Mechanical Properties Metric English Comments
Izod Impact, Notched 0.402 - 1.23 J/cm
0.753 - 2.30 ft-lb/in
Average value: 0.681 J/cm Grade Count:45
Overview of materials for Acrylonitrile Butadiene Styrene (ABS), 30% Glass Fiber Filled
This property data is a summary of similar materials in the MatWeb database for the category "Acrylonitrile Butadiene Styrene (ABS), 30% Glass Fiber Filled". Specific grades with glass content betwe..
Izod Impact, Notched 0.690 - 1.23 J/cm

@Temperature -40.0 - -40.0 °C
1.29 - 2.30 ft-lb/in

@Temperature -40.0 - -40.0 °F
Average value: 1.01 J/cm Grade Count:45
Overview of materials for Cellulose Acetate Propionate, Molded
This property data is a summary of similar materials in the MatWeb database for the category "Cellulose Acetate Propionate, Molded". Each property range of values reported is minimum and maximum val..
Izod Impact, Notched 0.370 - 1.23 J/cm

@Temperature -40.0 - -40.0 °C
0.693 - 2.30 ft-lb/in

@Temperature -40.0 - -40.0 °F
Average value: 0.991 J/cm Grade Count:38
Overview of materials for Cellulose Acetate Butyrate, Molded
This property data is a summary of similar materials in the MatWeb database for the category "Cellulose Acetate Butyrate, Molded". Each property range of values reported is minimum and maximum value..
Izod Impact, Notched 0.267 - 1.23 J/cm
0.500 - 2.30 ft-lb/in
Average value: 0.432 J/cm Grade Count:11
Overview of materials for Polyphthalamide (PPA), 10% Glass Fiber Reinforced
This property data is a summary of similar materials in the MatWeb database for the category "Polyphthalamide, 10% Glass Fiber Reinforced". Specific grades with glass content between 5% and 14% are ..
Izod Impact, Notched 0.641 - 1.23 J/cm
1.20 - 2.30 ft-lb/in
Average value: 0.894 J/cm Grade Count:8
Overview of materials for Polystyrene + Polyphenylene Ether, Glass Filler
This property data is a summary of similar materials in the MatWeb database for the category "Polystyrene + Polyphenylene Ether, Glass Filler". Each property range of values reported is minimum and ..
Izod Impact, Notched 0.320 - 1.23 J/cm
0.600 - 2.30 ft-lb/in
Average value: 0.776 J/cm Grade Count:11
Overview of materials for Acrylic, Gamma Radiation Resistant, Molded
This property data is a summary of similar materials in the MatWeb database for the category "Acrylic, Gamma Radiation Resistant, Molded". Each property range of values reported is minimum and maxim..