Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Izod Impact, Notched | 0.180 - 2.14 J/cm | 0.337 - 4.00 ft-lb/in | Average value: 0.563 J/cm Grade Count:25 |
Overview of materials for Polyphthalamide (PPA), 20% Glass Fiber Reinforced This property data is a summary of similar materials in the MatWeb database for the category "Polyphthalamide, 20% Glass Fiber Reinforced". Specific grades with glass content between 15% and 24% are.. |
|||
Izod Impact, Notched | 0.107 - 2.14 J/cm | 0.200 - 4.00 ft-lb/in | Average value: 0.596 J/cm Grade Count:13 |
Overview of materials for Epoxy Adhesive This property data is a summary of similar materials in the MatWeb database for the category "Epoxy Adhesive". Each property range of values reported is minimum and maximum values of appropriate Mat.. |
|||
Izod Impact, Notched | 0.107 - 2.14 J/cm | 0.200 - 4.00 ft-lb/in | Average value: 0.498 J/cm Grade Count:65 |
Overview of materials for Polystyrene, Molded, Unreinforced This property data is a summary of similar materials in the MatWeb database for the category "Polystyrene". Each property range of values reported is minimum and maximum values of appropriate MatWeb.. |
|||
Izod Impact, Notched | 0.961 - 2.14 J/cm | 1.80 - 4.00 ft-lb/in | Average value: 1.40 J/cm Grade Count:7 |
Overview of materials for Nylon 11 + Carbon Fiber This property data is a summary of similar materials in the MatWeb database for the category "Nylon 11 + Carbon Fiber". Each property range of values reported is minimum and maximum values of approp.. |
|||
Izod Impact, Notched | 1.07 - 2.14 J/cm | 2.00 - 4.00 ft-lb/in | ASTM D256 |
Mar-Bal MB2000-8 Thermoset Polyester Composite Molding Compound An excellent flame and track resistant material with excellent electrical and mechanical properties. Good dielectric strength and low shrink for close dimensional control.Mar-Bal standard grades can.. |
|||
Izod Impact, Notched | 1.07 - 2.14 J/cm | 2.00 - 4.00 ft-lb/in | ASTM D256 |
Arkema Group KYNAR® 740 Black/Red Polyvinylidene Fluoride Homopolymer - Injection Molding and Extrusion Characteristics: Pigmented. High stability in harsh thermal, chemical and ultraviolet environments. High toughness and mechanical strength, low permeability, abrasion resistance; high purityAppli.. |
|||
Izod Impact, Notched | 1.07 - 2.14 J/cm | 2.00 - 4.00 ft-lb/in | ASTM D256 |
Arkema Group KYNAR® 740 Polyvinylidene Fluoride Homopolymer - Injection Molding and Extrusion Characteristics: Natural resin - translucent, off-white hemispheres. High stability in harsh thermal, chemical and ultraviolet environments. High toughness and mechanical strength, low permeabili.. |
|||
Izod Impact, Notched | 1.07 - 2.14 J/cm | 2.00 - 4.00 ft-lb/in | ASTM D256 |
Arkema Group KYNAR® 740-02 Polyvinylidene Fluoride Homopolymer - Injection Molding and Extrusion Characteristics: Natural resin - translucent, off-white hemispheres. Flame and smoke suppressant. High stability in harsh thermal, chemical and ultraviolet environments. High toughness and mecha.. |
|||
Izod Impact, Notched | 1.07 - 2.14 J/cm | 2.00 - 4.00 ft-lb/in | ASTM D256 |
Arkema Group KYNAR® 760 Polyvinylidene Fluoride Homopolymer - Extrusion Characteristics: Natural resin - translucent, off-white hemispheres. High stability in harsh thermal, chemical and ultraviolet environments. High toughness and mechanical strength, low permeabili.. |
|||
Izod Impact, Notched | 1.07 - 2.14 J/cm | 2.00 - 4.00 ft-lb/in | |
Bulk Molding Compounds BMC 100 Thermoset Polyester, GP BMC 100 is a high strength, low shrink general purpose molding compound. It can be supplied in bulk or extruded in pre-weighted slugs. Due to the excellent flow and controlled reactivity, BMC 100 is.. |
