Mechanical Properties Metric English Comments
Izod Impact, Notched 2.25 J/cm

@Temperature 23.0 °C
4.22 ft-lb/in

@Temperature 73.4 °F
ASTM D256
Reliance Industries Repol C015EG Polypropylene
REPOL Polypropylene C015EG is manufactured using Unipol PP process which combines the production efficiency of gas phase fluidized bed reactor technology with the high activity stereospecific cataly..
Izod Impact, Notched 2.26 J/cm
4.22 ft-lb/in
ASTM D256
SK Chemicals SKYPEL P128DW Productivity Grade
SKYPEL is a thermoplastic polyester elastomer (TPEE). It is a polymer resin having the property somewhere between plastics and rubber, which have various properties ranging from high hardness plasti..
Izod Impact, Notched 2.26 J/cm

@Thickness 6.35 mm
4.22 ft-lb/in

@Thickness 0.250 in
ASTM D256
Samsung Cheil Industries Starex® VH-0810 ABS, Unreinforced FR
Flame-retardant ABS with excellent weather resistance that is used in the exterior of OA devices such as monitors, printers, fax machines, duplicators etc.Information provided by Samsung Cheil Indus..
Izod Impact, Notched 2.26 J/cm
4.22 ft-lb/in
ASTM D256
SK Chemicals SKYPEL G168D General Grade
SKYPEL is a thermoplastic polyester elastomer (TPEE). It is a polymer resin having the property somewhere between plastics and rubber, which have various properties ranging from high hardness plasti..
Izod Impact, Notched 2.26 J/cm

@Thickness 6.35 mm
4.22 ft-lb/in

@Thickness 0.250 in
ASTM D256
Samsung Cheil Industries Starex® VH-0810 ABS, Unreinforced FR
Flame-retardant ABS with excellent weather resistance that is used in the exterior of OA devices such as monitors, printers, fax machines, duplicators etc.Information provided by Samsung Cheil Indus..
Izod Impact, Notched 2.25 J/cm

@Thickness 3.17 mm
4.22 ft-lb/in

@Thickness 0.125 in
ASTM D256
Unitika U-100 Engineering Plastic
CAS No: 26590-50-1Information provided by Unitika Ltd.
Izod Impact, Notched 2.25 J/cm

@Thickness 3.17 mm
4.22 ft-lb/in

@Thickness 0.125 in
ASTM D256
Diamond Polymers NPP25-0504LGF40 40% Long Glass Fiber Filled Copolymer Polypropylene
Information Provided by Diamond Polymers, Inc. & Network Polymers, Inc.
Izod Impact, Notched 2.25 J/cm
4.22 ft-lb/in
ASTM-D256
Braskem GF4960 HDPE Blow Molding Polyethylene Homopolymer
GF 4960 is a high-density polyethylene homopolymer with high density and stiffness combined with high impact resistance. It was developed for the blow-molding segment. It is used in containers for y..
Izod Impact, Notched 2.25 J/cm

@Thickness 3.17 mm
4.22 ft-lb/in

@Thickness 0.125 in
ASTM Test
BASF Ultramid® TG7S 35% Glass Filled PA6 (Dry)
Ultramid TG7S is a 34% glass reinforced, heat stabilized, impact modified PA6 injection molding grade. It was developed to meet the demanding requirements of the first North American seat cushion ..
Izod Impact, Notched 2.25 J/cm
4.22 ft-lb/in
ASTM D256
Eastman Tenite Propionate 350E0096914 Natural, Trsp Cellulose Acetate Propionate
Plasticizer 12%. Weight loss on heating = 0.5% per ASTM D 707. Soluble matter loss = 0.1% per ASTM D 570.Product Description: TENITE cellulosic plastics are noted for their excellent balance of p..
Izod Impact, Notched 2.25 J/cm
4.22 ft-lb/in
ASTM D256
Braskem Green PE SGF4960 Blow Molding and Monofilament High Density Polyethylene
Description: SGF4960 is a homopolymer high-density polyethylene, developed for the blow-molding segment with high density and stiffness combined with high impact resistance. The minimum biobased con..