Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Izod Impact, Notched | 1.49 J/cm @Temperature 23.0 °C |
2.80 ft-lb/in @Temperature 73.4 °F |
ASTM D256 |
RheTech Products P252-670UV Polypropylene Copolymer, UV Stabilized, 134B Stone Applications: Interior trimElectrical housingsInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Izod Impact, Notched | 1.49 J/cm | 2.80 ft-lb/in | ASTM D256 |
Omni Plastics OmniLon™ 6/6 PA6/6 IM8 Unfilled/ Impact Modified Nylon Applications: Structural and appearance parts across industry segments including automotive, heavy truck fans, appliances, furniture, lawn and garden.Information provided by Omni Plastics |
|||
Izod Impact, Notched | 1.49 J/cm | 2.80 ft-lb/in | ASTM D256 |
Omni Plastics OmniTech™ HDPE GRC30 Glass Reinforced OmniTech™ is a family of non-standard products custom developed for applications with unique functional requirements, including but not limited to: Flame Retardant, Conductive, Wear Resistant, and .. |
|||
Izod Impact, Notched | 1.49 J/cm @Temperature 22.8 °C |
2.80 ft-lb/in @Temperature 73.0 °F |
ASTM D256 |
Polymer Resources NY6-G43 Nylon 6, 43% Glass Reinforced Nylon 6, 43% Glass Reinforced, LubricatedProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples. Nylon grades are teste.. |
|||
Izod Impact, Notched | 1.49 J/cm | 2.80 ft-lb/in | 0.25 in; ASTM D256 |
Ravago Manufacturing Americas Hylac® HF143 ABS Entec's proprietary products include a full range of compounds in the Nylon 6/6, Nylon 6, ABS, PBT, Polycarbonate, PC/ABS, PC/ASA, PC/PBT, and PPO/PPE resin families.Information provided by Rava.. |
|||
Izod Impact, Notched | 1.49 J/cm | 2.80 ft-lb/in | ASTM D256 |
Ravago Manufacturing Americas Enviramid™ N2335STHL BK Post Consumer Recycle Nylon 6, 35% Glass Filled Superior Toughness, Heat Stabilized, Lubricated, Black and made from EnViramid™ Post Consumer Recycled NylonInformation provided by Ravago. |
|||
Izod Impact, Notched | 1.50 J/cm @Thickness 3.17 mm |
2.80 ft-lb/in @Thickness 0.125 in |
ASTM D256 |
Lucent Polymers CPP-320 Polypropylene, 20% Calcium Carbonate Filled, Impact Modified Melt Flow Adjustable for ApplicationAdd "U" for UV StabilizedAdd "H" for Heat StabilizedInformation provided by Lucent Polymers, Inc. |
|||
Izod Impact, Notched | 1.50 J/cm @Thickness 3.17 mm |
2.80 ft-lb/in @Thickness 0.125 in |
ASTM D256 |
Lucent Polymers CPP-330 Polypropylene, 30% Calcium Carbonate Filled, Impact Modified Melt Flow Adjustable for ApplicationAdd "U" for UV StabilizedAdd "H" for Heat StabilizedInformation provided by Lucent Polymers, Inc. |
|||
Izod Impact, Notched | 1.50 J/cm @Thickness 3.17 mm |
2.80 ft-lb/in @Thickness 0.125 in |
ASTM D256 |
Lucent Polymers PPC-320 Polypropylene, Impact Modified Add "U" for UV StabilizedAdd "H" for Heat StabilizedInformation provided by Lucent Polymers, Inc. |
|||
Izod Impact, Notched | 1.49 J/cm @Thickness 3.17 mm |
2.80 ft-lb/in @Thickness 0.125 in |
ASTM D256 |
Techmer ES Elastoblend® PA6 GF20 IM2 BK 20% Glass Filled (Conditioned) Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 20% Filler by WeightAdditive: Heat Stabilizer, Impact Modifier and LubricantFeatures: Heat Stabilized, Impac.. |
|||
Izod Impact, Notched | 1.49 J/cm @Thickness 3.17 mm |
2.80 ft-lb/in @Thickness 0.125 in |
ASTM D256 |
