Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Izod Impact, Notched = 2.44 ft-lb/in Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Izod Impact, Notched 0.530 - 1.30 J/cm

@Thickness 6.35 mm,
Temperature 23.0 °C
0.993 - 2.44 ft-lb/in

@Thickness 0.250 in,
Temperature 73.4 °F
Injection Molded; ASTM D256A
PolyOne Stat-Tech™ AT-CB2/000 CR Acetal (POM) Copolymer
Stat-Tech™ AT-CB2/000 CR XP020229R2Information provided by PolyOne
Izod Impact, Notched 0.0981 - 1.30 J/cm
0.184 - 2.44 ft-lb/in
Average value: 0.294 J/cm Grade Count:58
Overview of materials for Polystyrene, Heat Resistant Grade
This property data is a summary of similar materials in the MatWeb database for the category "Polystyrene, Heat Resistant Grade". Each property range of values reported is minimum and maximum values..
Izod Impact, Notched 0.260 - 1.30 J/cm

@Temperature -30.0 - -30.0 °C
0.487 - 2.44 ft-lb/in

@Temperature -22.0 - -22.0 °F
Average value: 0.758 J/cm Grade Count:6
Overview of materials for Polystyrene + Polyphenylene Ether, Unreinforced
This property data is a summary of similar materials in the MatWeb database for the category "Polystyrene + Polyphenylene Ether, Unreinforced". Each property range of values reported is minimum and ..
Izod Impact, Notched 0.600 - 1.30 J/cm

@Temperature -30.0 - 0.000 °C
1.12 - 2.44 ft-lb/in

@Temperature -22.0 - 32.0 °F
Average value: 0.875 J/cm Grade Count:2
Overview of materials for Acrylonitrile Butadiene Styrene (ABS), Transparent, Molded
This property data is a summary of similar materials in the MatWeb database for the category "Acrylonitrile Butadiene Styrene (ABS), Transparent, Molded". Each property range of values reported is m..
Izod Impact, Notched 0.600 - 1.30 J/cm

@Thickness 3.17 - 3.17 mm
1.12 - 2.44 ft-lb/in

@Thickness 0.125 - 0.125 in
Average value: 0.875 J/cm Grade Count:2
Overview of materials for Acrylonitrile Butadiene Styrene (ABS), Transparent, Molded
This property data is a summary of similar materials in the MatWeb database for the category "Acrylonitrile Butadiene Styrene (ABS), Transparent, Molded". Each property range of values reported is m..
Izod Impact, Notched 0.350 - 1.30 J/cm
0.656 - 2.44 ft-lb/in
Average value: 0.771 J/cm Grade Count:23
Overview of materials for Polyarylamide, Glass Fiber Filled
This property data is a summary of similar materials in the MatWeb database for the category "Polyarylamide, Glass Fiber Filled". Each property range of values reported is minimum and maximum values..
Izod Impact, Notched 0.800 - 1.30 J/cm
1.50 - 2.44 ft-lb/in
Solvay Specialty Polymers Hylar® MP10 PVDF Polyvinylidene Fluoride  (discontinued **)
Data provided by the manufacturer.Hylar® polymers have the characteristic stability of fluoropolymers combined with a unique polarity that influences its solubility and electrical properties. In a..
Izod Impact, Notched 0.250 - 1.30 J/cm
0.468 - 2.44 ft-lb/in
Average value: 0.478 J/cm Grade Count:50
Overview of materials for Nylon 66, 40% Mineral Filled
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66, 40% Mineral Filled". Specific grades with primary filler content between 35% and 44% are inclu..
Izod Impact, Notched 0.800 - 1.30 J/cm

@Thickness 6.35 mm
1.50 - 2.44 ft-lb/in

@Thickness 0.250 in
ASTM D256
Chang Chun Plastic PBT3030 30% Glass Fiber Enforced PBT
Information provided by Dowell Trading Company Ltd.
Izod Impact, Notched 0.700 - 1.30 J/cm

@Thickness 6.35 mm
1.31 - 2.44 ft-lb/in

@Thickness 0.250 in
ASTM D256
Chang Chun Plastic PBT4830 Fire Retardant & 30% Glass Fiber Enforced Grade PBT
Information provided by Dowell Trading Company Ltd.
Izod Impact, Notched 0.700 - 1.30 J/cm

@Thickness 6.35 mm
1.31 - 2.44 ft-lb/in

@Thickness 0.250 in
ASTM D256
Chang Chun Plastic PBT4130 Fire Retardant & 30% Glass Fiber Enforced Grade PBT
Information provided by Dowell Trading Company Ltd.
Izod Impact, Notched 0.800 - 1.30 J/cm
1.50 - 2.44 ft-lb/in
Solvay Specialty Polymers Hylar® MP20 PVDF Polyvinylidene Fluoride  (discontinued **)
Data provided by the manufacturer.Hylar® polymers have the characteristic stability of fluoropolymers combined with a unique polarity that influences its solubility and electrical properties. In a..
Izod Impact, Notched 1.30 - 1.30 J/cm

@Temperature -40.0 - -40.0 °C
2.44 - 2.44 ft-lb/in

@Temperature -40.0 - -40.0 °F
Average value: 1.30 J/cm Grade Count:2
Overview of materials for Polypropylene, Glass Reinforced, Impact Modified
This property data is a summary of similar materials in the MatWeb database for the category "Polypropylene, Glass Reinforced, Impact Modified". Each property range of values reported is minimum and..
Izod Impact, Notched 0.400 - 1.30 J/cm

@Temperature -28.9 - -20.0 °C
0.749 - 2.44 ft-lb/in

@Temperature -20.0 - -4.00 °F
Average value: 0.854 J/cm Grade Count:5
Overview of materials for ABS/PVC Alloy
This property data is a summary of similar materials in the MatWeb database for the category "ABS/PVC Alloy". Each property range of values reported is minimum and maximum values of appropriate MatW..
Izod Impact, Notched 0.160 - 1.30 J/cm
0.300 - 2.44 ft-lb/in
Average value: 0.306 J/cm Grade Count:125
Overview of materials for Acrylic, Optical Grade, Molded
This property data is a summary of similar materials in the MatWeb database for the category "Acrylic, Optical Grade, Molded". Each property range of values reported is minimum and maximum values of..
Izod Impact, Notched 1.10 - 1.30 J/cm

@Temperature -20.0 - 0.000 °C
2.06 - 2.44 ft-lb/in

@Temperature -4.00 - 32.0 °F
Average value: 1.20 J/cm Grade Count:1
Overview of materials for Polypropylene, Long Glass Fiber 50%
This property data is a summary of similar materials in the MatWeb database for the category "Polypropylene, Long Glass Fiber 50%". Specific grades with glass content between 45% and 54% are include..