Mechanical Properties Metric English Comments
Izod Impact, Notched 1.60 - 2.40 J/cm
3.00 - 4.50 ft-lb/in
Average value: 2.25 J/cm Grade Count:10
Overview of materials for Diallyl Phthalate (DAP) Molding Compound, Long Glass Fiber Filled
This property data is a summary of similar materials in the MatWeb database for the category "Diallyl Phthalate (DAP) Molding Compound, Long Glass Fiber Filled". Each property range of values report..
Izod Impact, Notched 0.149 - 2.40 J/cm
0.280 - 4.50 ft-lb/in
Average value: 0.528 J/cm Grade Count:67
Overview of materials for Polypropylene with 30% Talc Filler
This property data is a summary of similar materials in the MatWeb database for the category "Polypropylene with 30% Talc Filler". Specific grades with primary filler content between 25% and 34% are..
Izod Impact, Notched 0.267 - 2.40 J/cm
0.500 - 4.50 ft-lb/in
Average value: 1.16 J/cm Grade Count:33
Overview of materials for Nylon 6, Glass Fiber/Solid Lube Filled
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 6, Glass Fiber/Solid Lube Filled". Each property range of values reported is minimum and maximum v..
Izod Impact, Notched 0.534 - 2.40 J/cm
1.00 - 4.50 ft-lb/in
Average value: 1.31 J/cm Grade Count:18
Overview of materials for Nylon 66, 30% Carbon Fiber Filled
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66, 30% Carbon Fiber Filled". Specific grades with carbon fiber content between 25% and 34% are in..
Izod Impact, Notched 0.320 - 2.40 J/cm
0.600 - 4.50 ft-lb/in
Average value: 0.882 J/cm Grade Count:64
Overview of materials for Nylon 66, Carbon Fiber/PTFE Filled
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66, Carbon Fiber/PTFE Filled". Each property range of values reported is minimum and maximum value..
Izod Impact, Notched 1.71 - 2.40 J/cm
3.20 - 4.50 ft-lb/in
ASTM D256
Westlake Plastics Ultra Ethylux® HDPE
Ultra Ethylux is made from high density polyethylene resin. This material is a cost effective alternative for a variety of end uses including mild chemical and wear applications. Information provid..
Izod Impact, Notched 2.30 - 2.40 J/cm
4.30 - 4.50 ft-lb/in
Bulk Molding Compounds BMC G10(12) Mineral Filled, Glass Fiber Reinforced Polyester
BMC G10 is a general purpose, mineral filled, glass fiber-reinforced polyester that is suitable for compression, transfer and stuffer injection molding. G10 is well suited to applications where hig..
Izod Impact, Notched 0.112 - 2.40 J/cm
0.210 - 4.50 ft-lb/in
Average value: 0.914 J/cm Grade Count:79
Overview of materials for Polyetheretherketone, Glass Fiber Filled
This property data is a summary of similar materials in the MatWeb database for the category "Polyetheretherketone, Glass Fiber Filled". Each property range of values reported is minimum and maximum..