Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Izod Impact, Notched | 1.23 J/cm @Temperature 22.8 °C |
2.30 ft-lb/in @Temperature 73.0 °F |
ASTM D256 |
Polymer Resources NY66-G43 Nylon 66, 43% Glass Reinforced Nylon 66, 43% Glass Reinforced, LubricatedProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples. Nylon grades are test.. |
|||
Izod Impact, Notched | 1.23 J/cm @Thickness 3.17 mm |
2.30 ft-lb/in @Thickness 0.125 in |
ASTM D256 |
Ravago Manufacturing Americas Echo® RPC30G BK Polypropylene Homopolymer Available in North America Filler: Glass Fiber Reinforcement, 30% Filler by weight Recycled Content: YesFeatures: Homopolymer Color: Black Form: Pellets Information provided by Ravago |
|||
Izod Impact, Notched | 1.23 J/cm | 2.30 ft-lb/in | 73°F; ASTM D256 |
Ravago Manufacturing Americas Hylon® N1000NL2 Nylon 6/6 (Cond) Information provided by Ravago. |
|||
Izod Impact, Notched | 1.23 J/cm | 2.30 ft-lb/in | ASTM D256 |
RedEye On Demand PC/ABS for FDM Rapid Prototyping This thermoplastic polymer blend combines PC (Polycarbonate) and ABS (Acrylonitrile Butadiene Styrene) to produce an industrial material with a lot to offer. It combines the strength of PC with the .. |
|||
Izod Impact, Notched | 1.23 J/cm @Thickness 3.18 mm |
2.30 ft-lb/in @Thickness 0.125 in |
ASTM D256 |
LNP Lubricomp® EFL-4036 Polyetherimide, Glass Fiber Reinforcement, PTFE Lubricant
(discontinued **) Features: LubricatedForms: PelletsProcessing Method: Injection MoldingInformation provided by LNP, a GE Plastics Company.This data sheet is labeled Discontinued; however many LNP grades are still ac.. |
|||
Izod Impact, Notched | 1.23 J/cm @Thickness 3.20 mm |
2.30 ft-lb/in @Thickness 0.126 in |
ASTM D256 |
KKPC Kuhmo HF 430U Weather-resistant Flame Retarded HIPS Key features: Excellent weather-resistance, non-deca heat-resistance. Common Uses: TV and VCR housing, parts needing non-deca type.HIPS is a functional resin made by copolymerization of styrene mono.. |
|||
Izod Impact, Notched | 1.23 J/cm @Thickness 3.17 mm |
2.30 ft-lb/in @Thickness 0.125 in |
ASTM D256 |
Techmer ES HiFill FR® PA6/6 FR NAT Availability: North AmericaForms: PelletsFeatures: Flame Retardant UL File Number: E157318Appearance: Natural ColorProcessing Method: Injection MoldingInformation provided by TP Composites, Inc. |
|||
Izod Impact, Notched | 1.23 J/cm @Thickness 3.17 mm |
2.30 ft-lb/in @Thickness 0.125 in |
ASTM D256 |
Techmer ES HiFill FR® PA6/6 GF30 FR NAT 30% Glass Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber, 30% Filler by WeightAdditive: Heat Stabilizer and LubricantFeatures: Flame Retardant, Lubricated and Heat StabilizedAppear.. |
|||
Izod Impact, Notched | 1.23 J/cm @Thickness 3.17 mm |
2.30 ft-lb/in @Thickness 0.125 in |
ASTM D256 |
Techmer ES HiFill® PA6/10 GF30 L 30% Glass Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 30% Filler by WeightAdditive: Lubricant Features: LubricatedInformation provided by TP Composites, Inc. |
|||
Izod Impact, Notched | 1.23 J/cm | 2.30 ft-lb/in | ASTM D256 |
Techmer ES Plaslube® J-4/30/TF/13/SI/2 NAT PA6/12 |
|||
Izod Impact, Notched | 1.23 J/cm @Thickness 3.17 mm |
2.30 ft-lb/in @Thickness 0.125 in |
ASTM D256 |
Techmer ES HiFill® PA4/6 GF40 HS 40% Glass Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 40% Filler by WeightAdditive: Heat StabilizerFeatures: Heat StabilizedTPCI# 9627150Information provided by T.. |
|||
Izod Impact, Notched | 1.23 J/cm | 2.30 ft-lb/in | ASTM D256 |
Chase Plastics CP Pryme® NN230GL (DAM) Nylon 66, 33% Glass Fiber Reinforced, Internally Lubricated Information provided by Chase Plastics. |
|||
Izod Impact, Notched | 1.23 J/cm | 2.30 ft-lb/in | ASTM D256 |
Washington Penn Medium Impact Copolymer Grades are available to meet FDA food and drug packaging requirements. These products have excellent mold detail and surface reproduction with fast set-up times. They are also available in an array .. |
|||
Izod Impact, Notched | 1.23 J/cm | 2.30 ft-lb/in | 1/8 in.; ASTM D256 |
