Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Izod Impact, Notched | 1.60 - 2.40 J/cm | 3.00 - 4.50 ft-lb/in | Average value: 2.25 J/cm Grade Count:10 |
Overview of materials for Diallyl Phthalate (DAP) Molding Compound, Long Glass Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Diallyl Phthalate (DAP) Molding Compound, Long Glass Fiber Filled". Each property range of values report.. |
|||
Izod Impact, Notched | 0.149 - 2.40 J/cm | 0.280 - 4.50 ft-lb/in | Average value: 0.528 J/cm Grade Count:67 |
Overview of materials for Polypropylene with 30% Talc Filler This property data is a summary of similar materials in the MatWeb database for the category "Polypropylene with 30% Talc Filler". Specific grades with primary filler content between 25% and 34% are.. |
|||
Izod Impact, Notched | 0.267 - 2.40 J/cm | 0.500 - 4.50 ft-lb/in | Average value: 1.16 J/cm Grade Count:33 |
Overview of materials for Nylon 6, Glass Fiber/Solid Lube Filled This property data is a summary of similar materials in the MatWeb database for the category "Nylon 6, Glass Fiber/Solid Lube Filled". Each property range of values reported is minimum and maximum v.. |
|||
Izod Impact, Notched | 0.534 - 2.40 J/cm | 1.00 - 4.50 ft-lb/in | Average value: 1.31 J/cm Grade Count:18 |
Overview of materials for Nylon 66, 30% Carbon Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66, 30% Carbon Fiber Filled". Specific grades with carbon fiber content between 25% and 34% are in.. |
|||
Izod Impact, Notched | 0.320 - 2.40 J/cm | 0.600 - 4.50 ft-lb/in | Average value: 0.882 J/cm Grade Count:64 |
Overview of materials for Nylon 66, Carbon Fiber/PTFE Filled This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66, Carbon Fiber/PTFE Filled". Each property range of values reported is minimum and maximum value.. |
|||
Izod Impact, Notched | 1.71 - 2.40 J/cm | 3.20 - 4.50 ft-lb/in | ASTM D256 |
Westlake Plastics Ultra Ethylux® HDPE Ultra Ethylux is made from high density polyethylene resin. This material is a cost effective alternative for a variety of end uses including mild chemical and wear applications. Information provid.. |
|||
Izod Impact, Notched | 2.30 - 2.40 J/cm | 4.30 - 4.50 ft-lb/in | |
Bulk Molding Compounds BMC G10(12) Mineral Filled, Glass Fiber Reinforced Polyester BMC G10 is a general purpose, mineral filled, glass fiber-reinforced polyester that is suitable for compression, transfer and stuffer injection molding. G10 is well suited to applications where hig.. |
|||
Izod Impact, Notched | 0.112 - 2.40 J/cm | 0.210 - 4.50 ft-lb/in | Average value: 0.914 J/cm Grade Count:79 |
Overview of materials for Polyetheretherketone, Glass Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Polyetheretherketone, Glass Fiber Filled". Each property range of values reported is minimum and maximum.. |