Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Izod Impact, Notched | 6.94 J/cm | 13.0 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics Cycoloy® C3650 PC+ABS (Asia Pacific) Flame retardant PC/ABS blend using non-brominated and non-chlorinated flame retardant systems, offering high impact and excellent extrusion and thermoforming characteristics. Halogen free according .. |
|||
Izod Impact, Notched | 6.94 J/cm | 13.0 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics Lexan® 121 PC UL rated HB as of 10/97. 200 series recommended when V-2 rating required. Nonhalogenated. 17.5 MFR, for small intricate parts. |
|||
Izod Impact, Notched | 6.94 J/cm | 13.0 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics Lexan® 121R PC (Asia Pacific) Nonhalogenated. 17.5 MFR, for small, intricate parts. Internal mold release. |
|||
Izod Impact, Notched | 6.94 J/cm | 13.0 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics Lexan® 124R PC (Asia Pacific) LEXAN 124R is a low viscosity multi purpose grade. FDA food contact compliant in limited colors. Effective January 15th, 2007 this grade is no longer supported with biocompatibility information an.. |
|||
Izod Impact, Notched | 6.94 J/cm | 13.0 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics Lexan® 221 PC (Asia Pacific) 17.5 MFR, for small, intricate parts. Improved flame retardance. |
|||
Izod Impact, Notched | 6.94 J/cm @Temperature 23.0 °C |
13.0 ft-lb/in @Temperature 73.4 °F |
ASTM D 256 |
SABIC Innovative Plastics Lexan® 223 PC 17.5 MFR, for small, intricate parts. Improved flame retardance. UV stabilized.This data was supplied by SABIC-IP for the Americas region. |
|||
Izod Impact, Notched | 6.94 J/cm @Temperature -30.0 °C |
13.0 ft-lb/in @Temperature -22.0 °F |
ASTM D256 |
SABIC Innovative Plastics Lexan® EM1210 PC (Asia Pacific) Automotive interiors. Excellent heat/impact resistance and outstanding property retention over wide temperature range/severe automotive conditions |
|||
Izod Impact, Notched | 6.94 J/cm @Thickness 6.40 mm |
13.0 ft-lb/in @Thickness 0.252 in |
ASTM D256 |
SABIC Innovative Plastics Lexan® EM1210 PC (Asia Pacific) Automotive interiors. Excellent heat/impact resistance and outstanding property retention over wide temperature range/severe automotive conditions |
|||
Izod Impact, Notched | 6.94 J/cm @Temperature 22.8 °C |
13.0 ft-lb/in @Temperature 73.0 °F |
ASTM D256 |
Polymer Resources PC-GP3-D Polycarbonate, General Purpose, High Flow Polycarbonate, General Purpose, High FlowFeatures: • High Impact Resistance • Self ExtinguishingProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inc.. |
|||
Izod Impact, Notched | 6.94 J/cm @Temperature 22.8 °C |
13.0 ft-lb/in @Temperature 73.0 °F |
ASTM D256 |
Polymer Resources PC-GP3-D-[color]-5 Polycarbonate, FDA-compliant Feedstocks, High Flow Polycarbonate, FDA-compliant Feedstocks, High FlowProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Information pr.. |
|||
Izod Impact, Notched | 6.94 J/cm @Temperature 22.8 °C |
13.0 ft-lb/in @Temperature 73.0 °F |
ASTM D256 |
Polymer Resources PC-GP3-D-[color]-6 Polycarbonate, FDA-compliant Feedstocks, High Flow with Mold Release Polycarbonate, FDA-compliant Feedstocks, High Flow with Mold ReleaseProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samp.. |
|||
Izod Impact, Notched | 6.94 J/cm | 13.0 ft-lb/in | 73°F, 0.125 in; ASTM D256 |
Ravago Manufacturing Americas Hybrid B3030U Polycarbonate + PBT Alloy Entec's proprietary products include a full range of compounds in the Nylon 6/6, Nylon 6, ABS, PBT, Polycarbonate, PC/ABS, PC/ASA, PC/PBT, and PPO/PPE resin families.Information provided by Rava.. |
|||
Izod Impact, Notched | 6.94 J/cm | 13.0 ft-lb/in | 73°F, 0.125 in; ASTM D256 |
Ravago Manufacturing Americas Hybrid S464 ABS + Polycarbonate Alloy Entec's proprietary products include a full range of compounds in the Nylon 6/6, Nylon 6, ABS, PBT, Polycarbonate, PC/ABS, PC/ASA, PC/PBT, and PPO/PPE resin families.Information provided by Rava.. |
|||
Izod Impact, Notched | 6.94 J/cm @Thickness 3.17 mm |
13.0 ft-lb/in @Thickness 0.125 in |
ASTM D256 |
Ravago Manufacturing Americas Hylex® P1010FRVNH Polycarbonate, Unreinforced Information provided by Ravago. |
|||