Chevron Phillips EA6740 Rubber Modified Polystyrene DescriptionChevron EA6740 is a high impact polystyrene material developed for packaging applications. Its processing characteristics make EA6740 excellent for extrusion and deep-draw thermoforming... |
|||
Izod Impact, Notched | 1.23 J/cm @Temperature 22.8 °C |
2.30 ft-lb/in @Temperature 73.0 °F |
ASTM D256 |
Ensinger TECATOR™ TI 5013 Polyamide-imide (PAI) TECATOR™ is a high performance melt processable polyamideimide that maintains its excellent mechanical and wear properties in temperature environments exceeding 500°F. Stock shapes from Ensinger .. |
|||
Izod Impact, Notched | 1.23 J/cm | 2.30 ft-lb/in | 0°F; ASTM D256A |
Dow DT702 TPO Dow Fascia TPO for Painted ApplicationsInformation provided by Dow |
|||
Izod Impact, Notched | 1.23 J/cm | 2.30 ft-lb/in | ASTM D256A |
Braskem KN-501 Impact Copolymer Polypropylene Description: Excellent color and processing stability, excellent long term heat aging properties, wet / dry environment resistance.Applications: Suggested uses include automotive, housewares, toys, .. |
|||
Izod Impact, Notched | 1.23 J/cm | 2.30 ft-lb/in | injection molded; ASTM D256 |
Americas Styrenics EC6600 High Impact Polystyrene Product CharacteristicsExcellent printabilityMatte surface finishHigh heat distortion temperatureGood low temperature toughnessFood Contact CompliantTypical ApplicationsLithographic sheetPrinted toy.. |
|||
Izod Impact, Notched | 1.23 J/cm | 2.30 ft-lb/in | ASTM D256 |
Cheng Yu Plastic A703G25 ABS 25% Glass Fiber Reinforced |
|||
Izod Impact, Notched | 1.23 J/cm | 2.30 ft-lb/in | ASTM D256 |
Adell ZR-17 33% Glass Reinforced Nylon/Olefin Alloy Data provided by Adell Plastics, Inc. |
|||
Izod Impact, Notched | 1.23 J/cm | 2.30 ft-lb/in | ASTM D256 |
A. Schulman ComAlloy Aqualoy® 150 Polypropylene, Glass Reinforced, Chemically Coupled NSF Data provided by the manufacturer, ComAlloy International Company.50% Glass Reinforced. In Aqualoy® materials, carefully selected base resins and proprietary additives meld hydrolytic stability an.. |
|||
Izod Impact, Notched | 1.23 J/cm | 2.30 ft-lb/in | ASTM D256 |
A. Schulman ComAlloy Comtuf® 615 Nylon 6, Glass Reinforced, Impact Modified Data provided by the manufacturer, ComAlloy International Company.45% Glass Reinforced. Superior toughness and impact resistance characterize Comtuf® materialsThe ComAlloy product line has been int.. |
|||
Izod Impact, Notched | 1.23 J/cm @Thickness 3.18 mm |
2.30 ft-lb/in @Thickness 0.125 in |
ASTM D256 |
LNP Thermocomp® QF-1006 Polyamide 6/10 Copolymer, Glass Fiber Reinforcement
(discontinued **) Forms: PelletsProcessing Method: Injection MoldingInformation provided by LNP, a GE Plastics Company.This data sheet is labeled Discontinued; however many LNP grades are still active under new names.. |
|||
Izod Impact, Notched | 1.23 J/cm | 2.30 ft-lb/in | ASTM D256 |
A. Schulman POLYFORT™ PP 1329 Medium Impact Copolymer Polypropylene DescriptionPolyfort® PP 1329 is a medium impact copolymer polypropylene, available in matched automotive colors. Information provided by A. Schulman. |
|||
Izod Impact, Notched | 1.23 J/cm | 2.30 ft-lb/in | ASTM D256 |
A. Schulman POLYFORT™ PP 1329 Medium Impact Copolymer Polypropylene DescriptionPolyfort® PP 1329 is a medium impact copolymer polypropylene, available in matched automotive colors. Information provided by A. Schulman. |
|||
Izod Impact, Notched | 1.23 J/cm | 2.30 ft-lb/in | ASTM D256 |
Ineos Nova Zyntar® 7041 High Performance Flame Retardant Polystyrene
(discontinued **) Non-Decabromodiphenyl Oxide, High flow, Ease of processingApplications: Electronics, TelevisionsThis is an impact grade of polystyrene containing chemicals to increase resistance to ignition in labo.. |
|||
Izod Impact, Notched | 1.23 J/cm | 2.30 ft-lb/in | 0.125 in.; ASTM D256 |
Resirene Resirene® 6110 High Impact Polystyrene Features:High ImpactEasy ProcessingFDA Rating: 21 CFR 177.1640FlexibilityApplications:Injection MoldingTV CabinetsRemote ControlsToysInformation provided by US distributor Calsak Corporation. |