|||
Izod Impact, Notched | 1.07 - 2.14 J/cm | 2.00 - 4.00 ft-lb/in | |
Bulk Molding Compounds BMC 102 Glass Filled Thermoset Polyester BMC 102 is a medium strength, glass fiber reinforced molding compound that meets Ford Specification ESF-M3D56-A. It can be supplied in bulk or extruded in pre-weighed slugs and is well suited for in.. |
|||
Izod Impact, Notched | 1.60 - 2.14 J/cm | 3.00 - 4.00 ft-lb/in | |
Bulk Molding Compounds BMC 1403 Electrical Grade BMC 1403 is one of the most useful general-purpose electrical grade materials available on the market. Competitive against phenolic, melamine, and urea materials for electrical applications. Easy mo.. |
|||
Izod Impact, Notched | 1.60 - 2.14 J/cm | 3.00 - 4.00 ft-lb/in | |
Bulk Molding Compounds BMC 2270 Mineral Filled, Glass Reinforced Polyester BMC 2270 molding compound is a mineral filled, glass-fiber-reinforced polyester compound suitable for compression and transfer molding. It is a general purpose material with medium impact strength a.. |
|||
Izod Impact, Notched | 1.07 - 2.14 J/cm | 2.00 - 4.00 ft-lb/in | |
Bulk Molding Compounds BMC 5436 Mineral Filled, Glass Reinforced Polyester BMC 5436 molding compound is a low cost, mineral filled, glass-fiber-reinforced polyester compound suitable for compression, transfer and stuffer injection molding. It is characterized by good molda.. |
|||
Izod Impact, Notched | 1.07 - 2.14 J/cm | 2.00 - 4.00 ft-lb/in | |
Bulk Molding Compounds BMC 600 Mineral Filled, Glass Fiber Reinforced Polyester Compound BMC 600 molding compound is a mineral filled glass-fiber-reinforced polyester compound suitable for compression, transfer and stuffer injection molding. It is a general purpose material with medium .. |
|||
Izod Impact, Notched | 1.07 - 2.14 J/cm | 2.00 - 4.00 ft-lb/in | |
Bulk Molding Compounds BMC 600LS Mineral Filled, Glass Fiber Reinforced Polyester Compound BMC 600LS molding compound is a low-shrink, Mineral filled, glass-fiber-reinforced polyester compound suitable for compression, transfer and stuffer injection molding It is a general purpose materia.. |
|||
Izod Impact, Notched | 1.07 - 2.14 J/cm | 2.00 - 4.00 ft-lb/in | |
Bulk Molding Compounds BMC 604 Mineral Filled, Glass Fiber Reinforced Polyester Compound BMC 604 molding compound is a low-cost, mineral filled glass-fiber-reinforced polyester compound suitable for compression, transfer and stuffer injection molding It is a general purpose material wit.. |
|||
Izod Impact, Notched | 1.07 - 2.14 J/cm | 2.00 - 4.00 ft-lb/in | |
Bulk Molding Compounds BMC 605L Mineral Filled, Glass Fiber Reinforced Polyester Compound BMC 605L molding compound is a low cost, mineral filled, glass-fiber-reinforced polyester compound suitable for compression, transfer and stuffer injection molding. It is characterized by good molda.. |
|||
Izod Impact, Notched | 1.07 - 2.14 J/cm | 2.00 - 4.00 ft-lb/in | |
Bulk Molding Compounds BMC 610 - SP Mineral Filled, Glass Reinforced Polyester Compound, with UV Stabilizer BMC 610 molding compound is a mineral filled, glass fiber-reinforced polyester compound suitable for compression, transfer and stuffer injection molding. It is set a part form other medium impact el.. |
|||
Izod Impact, Notched | 1.07 - 2.14 J/cm | 2.00 - 4.00 ft-lb/in | ASTM D256 |
Arkema Group KYNAR® 460 Polyvinylidene Fluoride Homopolymer - Extrusion Characteristics: Natural resin - translucent, off-white hemispheres. Broad molecular weight distribution. High stability in harsh thermal, chemical and ultraviolet environments. High toughness a.. |
