Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Izod Impact, Notched | 2.25 J/cm @Temperature 23.0 °C |
4.22 ft-lb/in @Temperature 73.4 °F |
ASTM D256 |
Reliance Industries Repol C015EG Polypropylene REPOL Polypropylene C015EG is manufactured using Unipol PP process which combines the production efficiency of gas phase fluidized bed reactor technology with the high activity stereospecific cataly.. |
|||
Izod Impact, Notched | 2.25 J/cm @Thickness 3.17 mm |
4.22 ft-lb/in @Thickness 0.125 in |
ASTM D256 |
Unitika U-100 Engineering Plastic CAS No: 26590-50-1Information provided by Unitika Ltd. |
|||
Izod Impact, Notched | 2.25 J/cm @Thickness 3.17 mm |
4.22 ft-lb/in @Thickness 0.125 in |
ASTM D256 |
Diamond Polymers NPP25-0504LGF40 40% Long Glass Fiber Filled Copolymer Polypropylene Information Provided by Diamond Polymers, Inc. & Network Polymers, Inc. |
|||
Izod Impact, Notched | 2.25 J/cm | 4.22 ft-lb/in | ASTM-D256 |
Braskem GF4960 HDPE Blow Molding Polyethylene Homopolymer GF 4960 is a high-density polyethylene homopolymer with high density and stiffness combined with high impact resistance. It was developed for the blow-molding segment. It is used in containers for y.. |
|||
Izod Impact, Notched | 2.25 J/cm @Thickness 3.17 mm |
4.22 ft-lb/in @Thickness 0.125 in |
ASTM Test |
BASF Ultramid® TG7S 35% Glass Filled PA6 (Dry) Ultramid TG7S is a 34% glass reinforced, heat stabilized, impact modified PA6 injection molding grade. It was developed to meet the demanding requirements of the first North American seat
cushion .. |
|||
Izod Impact, Notched | 2.25 J/cm | 4.22 ft-lb/in | ASTM D256 |
Eastman Tenite Propionate 350E0096914 Natural, Trsp Cellulose Acetate Propionate Plasticizer 12%. Weight loss on heating = 0.5% per ASTM D 707. Soluble matter loss = 0.1% per ASTM D 570.Product Description: TENITE cellulosic plastics are noted for their excellent balance of p.. |
|||
Izod Impact, Notched | 2.25 J/cm | 4.22 ft-lb/in | ASTM D256 |
Braskem Green PE SGF4960 Blow Molding and Monofilament High Density Polyethylene Description: SGF4960 is a homopolymer high-density polyethylene, developed for the blow-molding segment with high density and stiffness combined with high impact resistance. The minimum biobased con.. |