Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Izod Impact, Notched | 1.00 J/cm @Thickness 6.35 mm, Temperature 23.0 °C |
1.87 ft-lb/in @Thickness 0.250 in, Temperature 73.4 °F |
Injection Molded; ASTM D256A |
PolyOne LubriOne™ PC-000/15T-S2 NATURAL Polycarbonate (PC) Information provided by PolyOne |
|||
Izod Impact, Notched | 1.00 J/cm @Temperature 23.0 °C |
1.87 ft-lb/in @Temperature 73.4 °F |
ASTM D 256 |
SABIC Innovative Plastics Cycoloy® C4220K PC+ABS (Asia Pacific) Cycoloy* C4220K resin is an injection moldable 20% glass reinforced non FR PC-ABS.
Key features include improved Knit Line strength, good flow, excellent strength & rigidity, heat resistance & hyd.. |
|||
Izod Impact, Notched | 1.00 J/cm @Temperature -30.0 °C |
1.87 ft-lb/in @Temperature -22.0 °F |
ASTM D256 |
SABIC Innovative Plastics Cycoloy® CX7240U PC+ABS (Asia Pacific) Cycoloy* CX7240U resin is an injection moldable PC/ABS blend with a UV stabilization package. It contains non-brominated and non-chlorinated flame retardant systems to meet thin wall flame resistanc.. |
|||
Izod Impact, Notched | 1.00 J/cm | 1.87 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics Lexan® CFR5630 PC COPOLYMER (Asia Pacific) LEXAN™ CFR5630 Polycarbonate (PC) is a non-filled resin, suitable for injection molding and extrusion. This non-chlorinated, non-brominated flame retardant PC resin meets FAR25.853 smoke density an.. |
|||
Izod Impact, Notched | 1.00 J/cm | 1.87 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics Lexan® CFR5630D PC COPOLYMER (Asia Pacific) LEXAN™ CFR5630D Polycarbonate (PC) is a non-filled resin, suitable for injection molding and extrusion. This non-chlorinated, non-brominated flame retardant PC resin meets FAR25.853 smoke density a.. |
|||
Izod Impact, Notched | 1.00 J/cm @Temperature -30.0 °C |
1.87 ft-lb/in @Temperature -22.0 °F |
ASTM D256 |
SABIC Innovative Plastics Lexan® HP1REU PC (Europe-Africa-Middle East) High flow polycarbonate. For medical devices and pharmaceutical applications. Healthcare management of change, biocompatible (ISO10993 or USP Class VI). EtO sterilizable. Contains mold release. |
|||
Izod Impact, Notched | 1.00 J/cm @Temperature -30.0 °C |
1.87 ft-lb/in @Temperature -22.0 °F |
ASTM D256 |
SABIC Innovative Plastics Lexan® HP8REU PC (Europe-Africa-Middle East) Very low flow polycarbonate. For medical devices and pharmaceutical applications. Healthcare management of change, biocompatible (ISO10993 or USP Class VI). EtO and steam sterilizable. Contains mold.. |
|||
Izod Impact, Notched | 1.00 J/cm @Temperature -30.0 °C |
1.87 ft-lb/in @Temperature -22.0 °F |
ASTM D256 |
SABIC Innovative Plastics Lexan® LUX7189 PC Lexan* LUX7189 is an injection moldable, high light reflectance FR grade. Contains non-brominated, non-chlorinated flame retardant systems. |
|||
Izod Impact, Notched | 1.00 J/cm | 1.87 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics Lexan® LUX7432C PC COPOLYMER Lexan* LUX7432C Polycarbonate (PC) resin is a non-filled, injection moldable grade. This non-chlorinated, non-brominated flame retardant PC has an UL-94 V0 rating at 1.2 mm / 5VA rating at 3.0mm a.. |
|||
Izod Impact, Notched | 1.00 J/cm | 1.87 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics Lexan® LUX9132C PC COPOLYMER (Europe-Africa-Middle East) Lexan* LUX9132C Polycarbonate (PC) resin is a non-filled, injection moldable grade. This non-chlorinated, non-brominated flame retardant PC has an UL-94 V0 rating at 1.5 mm, high flow capability and.. |
|||
Izod Impact, Notched | 1.00 J/cm @Temperature -30.0 °C |
1.87 ft-lb/in @Temperature -22.0 °F |
ASTM D256 |
SABIC Innovative Plastics Lexan® SLX2431T PC Copolymer (Asia Pacific) Medium viscosity PC copolymer blend with enhanced UV stabilization and added release agent. V2 rated. Available in transparent and tinted colors |
|||
Izod Impact, Notched | 1.00 J/cm | 1.87 ft-lb/in | ASTM D256 |
Solvay Specialty Polymers Kadel® E-1130 Polyketone
(discontinued **) High performance proprietary semi-crystalline polymer based resins with exceptional solvent resistance and high temperature performance. They provide strength and stiffness, plus superior chemical r.. |
|||
Izod Impact, Notched | 1.00 J/cm @Temperature 0.000 °C |
1.87 ft-lb/in @Temperature 32.0 °F |
ASTM D256 |
Gichem GILAC G160 Acrylonitrile Butadiene Styrene
(discontinued **) ABS very high fluidity, good resilience. Medium-High Injection speed.Information provided by GICHEM Gruppo Industriale Chimico |
|||
Izod Impact, Notched | 1.00 J/cm @Temperature -30.0 °C |
1.87 ft-lb/in @Temperature -22.0 °F |
ASTM D256 |
SABIC Innovative Plastics Lexan® HP3NREU PC (Europe-Africa-Middle East) Medium flow polycarbonate. For medical devices and pharmaceutical applications. Healthcare management of change, biocompatible (ISO10993 or USP Class VI). EtO and steam sterilizable. Contains no mo.. |