|||
Izod Impact, Notched | 1.07 - 2.14 J/cm | 2.00 - 4.00 ft-lb/in | ASTM D256 |
Arkema Group KYNAR® 720, 720 HDP Polyvinylidene Fluoride Homopolymer- Injection Molding and Extrusion Characteristics: Natural resin - translucent, off-white hemispheres. HDP indicates higher color stability. High stability in harsh thermal, chemical and ultraviolet environments. High toughness .. |
|||
Izod Impact, Notched | 1.60 - 2.14 J/cm | 3.00 - 4.00 ft-lb/in | |
Bulk Molding Compounds BMC 1423 Wear Resistant, Electrical Grade BMC 1423 is a wear-resistant electrical grade material used in applications where there are moving parts. Best anti-wear properties are exhibited when used in conjunction with mating parts molded fr.. |
|||
Izod Impact, Notched | 1.07 - 2.14 J/cm | 2.00 - 4.00 ft-lb/in | |
Bulk Molding Compounds BMC 1901 Mineral Filled Alkyd BMC 1901 molding compound is a mineral filled, glass-fiber-reinforced alkyd compound suitable for compression transfer molding. It is a general purpose with medium impact strength and good overall e.. |
|||
Izod Impact, Notched | 1.07 - 2.14 J/cm | 2.00 - 4.00 ft-lb/in | |
Bulk Molding Compounds BMC 200 Thermoset Polyester, Electrical Grade BMC 200 is a high strength, low shrink molding compound. It can be supplied in bulk or extruded in pre-weighted slugs.Typical applications are circuit breakers, insulators, bobbins, electrical conne.. |
|||
Izod Impact, Notched | 1.07 - 2.14 J/cm | 2.00 - 4.00 ft-lb/in | |
Bulk Molding Compounds BMC 2201 Mineral Filled Alkyd BMC 2201 molding compound is a mineral filled, glass-fiber-and nylon-floc reinforced alkyd compound suitable for compression and transfer molding. It was developed for applications requiring better .. |
|||
Izod Impact, Notched | 1.07 - 2.14 J/cm | 2.00 - 4.00 ft-lb/in | |
Bulk Molding Compounds BMC 2274 Mineral Filled, Glass Reinforced Polyester BMC 2274 molding compound is a mineral filled, glass-fiber-reinforced polyester compound suitable for compression transfer and stuffer injection molding. It is a general-purpose material with medium.. |
|||
Izod Impact, Notched | 1.07 - 2.14 J/cm | 2.00 - 4.00 ft-lb/in | |
Bulk Molding Compounds BMC 610 Mineral Filled, Glass Reinforced Polyester Compound BMC 610 molding compound is a mineral filled, glass fiber-reinforced polyester compound suitable for compression, transfer and stuffer injection molding. It is set a part form other medium impact el.. |
|||
Izod Impact, Notched | 0.214 - 2.14 J/cm | 0.400 - 4.00 ft-lb/in | Average value: 0.673 J/cm Grade Count:190 |
Overview of materials for Polyethersulfone (PES) This property data is a summary of similar materials in the MatWeb database for the category "Polyethersulfone". Each property range of values reported is minimum and maximum values of appropriate M.. |
|||
Izod Impact, Notched | 0.518 - 2.14 J/cm | 0.970 - 4.00 ft-lb/in | Average value: 1.24 J/cm Grade Count:30 |
Overview of materials for Polypropylene, Glass Reinforced, Impact Modified This property data is a summary of similar materials in the MatWeb database for the category "Polypropylene, Glass Reinforced, Impact Modified". Each property range of values reported is minimum and.. |
|||
Izod Impact, Notched | 0.320 - 2.14 J/cm | 0.600 - 4.00 ft-lb/in | Average value: 0.644 J/cm Grade Count:22 |
Overview of materials for Polybutylene Terephthalate (PBT), Carbon Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Polybutylene Terephthalate (PBT), Carbon Fiber Filled". Each property range of values reported is minimu.. |