Polymer Property : Izod Impact, Notched = 2.80 J/cm Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Izod Impact, Notched 2.80 J/cm
5.25 ft-lb/in
ASTM D256
SABIC Innovative Plastics Lexan® EXL4419 PC Copolymer
Lexan* EXL4419 polycarbonate (PC) siloxane copolymer resin is a 9% Glass Fiber (GF) reinforced opaque injection molding (IM) grade. This medium flow resin offers much higher ductility, improved rele..
Izod Impact, Notched 2.80 J/cm
5.25 ft-lb/in
ASTM D256
SABIC Innovative Plastics Lexan® EXL4419 PC Copolymer (Asia Pacific)
Lexan* EXL4419 polycarbonate (PC) siloxane copolymer resin is a 9% Glass Fiber (GF) reinforced opaque injection molding (IM) grade. This medium flow resin offers much higher ductility, improved rele..
Izod Impact, Notched 2.80 J/cm
5.25 ft-lb/in
ASTM D256
Glastic BMC SLC-1000 Glass-Reinforced Polyester
Data provided by Glastic Corporation.Medium strength, V-0, adjustable shrinkage.
Izod Impact, Notched 2.80 J/cm

@Thickness 3.17 mm
5.25 ft-lb/in

@Thickness 0.125 in
ASTM Test
Styrolution Luran® S 797 SE ASA
Luran S 797 SE is an extrusion ASA grade with especially high notched impact strength, used for sheet and profile extrusions. The data representable is based on extruded sheet.Information provided ..
Izod Impact, Notched 2.80 J/cm
5.25 ft-lb/in
ASTM D256
SABIC Innovative Plastics NORYL GTX GTX914 PPE+PA
NORYL GTX914 is an unfilled GTX grade with an ideal combination of impact performance, dimensional stability at elevated temperatures, chemical resistance and processability.
Izod Impact, Notched 2.80 J/cm
5.25 ft-lb/in
ASTM D256
SABIC Innovative Plastics NORYL GTX GTX914 PPE+PA (Asia Pacific)
NORYL GTX914 is an unfilled GTX grade with an ideal combination of impact performance, dimensional stability at elevated temperatures, chemical resistance and processability.
Izod Impact, Notched 2.80 J/cm
5.25 ft-lb/in
ASTM D256
SABIC Innovative Plastics NORYL GTX GTX914 PPE+PA (Europe-Africa-Middle East)
NORYL GTX914 is an unfilled GTX grade with an ideal combination of impact performance, dimensional stability at elevated temperatures, chemical resistance and processability.
Izod Impact, Notched 2.80 J/cm

@Temperature -30.0 °C
5.25 ft-lb/in

@Temperature -22.0 °F
ASTM D256
SABIC Innovative Plastics NORYL GTX GTX944 PPE+PA
NORYL GTX944 is an unfilled GTX grade with improved processability and increased impact performance.
Izod Impact, Notched 2.80 J/cm

@Temperature -30.0 °C
5.25 ft-lb/in

@Temperature -22.0 °F
ASTM D256
SABIC Innovative Plastics NORYL GTX GTX944 PPE+PA (Asia Pacific)
NORYL GTX944 is an unfilled GTX grade with improved processability and increased impact performance.
Izod Impact, Notched 2.80 J/cm

@Temperature -30.0 °C
5.25 ft-lb/in

@Temperature -22.0 °F
ASTM D256
SABIC Innovative Plastics NORYL GTX GTX944 PPE+PA (Europe-Africa-Middle East)
NORYL GTX944 is an unfilled GTX grade with improved processability and increased impact performance.
Izod Impact, Notched 2.80 J/cm
5.25 ft-lb/in
ASTM D256
A. Schulman POLYPUR™ FPU 1515 Thermoplastic Polyurethane Compound
Information provided by A. Schulman.
Izod Impact, Notched 2.80 J/cm
5.25 ft-lb/in
ASTM D256
A. Schulman POLYPUR™ FPU 1515 Thermoplastic Polyurethane Compound
Information provided by A. Schulman.
Izod Impact, Notched 2.80 J/cm

@Thickness 3.17 mm
5.25 ft-lb/in

@Thickness 0.125 in
ASTM D256
Unitika L-1003PA
Heat resistance, creep resistance, and excellent lubricantInformation provided by Unitika Ltd.
Izod Impact, Notched 2.80 J/cm
5.25 ft-lb/in
ASTM D256
A. Schulman POLYPUR™ FPU 1515 Thermoplastic Polyurethane Compound
Information provided by A. Schulman.
Izod Impact, Notched 2.80 J/cm
5.25 ft-lb/in
ASTM D256
A. Schulman POLYPUR™ FPU 1515 Thermoplastic Polyurethane Compound
Information provided by A. Schulman.
Izod Impact, Notched 2.80 J/cm
5.25 ft-lb/in
ASTM D256
A. Schulman POLYPUR™ FPU 1515 Thermoplastic Polyurethane Compound
Information provided by A. Schulman.
Izod Impact, Notched 2.80 J/cm
5.25 ft-lb/in
ASTM D256
A. Schulman POLYPUR™ FPU 1515 Thermoplastic Polyurethane Compound
Information provided by A. Schulman.