Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Izod Impact, Notched | 2.67 J/cm | 5.00 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics Cycolac® FR23 ABS (Asia Pacific) Flame retardant ABS (non-PBBE additives). Good properties/toughness. Excellent moldability. UL94 V-0 rated. |
|||
Izod Impact, Notched | 2.67 J/cm @Temperature 22.8 °C |
5.00 ft-lb/in @Temperature 73.0 °F |
ASTM D256 |
Polymer Resources PC-G5-IM Polycarbonate, 5% Glass Reinforced, Impact Modified, Foamable Polycarbonate, 5% Glass Reinforced, Impact Modified, FoamableProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Inf.. |
|||
Izod Impact, Notched | 2.67 J/cm | 5.00 ft-lb/in | ASTM D-256 |
PlastiComp Complet® LCF30-PA12 Nylon 12, 30% Long Carbon Fiber Content Complēt® long-fiber reinforced pellets are manufactured to exceed expectation for quality and performance.Nylon 12 with 30% long carbon fiber reinforcementInformation provided by PlastiComp, I.. |
|||
Izod Impact, Notched | 2.67 J/cm @Temperature -30.0 °C |
5.00 ft-lb/in @Temperature -22.0 °F |
ASTM D256 |
LTL Color Compounds Surlyn Reflection Series® SURSG201UG Surlyn Resin/Nylon 6 Alloy A patented alloy of DuPont™ Surlyn® resin and nylon 6 for applications that require a high gloss, molded in color surface finish directly from the mold.All information provided by LTL Color .. |
|||
Izod Impact, Notched | 2.67 J/cm @Temperature 23.0 °C |
5.00 ft-lb/in @Temperature 73.4 °F |
ASTM D 256 |
SABIC Innovative Plastics LNP Lubricomp FX00617 PE (Asia Pacific) LNP* Lubricomp* FX00617 is a compound based on Polyethylene resin containing Silicone. Added features of this material include: Internally Lubricated.This data was supplied by SABIC-IP for the Asia.. |
|||
Izod Impact, Notched | 2.67 J/cm @Thickness 3.20 mm |
5.00 ft-lb/in @Thickness 0.126 in |
reverse notched; ASTM D 256 |
SABIC Innovative Plastics Ultem 2313 PEI (Asia Pacific) 30% Milled glass filled, enhanced flow Polyetherimide (Tg 217C) with enhanced electroplatability. ECO Conforming, UL94 V0 and 5VA listing.This data was supplied by SABIC-IP for the Asia Pacific regi.. |
|||
Izod Impact, Notched | 2.67 J/cm @Thickness 3.17 mm |
5.00 ft-lb/in @Thickness 0.125 in |
ASTM D256 |
Techmer ES HiFill® TPU 0266 A Availability: North AmericaForms: PelletsFeatures: High Density and High Specific GravityInformation provided by TP Composites, Inc. |
|||
Izod Impact, Notched | 2.67 J/cm @Thickness 3.17 mm |
5.00 ft-lb/in @Thickness 0.125 in |
ASTM D256 |
Techmer ES HiFill® TPU 1000 Availability: North AmericaForms: PelletsFeatures: High DensityAppearance: BlackInformation provided by TP Composites, Inc. |
|||
Izod Impact, Notched | 2.67 J/cm @Thickness 3.17 mm |
5.00 ft-lb/in @Thickness 0.125 in |
ASTM D256 |
Techmer ES Statiblend® ABS AS Availability: North AmericaForms: PelletsAdditive: AntistaticFeatures: AntistaticInformation provided by TP Composites, Inc. |
|||
Izod Impact, Notched | 2.67 J/cm | 5.00 ft-lb/in | ASTM Data |
Styron Magnum™ 9095 ABS, High Gloss MAGNUM® ABS resins are thermoplastic materials which provide an excellent balance of processability, impact resistance and heat resistance as imparted by the various polymer compositions. MAGNUM .. |
|||
Izod Impact, Notched | 2.67 J/cm @Temperature -50.0 °C |
5.00 ft-lb/in @Temperature -58.0 °F |
ASTM Data |
Styron Pulse® 1350 ABS + Polycarbonate PULSE® 1350 Engineering resin offers a superior total performance with a balance of heat resistance, practical toughness, high and low temperature impact strength retention and ease of processing.. |
|||
Izod Impact, Notched | 2.67 J/cm @Thickness 3.17 mm |
5.00 ft-lb/in @Thickness 0.125 in |
ASTM D256 |
Techmer ES HiFill® TPU/E 0140 Availability: North AmericaForms: PelletsFeatures: High DensityInformation provided by TP Composites, Inc. |
|||
Izod Impact, Notched | 2.67 J/cm | 5.00 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics LNP VERTON MX02795 PP LNP* VERTON* MX02795 is a compound based on Polypropylene resin containing Proprietary Fillers. Added features of this material include: Heat Stabilized, UV Stabilized, Structural. |
|||
Izod Impact, Notched | 2.67 J/cm | 5.00 ft-lb/in | ASTM D256 |