Techmer ES HiFill FR® ABS FR BK Availability: North AmericaForms: PelletsFeatures: Flame RetardantAppearance: BlackTPCI# 9224121Information provided by TP Composites, Inc. |
|||
Izod Impact, Notched | 1.49 J/cm @Thickness 3.17 mm |
2.80 ft-lb/in @Thickness 0.125 in |
ASTM D256 |
Techmer ES HiFill® PA6 GF30 L UV 30% Glass Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 30% Filler by WeightProcessing Method: Injection MoldingInformation provided by TP Composites, Inc. |
|||
Izod Impact, Notched | 1.49 J/cm @Thickness 3.17 mm |
2.80 ft-lb/in @Thickness 0.125 in |
ASTM D256 |
Techmer ES HiFill® PA6 GF50 HS UV BK 50% Glass Filled (Dry) Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 50% Filler by WeightAdditive: Lubricant, UV Stabilizer and Heat StabilizerFeatures: Lubricated, Good UV Resi.. |
|||
Izod Impact, Notched | 1.49 J/cm @Thickness 3.17 mm |
2.80 ft-lb/in @Thickness 0.125 in |
ASTM D256 |
Techmer ES HiFill® PA6/6 GF35 L UV 35% Glass Filled (Conditioned) Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 35% Filler by WeightAdditive: Lubricant, UV Stabilizer and Heat StabilizerFeatures: Lubricated, Good UV Resi.. |
|||
Izod Impact, Notched | 1.49 J/cm @Thickness 3.17 mm |
2.80 ft-lb/in @Thickness 0.125 in |
ASTM D256 |
Techmer ES Luriblend® ABS TX15 Availability: North AmericaForms: PelletsAdditive: PTFE Lubricant(15%)Features: Lubricated and Good Wear ResistanceInformation provided by TP Composites, Inc. |
|||
Izod Impact, Notched | 1.49 J/cm | 2.80 ft-lb/in | ASTM D256 |
Teknor Apex Sinvicomp SIC 3710 Polyvinyl Chloride, Rigid Notes: RoHS Compliant Availability: Asia Pacific Features: High Impact ResistanceUses: Rigid Packing; Tubing Forms: Pellets Processing Method: ExtrusionInformation Provided by Teknor Apex |
|||
Izod Impact, Notched | 1.49 J/cm | 2.80 ft-lb/in | ASTM D256 |
A. Schulman SCHULAMID® 66 GF40H 40% Glass Fiber Reinforced, Heat Stabilized Nylon 66 Information provided by A. Schulman. |
|||
Izod Impact, Notched | 1.49 J/cm | 2.80 ft-lb/in | ASTM D256 |
A. Schulman SCHULAMID® 66 GF40H 40% Glass Fiber Reinforced, Heat Stabilized Nylon 66 Information provided by A. Schulman. |
|||
Izod Impact, Notched | 1.49 J/cm | 2.80 ft-lb/in | ASTM D256 |
A. Schulman SCHULAMID® 66 GF40H 40% Glass Fiber Reinforced, Heat Stabilized Nylon 66 Information provided by A. Schulman. |
|||
Izod Impact, Notched | 1.49 J/cm | 2.80 ft-lb/in | ASTM D256 |
Entec Hyrene® PS-HI 3/3 High Impact Polystyrene Available in North America Features: High Impact ResistanceRoHS Compliant Form: Pellets Information provided by Entec |
|||
Izod Impact, Notched | 1.49 J/cm | 2.80 ft-lb/in | ASTM D256 |
Clariant Renol PURSP0005 Polyurethane Elastomer, Glass Fiber Reinforced Data provided by Clariant Masterbatches |
|||
Izod Impact, Notched | 1.49 J/cm | 2.80 ft-lb/in | ASTM D256 |
Aclo Accutech Polypropylene Copolymer CP0437M30L Mica Reinforced |
|||
Izod Impact, Notched | 1.49 J/cm @Thickness 3.17 mm |
2.80 ft-lb/in @Thickness 0.125 in |
ASTM D256 |
Adell DR-16 30% Glass Reinforced Polycarbonate |
|||
Izod Impact, Notched | 1.49 J/cm | 2.80 ft-lb/in | ASTM D256 |
Omni Plastics OmniLon™ 6/6 PA6/6 GR20 IM10 Glass Reinforced/Impact Modified Nylon Applications: Structural and appearance parts across industry segments including automotive, heavy truck fans, appliances, furniture, lawn and garden.Information provided by Omni Plastics |