Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Izod Impact, Notched | 1.05 J/cm @Temperature 23.0 °C |
1.97 ft-lb/in @Temperature 73.4 °F |
ASTM D256 |
LATI LAESTRA E01 G/30 30% Glass Fiber Reinforced, Elastomer Modified Syndiotactic Polystyrene (SPS)
(disconti Description: Laestra compounds are syndiotactic polystyrene (SPS) products. SPS is a polymer offering a combination of properties unavailable with other materials. It exhibits a melting point of 270.. |
|||
Izod Impact, Notched | 1.05 - 4.64493 J/cm @Temperature -40.0 - 149 °C |
1.97 - 8.70186 ft-lb/in @Temperature -40.0 - 300 °F |
Average value: 2.82 J/cm Grade Count:4 |
Overview of materials for Nylon 66, 40% Glass Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66, 40% Glass Fiber Filled". Specific grades with glass content between 35% and 44% are included. .. |
|||
Izod Impact, Notched | 1.05 J/cm @Thickness 3.20 mm, Temperature 23.0 °C |
1.97 ft-lb/in @Thickness 0.126 in, Temperature 73.4 °F |
ASTM D256 |
Kingfa FRHIPS-1162 Flame Retardant Polystyrene Features:UL 94 V-2 @ 1.6mm, V-2 @ 3.2mmExcellent balance properties, high strengthExcellent heat stabilityExcellent electrical propertiesApplications:Injection moldingGas moldingTV & Audio housingEl.. |
|||
Izod Impact, Notched | 1.05 J/cm | 1.97 ft-lb/in | ASTM D256-03 |
Ipiranga Petrochem GF 5250 HDPE IPQ produces High Density Polyethylene (HDPE) for use by different segments of the plastics molding industry in several processes, including blow molding, extrusion and injection molding.To produce .. |
|||
Izod Impact, Notched | 1.05 J/cm | 1.97 ft-lb/in | ASTM D256 |
Kuraray Genestarâ„¢ G1300H Nylon, 30% Glass Filled Standard HB grade. Halogen free, following the standards that Br is less than 900ppm, Cl is less than 900ppm, and total of halogen amount (Br and Cl) is less than 1500ppm. It is suitable for use in .. |
|||
Izod Impact, Notched | 1.05 J/cm @Temperature 23.0 °C |
1.97 ft-lb/in @Temperature 73.4 °F |
ASTM D256 |
Lavergne VYTEEN ABS 2901 Acrylonitrile Butadiene Styrene Vyteen ABS 2901 is a black recycled general purpose ABS terpolymer with balanced impact/stiffness properties designed for injection molding applications.Features: -Good resilience -Good processabi.. |
|||
Izod Impact, Notched | 1.05 J/cm @Temperature 23.0 °C |
1.97 ft-lb/in @Temperature 73.4 °F |
ASTM D 256 |
SABIC Innovative Plastics LNP Lubricomp LFL36 PEEK LNP* Lubricomp* LFL36 is a compound based on PEEK containing Glass Fiber and PTFE.This data was supplied by SABIC-IP for the Americas region. |
|||
Izod Impact, Notched | 1.05 J/cm | 1.97 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics LNP LUBRICOMP QCL34 PA6.10 LNP* LUBRICOMP* QCL34 is a compound based on Nylon 6/10 resin containing 15% PTFE, 20% Carbon Fiber. Added features of this material include: Wear Resistant, Electrically Conductive. |
|||
Izod Impact, Notched | 1.05 J/cm | 1.97 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics LNP LUBRICOMP RFN169 PA 66 LNP* LUBRICOMP* RFN169 is a compound based on Nylon 66 containing 30% Glass Fiber, 5% MOS2. Added features of this grade include: Wear Resistant, Flame Retardant. |
|||
Izod Impact, Notched | 1.05 J/cm | 1.97 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics ULTEM 2410R PEI (Europe-Africa-Middle East) 40% Glass fiber filled, enhanced flow Polyetherimide (Tg 217C) with internal mold release. Resin is RoHS compliant. UL94 V0 and 5VA listing. |
|||
Izod Impact, Notched | 1.05 J/cm @Temperature 0.000 °C |
1.97 ft-lb/in @Temperature 32.0 °F |
ASTM D256 |