Izod Impact, Notched | 6.94 J/cm | 13.0 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics Lexan® HP2 PC Med/high flow polycarbonate. For medical devices and pharmaceutical applications. Healthcare management of change, biocompatible (ISO10993 or USP Class VI). EtO and steam sterilizable. Contains m.. |
|||
Izod Impact, Notched | 6.94 J/cm | 13.0 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics Lexan® HP2NR PC (Europe-Africa-Middle East) Med/high flow polycarbonate. For medical devices and pharmaceutical applications. Healthcare management of change, biocompatible (ISO10993 or USP Class VI). EtO and steam sterilizable. Contains no.. |
|||
Izod Impact, Notched | 6.94 J/cm | 13.0 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics Lexan® HPS2S PC (Asia Pacific) Med/high flow polycarbonate. For medical devices and pharmaceutical applications. Healthcare management of change, biocompatible (ISO10993 or USP Class VI). EtO, steam, e-beam, and gamma steriliza.. |
|||
Izod Impact, Notched | 6.94 J/cm @Temperature 22.8 °C |
13.0 ft-lb/in @Temperature 73.0 °F |
ASTM D256 |
Polymer Resources PC-UV3-D Polycarbonate, UV-stabilized, High Flow Polycarbonate, UV-stabilized, High FlowProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Information provided by P.. |
|||
Izod Impact, Notched | 6.94 J/cm @Temperature 22.8 °C |
13.0 ft-lb/in @Temperature 73.0 °F |
ASTM D256 |
Polymer Resources PC-UV3-D-[color]-1 Polycarbonate, UV-stabilized, High Flow with Mold Release Polycarbonate, UV-stabilized, High Flow with Mold ReleaseProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Informa.. |
|||
Izod Impact, Notched | 6.94 J/cm @Thickness 3.17 mm |
13.0 ft-lb/in @Thickness 0.125 in |
ASTM D256 |
PTS Tristar® PC-10FRNH 12 MFI Non-Bromine Non-Chlorine Flame Retardant Polycarbonate With Release Information provided by Polymer Technology and Services, LLC (PTS). |
|||
Izod Impact, Notched | 6.94 J/cm @Thickness 3.17 mm |
13.0 ft-lb/in @Thickness 0.125 in |
ASTM D256 |
PTS Tristar® PC-10R-(V22) 22 MFI UV Stabilized Polycarbonate With Release Information provided by Polymer Technology and Services, LLC (PTS). |
|||
Izod Impact, Notched | 6.95 J/cm @Temperature -10.0 °C |
13.0 ft-lb/in @Temperature 14.0 °F |
ASTM D256 |
SABIC Innovative Plastics Xenoy® 1105 PBT+PC (Asia Pacific) PBT/PC blend, injection molding grade, non-reinforced, impact modified, excellent toughness at low temperatures, very good paintability |
|||
Izod Impact, Notched | 6.94 J/cm | 13.0 ft-lb/in | 73°F, 0.125 in.; ASTM D256 |
Star Plastics PC7523R Molding Grade PC Information provided by Star Plastics, Inc. |
|||
Izod Impact, Notched | 6.94 J/cm | 13.0 ft-lb/in | 0.125 in; 10 mil notch; ASTM D256 |
Styron CALIBREâ„¢ IM 401-11 Polycarbonate Information provided by DowThis product line was spun off from Dow Chemical to Styron in 2010. |
|||
Izod Impact, Notched | 6.94 J/cm | 13.0 ft-lb/in | ASTM D256 |
Westlake Plastics Radel® R 5500 Polyphenylsulfone Stock shapes extruded from Radel R resins offer a superior combination of high performance properties that include excellent thermal stability, outstanding toughness, and good environmental stress c.. |
|||
Izod Impact, Notched | 6.94 J/cm | 13.0 ft-lb/in | ASTM D256 |
Westlake Plastics Radel® R Polyphenylsulfone Stock shapes extruded from Radel R resins offer a superior combination of high performance properties that include excellent thermal stability, outstanding toughness and good environmental stress cr.. |
|||
Izod Impact, Notched | 6.94 J/cm @Thickness 3.17 mm |
13.0 ft-lb/in @Thickness 0.125 in |
ASTM D256 |
Diamond Polymers PC 1035L Impact Modified, Polycarbonate, Injection Molding Grade Information Provided by Diamond Polymers, Inc. & Network Polymers, Inc. |
|||
Izod Impact, Notched | 6.94 J/cm | 13.0 ft-lb/in | ASTM D256 |
Aaron Industries AAROPRENE® AEPC 5000-4 Engineered Polycarbonate Resin Melt flow index may be specified. |
|||
Izod Impact, Notched | 6.94 J/cm | 13.0 ft-lb/in | 73°F, 0.125 in; ASTM D256 |
Ravago Manufacturing Americas Hybrid B3030 Polycarbonate + PBT Alloy Entec's proprietary products include a full range of compounds in the Nylon 6/6, Nylon 6, ABS, PBT, Polycarbonate, PC/ABS, PC/ASA, PC/PBT, and PPO/PPE resin families.Information provided by Rava.. |