Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Izod Impact, Notched | 7.20 J/cm @Thickness 3.18 mm, Temperature 23.0 °C |
13.5 ft-lb/in @Thickness 0.125 in, Temperature 73.4 °F |
Injection Molded; ASTM D256A |
PolyOne Geon™ Vinyl Packaging M2288 Polyvinyl Chloride, Rigid (PVC, Rigid) Opaque sheet extrusion compound.Information provided by PolyOne |
|||
Izod Impact, Notched | 7.21 J/cm | 13.5 ft-lb/in | ASTM D256 |
Nylene® Naxel™ PC530-112 UV Resistant Polycarbonate Description: Naxel™ PC530-112 is a high flow, UV resistant polycarbonate. Information provided by Custom Resins. ALM, Nylene Canada, and Custom Resins are all operting companies of Polymeric Resour.. |
|||
Izod Impact, Notched | 7.20 J/cm | 13.5 ft-lb/in | Notched/Unnotched not specified; ASTM D256 |
NOVA Chemicals Novapol® HB-W555-A HDPE Blow Molding Resin Molded Plaque Properties. Features: High molecular weight, rigidity, excellent ESCR, excellent impact strength.Applications: drums, large industrial parts.Data provided by the manufacturer. |
|||
Izod Impact, Notched | 7.20 J/cm @Thickness 3.20 mm |
13.5 ft-lb/in @Thickness 0.126 in |
ASTM D256 |
NOVA Chemicals Novapol® HB-W555-AC PE Blow Molding Resin High molecular weight, High rigidity, Excellent impact strength, Excellent ESCR, Used in high purity chemical packagingInformation provided by NOVA Chemicals. |
|||
Izod Impact, Notched | 7.21 J/cm @Temperature -30.0 °C |
13.5 ft-lb/in @Temperature -22.0 °F |
ASTM D256 |
SABIC Innovative Plastics Lexan® FXD1414T PC Copolymer (Asia Pacific) PC-siloxane copolymer in special light diffusion colors. Medium flow. Improved toughness compared to medium flow standard PC in same color. Color package may affect performance. |
|||
Izod Impact, Notched | 7.20 J/cm @Temperature -30.0 °C |
13.5 ft-lb/in @Temperature -22.0 °F |
ASTM D256 |
SABIC Innovative Plastics Lexan® ML7647 PC (Asia Pacific) Non FR Impact modified PC, excellent Fatigue performance with balanced Flow and impact. Available in Opaque only |
|||
Izod Impact, Notched | 7.20 J/cm @Temperature -30.0 °C |
13.5 ft-lb/in @Temperature -22.0 °F |
ASTM D256 |
SABIC Innovative Plastics Lexan® ML7647K PC (Asia Pacific) Non FR Impact modified PC, excellent Fatigue performance with balanced Flow and impact. Available in Opaque only |
|||
Izod Impact, Notched | 7.20 J/cm @Thickness 3.18 mm, Temperature 23.0 °C |
13.5 ft-lb/in @Thickness 0.125 in, Temperature 73.4 °F |
Compression Molded; ASTM D256A |
PolyOne Geon™ HTX Ultra LA425 Polyvinyl Chloride Alloy (PVC Alloy) Optimum for Black and Darker Colors below 50L value.Recommend drying material for a minimum of 2 hours at 160 degrees Farenheit. Ductile/Brittle transition as measured by Instrumented Impact is 5 de.. |
|||
Izod Impact, Notched | 7.20 J/cm @Thickness 3.18 mm, Temperature 23.0 °C |
13.5 ft-lb/in @Thickness 0.125 in, Temperature 73.4 °F |
Compression Molded; ASTM D256A |
PolyOne Geon™ HTX Ultra LA426 Gray 2382 Polyvinyl Chloride Alloy (PVC Alloy) Optimum for Black and Darker Colors between 50 and 70 L value. Also suitable for colors above 70 L value.Recommend drying material for a minimum of 2 hours at 160 degrees Farenheit. Physical propert.. |
|||
Izod Impact, Notched | 7.20 J/cm | 13.5 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics Lexan® R9453 PC (Asia Pacific) Lexan* R9453 Polycarbonate (PC) is a non-filled, non-chlorine and non-brominate flame retardant resin for general purpose, which contains 30% post-consumer recycled PC. This resin is of UL-94 V0 rat.. |
|||
Izod Impact, Notched | 7.21 J/cm @Temperature -30.0 °C |
13.5 ft-lb/in @Temperature -22.0 °F |
ASTM D256 |
SABIC Innovative Plastics Lexan® FXD1414T PC Copolymer PC-siloxane copolymer in special light diffusion colors. Medium flow. Improved toughness compared to medium flow standard PC in same color. Color package may affect performance. |
|||
Izod Impact, Notched | 7.21 J/cm | 13.5 ft-lb/in | 0.125 in; ASTM D256 |
Ravago Manufacturing Americas Hybrid S570 ABS + Polycarbonate Alloy Entec's proprietary products include a full range of compounds in the Nylon 6/6, Nylon 6, ABS, PBT, Polycarbonate, PC/ABS, PC/ASA, PC/PBT, and PPO/PPE resin families.Information provided by Rava.. |
|||
Izod Impact, Notched | 7.20 J/cm @Temperature 23.0 °C |
13.5 ft-lb/in @Temperature 73.4 °F |
ASTM D 256 |
SABIC Innovative Plastics Lexan® ML4588 PC Extrusion and extrusion blowmolding grade for aircraft applications. Meets FAR 25.853 (60 seconds/30 mils).This data was supplied by SABIC-IP for the Americas region. |
|||
Izod Impact, Notched | 7.21 - 7.68816 J/cm @Temperature -51.1 - 149 °C |
13.5 - 14.4031 ft-lb/in @Temperature -60.0 - 300 °F |
Average value: 7.51 J/cm Grade Count:2 |
Overview of materials for Nylon 66, 60% Glass Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66, 60% Glass Fiber Filled". Specific grades with glass content between 55% and 64% are included. .. |
|||
Izod Impact, Notched | 7.22 J/cm | 13.5 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics Xenoy® 5720U PBT+PC Unfilled PBT+PC alloy. Outstanding low temperature impact/chemical resistance. UV stabilized version of XENOY |
|||
Izod Impact, Notched | 7.22 J/cm | 13.5 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics Xenoy® 5720U PBT+PC (Asia Pacific) Unfilled PBT+PC alloy. Outstanding low temperature impact/chemical resistance. UV stabilized version of XENOY |
|||
Izod Impact, Notched | 7.22 J/cm | 13.5 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics Xenoy® 5720U PBT+PC (Europe-Africa-Middle East) Unfilled PBT+PC alloy. Outstanding low temperature impact/chemical resistance. UV stabilized version of XENOY |
|||
Izod Impact, Notched | 7.20 J/cm | 13.5 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics LNP THERMOCOMP D7002IXH PC LNP* THERMOCOMP* D7002IXH is a compound based on Polycarbonate siloxane copolymer resin containing proprietary antimicrobial additives. Designed for touch surfaces, housings, etc., in healthcare an.. |
|||
Izod Impact, Notched | 7.20 J/cm | 13.5 ft-lb/in | ASTM D256 |
Solvay Specialty Polymers Ixef® 1027 Polyarylamide (PARA)
(Unverified Data**) Ixef 1027 is a 50% glass-fiber reinforced, heat stabilized polyarylamide, which exhibits very high strength and rigidity, outstanding surface gloss, and excellent creep resistance. - Black: Ixef 102.. |