SABIC Innovative Plastics Valox® 420 PBT (Europe-Africa-Middle East) VALOX 420 is a 30% glass fiber reinforced PBT injection moulding resin with excellent mechanical and thermal properties. Applications: appliance handles, spotlights, electric motors. |
|||
Izod Impact, Notched | 1.05 J/cm @Temperature -30.0 °C |
1.97 ft-lb/in @Temperature -22.0 °F |
ASTM D256 |
SABIC Innovative Plastics Valox® 420 PBT (Europe-Africa-Middle East) VALOX 420 is a 30% glass fiber reinforced PBT injection moulding resin with excellent mechanical and thermal properties. Applications: appliance handles, spotlights, electric motors. |
|||
Izod Impact, Notched | 1.05 J/cm @Temperature -30.0 °C |
1.97 ft-lb/in @Temperature -22.0 °F |
ASTM D256 |
SABIC Innovative Plastics Valox® 5031 PBT (Europe-Africa-Middle East) VALOX 5031 is a 30% glass reinforced PBT+PC blend with low warpage characteristics. Applications: appliance handles, automotive doorhandles. This grade is a 508 with reduced warpage. |
|||
Izod Impact, Notched | 1.05 J/cm | 1.97 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics Xenoy® X5500EX PBT+PC (Asia Pacific) Non-FR, non-UV PC/PBT blend for film extrusion application |
|||
Izod Impact, Notched | 1.05 J/cm | 1.97 ft-lb/in | ASTM D256 |
Solvay TECHNYL® A 218W V30 Natural PA66, 30% glass fiber, DRY Description: TECHNYL® A 218W V30 Nat is a polyamide 66, reinforced with 30% of glass fiber, heat stabilized, for injection molding. This product is available in natural color.Benefits: The produc.. |
|||
Izod Impact, Notched | 1.05 J/cm @Temperature 23.0 °C |
1.97 ft-lb/in @Temperature 73.4 °F |
ASTM-D256 |
Polyram RamOfin PPH300G6 Polypropylene, 30% Glass Fiber 30% glass fiber reinforced polypropylene for injection molding applicationsInformation provided by Polyram Ram On Ind. |
|||
Izod Impact, Notched | 1.05 J/cm | 1.97 ft-lb/in | ASTM D256 |
Cheng Yu Plastic NG1500S Nylon 66, 50% Glass Fiber Reinforced |
|||
Izod Impact, Notched | 1.05 J/cm | 1.97 ft-lb/in | Dry; ASTM D256 |
Asahi Kasei Leona® 13G25 25% Glass Filled Nylon 66 Enhanced strength, stiffness and durability; with 25% GF.Applications:Automotive parts Information provided by Asahi Kasei |
|||
Izod Impact, Notched | 1.05 J/cm | 1.97 ft-lb/in | Dry; ASTM D256 |
Asahi Kasei Leona® 14G25 25% Glass Filled Nylon 66 Enhanced strength and stiffness; with 25% GF. Superior heat aging resistance, fatigue resistance, and creep resistance.Applications:Mechanical and electrical parts, engine mounts and other under-the.. |
|||
Izod Impact, Notched | 1.05 J/cm @Temperature -40.0 °C |
1.97 ft-lb/in @Temperature -40.0 °F |
ASTM Test |
BASF Ultramid® 8333G HI HS BK-102 33% Glass Filled PA6 (Dry) Ultramid 8333G HI HS BK-102 is a 33% glass reinforced, heat stabilized, impact modified, pigmented black, PA6 injection molding compound developed for applications requiring improved dry as molded t.. |
|||
Izod Impact, Notched | 1.05 J/cm @Temperature 23.0 °C |
1.97 ft-lb/in @Temperature 73.4 °F |
ASTM D256 |
LATI LARAMID G/45 45% Glass Filled Polyphthalamide (PPA) Based Compound
(Unverified Data**) Laramid compounds are based on a unique semi-crystalline engineering polymer (polyphthalamide) offering improved performance compared to traditional engineering thermoplastics at a lower cost than s.. |
|||
Izod Impact, Notched | 1.05 J/cm | 1.97 ft-lb/in | ASTM D256 |
Kuraray Genestar™ GN2450 Nylon, 45% Glass Filled High Strength V-0 Grade. Features a high strength and modulus. It is well suited for FPC sliders and IC sockets, as well as other components that require modulus and dimensional precision. |