|||
Izod Impact, Notched | 1.00 J/cm | 1.87 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics Lexan® LUX7636C PC COPOLYMER Lexan* LUX7636C Polycarbonate (PC) resin is a non-filled, extrudable grade. This non-chlorinated, non-brominated flame retardant PC has an UL-94 V0 rating at 1.0 mm / 5VA rating at 3.0mm and is U.. |
|||
Izod Impact, Notched | 1.00 - 7.84532 J/cm @Temperature -40.0 - -20.0 °C |
1.87 - 14.6975 ft-lb/in @Temperature -40.0 - -4.00 °F |
Average value: 3.76 J/cm Grade Count:35 |
Overview of materials for Polycarbonate/Polybutylene Terephthalate (PBT) Blend, Unreinforced This property data is a summary of similar materials in the MatWeb database for the category "Polycarbonate/Polybutylene Terephthalate (PBT) Blend, Unreinforced". Each property range of values repor.. |
|||
Izod Impact, Notched | 1.00 J/cm @Thickness 3.17 mm |
1.87 ft-lb/in @Thickness 0.125 in |
ASTM D256 |
Covestro Apec® DP9-9354 High-Heat Polycarbonate, Flame-Retardant
(discontinued **) Information provided by Bayer Corporation, Plastics DivisionAs of 1 September 2015, Bayer MaterialScience was separated from Bayer AG and has officially adopted its new name – Covestro. This produ.. |
|||
Izod Impact, Notched | 1.00 J/cm | 1.87 ft-lb/in | ASTM D256 |
Global 508 30% Glass Filled PBT Gray Information provided by Global Polymers Corporation. |
|||
Izod Impact, Notched | 1.00 J/cm | 1.87 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics NORYL RN0401 PPE+PS Noryl RN0401 resin is an unfilled Post Consumer Recycle (PCR) based injection moldable modified polyphenylene ether blend comprising at least 20% PCR content. Available in black only. |
|||
Izod Impact, Notched | 1.00 J/cm | 1.87 ft-lb/in | ASTM D256 |
Solvay Specialty Polymers Amodel® AS-4145 HS Polyphthalamide (PPA), 45% Glass Fiber (Dry) Amodel® AS-4145 HS polyphthalamide (PPA) is a 45% glass reinforced resin that is hot-water moldable. Key properties include high heat resistance, high strength and stiffness over a broad tempera.. |
|||
Izod Impact, Notched | 1.00 J/cm @Temperature 23.0 °C |
1.87 ft-lb/in @Temperature 73.4 °F |
ASTM-D256 |
Polyram PlusTek PA301G6 Nylon 6.6, Heat Stabilized, 30% Glass Fiber Heat stabilized, 30% glass fiber reinforced polyamide 6.6 for injection molding applicationsInformation provided by Polyram Ram On Ind. |
|||
Izod Impact, Notched | 1.00 J/cm @Temperature 23.0 °C |
1.87 ft-lb/in @Temperature 73.4 °F |
ASTM-D256 |
Polyram PlusTek PA810 Nylon 6.6, Impact Modified Impact modified polyamide 6.6 for injection molding applicationsInformation provided by Polyram Ram On Ind. |
|||
Izod Impact, Notched | 1.00 J/cm | 1.87 ft-lb/in | ASTM D256 |
A. Schulman PP 1329H-01 Polypropylene Medium Impact Polypropylene DescriptionPolypropylene PP 1329H-01 is a natural high flow, medium impact polypropylene that is suitable for molding thin parts with long mold flow distances. It permits reduction of injection tem.. |
|||
Izod Impact, Notched | 1.00 J/cm @Temperature 23.0 °C |
1.87 ft-lb/in @Temperature 73.4 °F |
ASTM-D256 |
Polyram RamOfin PPH300G8 Polypropylene, 40% Glass Fiber 40% glass fiber reinforced polypropylene for injection molding applicationsInformation provided by Polyram Ram On Ind. |
|||
Izod Impact, Notched | 1.00 J/cm @Temperature 23.0 °C |
1.87 ft-lb/in @Temperature 73.4 °F |
ASTM-D256 |
Polyram RamSter PE301G6 PET, 30% Glass Fiber 30% Glass-fiber reinforced, heat stabilized PET for injection molding applicationsInformation provided by Polyram Ram On Ind. |
|||
Izod Impact, Notched | 1.00 J/cm | 1.87 ft-lb/in | ASTM D256 |
E-Polymers TEKAMID® TA250GFR , Flame Retardant, 25% Glass Fiber Reinforced PA66, DAM GF reinforced, Flame RetardantInformation provided by E-Polymers Co. Ltd. |
|||
Izod Impact, Notched | 1.00 J/cm | 1.87 ft-lb/in | Izod Impact, double-gated, 23°C; SABIC Method |
SABIC Innovative Plastics Cycoloy® CX1440 PC+ABS (Asia Pacific) CYCOLOY CX1440 is a general purpose PC+ABS blend specially developped for thin wall applications requiring weld line strength and high flow with a good balance of properties |
|||
Izod Impact, Notched | 1.00 J/cm | 1.87 ft-lb/in | ASTM D256 |
Adell ER-16 Homopolymer Polypropylene, 30% Glass Reinforced Data provided by Adell Plastics, Inc. |
|||
Izod Impact, Notched | 1.00 J/cm @Temperature -30.0 °C |
1.87 ft-lb/in @Temperature -22.0 °F |
ASTM D256 |
SABIC Innovative Plastics Lexan® HP4EU PC (Europe-Africa-Middle East) Medium flow polycarbonate. For medical devices and pharmaceutical applications. Healthcare management of change, biocompatible (ISO10993 or USP Class VI). EtO and steam sterilizable. Contains mold .. |