A. Schulman POLYFORT™ FPP 3391 Chemically Coupled, Modified Polypropylene DescriptionPolyfort® FPP 3391 is a chemically coupled, mineral reinforced high impact resistant, modified polypropylene.Information provided by A. Schulman. |
|||
Izod Impact, Notched | 2.67 J/cm @Temperature 23.0 °C |
5.00 ft-lb/in @Temperature 73.4 °F |
ASTM D256A |
Formosa Plastics Formolene® 3302B Random Copolymer Polypropylene Random Copolymer for Extrusion and Thermoforming Applications Formolene® 3302B is a low melt flow random with excellent clarity, fast cycle time and easy mold release, designed for extrusion proces.. |
|||
Izod Impact, Notched | 2.67 J/cm | 5.00 ft-lb/in | ASTM D256; Depends on pigment |
Westlake Plastics Radel® R 4400 Polyphenylsulfone For Medical Applications Medical grade Radel R4400 resin offers exceptional hydrolytic stability, toughness, heat deflection temperature and resistance to stress cracking. This polymer also has excellent thermal stability,.. |
|||
Izod Impact, Notched | 2.67 J/cm | 5.00 ft-lb/in | ASTM D256 |
A. Schulman POLYFORT™ FPP 3391 Chemically Coupled, Modified Polypropylene DescriptionPolyfort® FPP 3391 is a chemically coupled, mineral reinforced high impact resistant, modified polypropylene.Information provided by A. Schulman. |
|||
Izod Impact, Notched | 2.67 J/cm | 5.00 ft-lb/in | ASTM D256 |
A. Schulman ComAlloy® 510-3010 10% Glass Fiber Reinforced Polycarbonate Information provided by A. Schulman.The ComAlloy product line has been integrated into the A Schulman product line. |
|||
Izod Impact, Notched | 2.67 J/cm | 5.00 ft-lb/in | ASTM D256 |
Ecomass® 1002TU96 Tungsten Powder Filled PEBA, Injection Molding Grade High Specific Gravity, Tungsten Powder Filled Polyether Block Amide (PEBA), Product Form - PelletsProcessing Method: Injection MoldingNontoxic alternative to Lead, weighting, balancing and radiatio.. |
|||
Izod Impact, Notched | 2.67 J/cm | 5.00 ft-lb/in | ASTM D256 |
Ecomass® 4703ZC76 Stainless Steel Filled Polyurethane Nontoxic alternative to Lead (Pb), weighting and balancing applicationsModerate Specific GravityStainless Steel Filled Polyurethane (TPU)FlexibleInformation provided by Technical Polymers |
|||
Izod Impact, Notched | 2.67 J/cm @Thickness 3.17 mm, Temperature 23.0 °C |
5.00 ft-lb/in @Thickness 0.125 in, Temperature 73.4 °F |
ASTM D256 |
Diamond Polymers ABS 3501 Natural 1002 ESCR Injection Molding Grade, Environmental Stress Crack Resistant Information Provided by Diamond Polymers, Inc. & Network Polymers, Inc. |
|||
Izod Impact, Notched | 2.67 J/cm @Thickness 3.17 mm, Temperature 23.0 °C |
5.00 ft-lb/in @Thickness 0.125 in, Temperature 73.4 °F |
ASTM D256 |
Diamond Polymers ABS 3501E Natural 1002 ESCR Extrusion Grade, Environmental Stress Crack Resistant Information Provided by Diamond Polymers, Inc. & Network Polymers, Inc. |
|||
Izod Impact, Notched | 2.67 J/cm @Thickness 3.17 mm, Temperature 23.0 °C |
5.00 ft-lb/in @Thickness 0.125 in, Temperature 73.4 °F |
bar; ASTM D256 |
Diamond Polymers ASA S710 Description: ASA Weatherable Polymer, Injection Molding Grade, High ImpactInformation provided by Diamond Polymers, Inc. |
|||
Izod Impact, Notched | 2.67 - 3.74 J/cm | 5.00 - 7.00 ft-lb/in | |
Bulk Molding Compounds BMC T9 General Purpose Molding Compound BMC T9 is a low cost, general purpose bulk molding compound designed for the electrical industry. It is UL listed and is used extensively in the manufacture of residential circuit breakers. BMC T9.. |
|||
Izod Impact, Notched | 2.67 J/cm | 5.00 ft-lb/in | ASTM D-256 |
PlastiComp Complet® LGF30 - PA66 Nylon 66, 30% Long Glass Fiber Reinforced Complēt® long-fiber reinforced pellets are manufactured to exceed expectation for quality and performance.Nylon 66 with 30% long glass fiber reinforcementInformation provided by PlastiComp, In.. |
|||
Izod Impact, Notched | 2.67 J/cm | 5.00 ft-lb/in | Low Temp; ASTM D256 |
DuPont Surlyn® SURSG201UG
(discontinued **) Surlyn Reflections® SG201UG is a modified ionomer resin for applications that require a high gloss, molded in color surface finish directly from the mold. The material is weatherable, durable and p.. |