft-lb/in @Temperature -40.0 °F |
ASTM D256 |
Eastman Tenite Propionate 383A2R30009 Natural, Trsp Cellulose Acetate Propionate Plasticizer 9%. Weight loss on heating = 0.4% per ASTM D 707. Soluble matter loss = 0.1% per ASTM D 570.Product Description: TENITE cellulosic plastics are noted for their excellent balance of pr.. |
|||
Izod Impact, Notched | 0.960 J/cm @Thickness 3.17 mm |
1.80 ft-lb/in @Thickness 0.125 in |
ASTM D256 |
Entec Hypro™ PPH-GF30 Natural Homopolymer Polypropylene, 30% Glass Reinforced Information provided by Entec |
|||
Izod Impact, Notched | 0.961 J/cm | 1.80 ft-lb/in | ASTM D256 |
Arkema Group Solarkote® P-610 Acrylic PVC Capstock, clear, low glossInformation provided by Arkema Group |
|||
Izod Impact, Notched | >= 0.961 J/cm | >= 1.80 ft-lb/in | ASTM D256 |
Buckeye Polymers BP RPP 3009 GK3 BLK Polypropylene, Glass Filled Product Information: Our glass reinforced product lines exhibit increased tensile strength, stiffness, and heat deflection. Highly optimized glass reinforced PP resins have successfully replaced en.. |
|||
Izod Impact, Notched | 0.960 J/cm | 1.80 ft-lb/in | ASTM D256 |
Ashley Polymers Ashlene® 528L-25G Nylon 66, 25% Glass Reinforced General purpose glass reinforced Nylon 66, designed for parts requiring excellent thermal and dimensional stability and higher strength than conventional resins.Data provided by the manufacturer |
|||
Izod Impact, Notched | 0.961 J/cm @Temperature 22.8 °C |
1.80 ft-lb/in @Temperature 73.0 °F |
ASTM D256 |
LTL Color Compounds ColorFast® FRPS200 Styrene, High Impact V0/5VA high impact styreneAll information provided by LTL Color Compounders, Inc. |
|||
Izod Impact, Notched | 0.961 J/cm | 1.80 ft-lb/in | 1/8 inch; ASTM D256 |
Adell ER-17 Homopolymer Polypropylene, 30% Glass Reinforced Data provided by Adell Plastics, Inc. |