Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Izod Impact, Notched = 6.56 ft-lb/in Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Izod Impact, Notched 3.50 J/cm

@Thickness 3.17 mm
6.56 ft-lb/in

@Thickness 0.125 in
ASTM D256
Polimeri Europa SINKRAL G320 ABS  (discontinued **)
Symbol according to ISO 1043-1: ABS Grade designation according to ISO 2580-ABS 1,MG,095-15-16-25 General purpose injection moulding grade with good impact resistance, good flow and high gloss. SI..
Izod Impact, Notched 3.50 J/cm

@Temperature 0.000 °C
6.56 ft-lb/in

@Temperature 32.0 °F
ASTM D256
Gichem GIBLEND F70500 Polycarbonate / ABS  (discontinued **)
Polycarbonate and ABS blend, excellent mechanical and thermal properties, very high fluidity. Medium Injection speed.Information provided by GICHEM Gruppo Industriale Chimico
Izod Impact, Notched 3.50 J/cm
6.56 ft-lb/in
ASTM D256
Gichem GIBLEND E45X3/VO ABS - Polycarbonate - PC/ABS Flame Retardant  (discontinued **)
Blend PC-ABS self-extinguishing class V0 medium fluidity. Medium injection speed.Information provided by GICHEM Gruppo Industriale Chimico
Izod Impact, Notched 3.50 J/cm
6.56 ft-lb/in
ASTM D256
Solvay Specialty Polymers Ixef® BXT-2000/0203 Polyarylamide (PARA)  (Unverified Data**)
Ixef BXT-2000/0203 resin was developed specifically for extrusion and blow-molding processes. Unlike grades targeted for injection molding, Ixef BXT-2000/0203 resin can be successfully extruded into..
Izod Impact, Notched 3.50 J/cm

@Temperature 23.0 °C
6.56 ft-lb/in

@Temperature 73.4 °F
ASTM D256
Flint Hills 44S2A Polypropylene Impact Copolymer
Features: Phosphorus free additive package for silicon coated applications. Product does not contain animal derived components.Applications: Extrusion: blown and cast filmInformation Provided by Fl..
Izod Impact, Notched 3.50 J/cm
6.56 ft-lb/in
Reverse notched; ASTM D256
LG Chemical LUCEL CF-620 Electrically Conductive POM, 20% Carbon Fiber Filled, High Strength, Wear Resistant
LUCEL semi-crystalline acetal copolymer resins are produced by gas phase polymerization. LUCEL resins can be widely accepted as the replacement of thermosets, aluminum and zinc die-casts or other m..
Izod Impact, Notched 3.50 J/cm
6.56 ft-lb/in
Reverse notched; ASTM D256
LG Chemical LUCEL GB-325 Low Warpage POM, 25% Glass Bead Filled
LUCEL semi-crystalline acetal copolymer resins are produced by gas phase polymerization. LUCEL resins can be widely accepted as the replacement of thermosets, aluminum and zinc die-casts or other m..
Izod Impact, Notched 3.50 J/cm
6.56 ft-lb/in
Reverse notched; ASTM D256
LG Chemical LUCEL MR-320 Low Warpage POM, 20% Mineral Filled
LUCEL semi-crystalline acetal copolymer resins are produced by gas phase polymerization. LUCEL resins can be widely accepted as the replacement of thermosets, aluminum and zinc die-casts or other m..
Izod Impact, Notched 3.50 J/cm
6.56 ft-lb/in
ASTM D256A
LyondellBasell Astryn BE17FC Polypropylene Copolymer, 40% Calcium Carbonate
Key Features: fractional melt flow, medium high modulus, UV-stabilized, mineral-filled, blow molding and extrusion grade polypropylene copolymer, excellent impact and stiffness balance, good melt st..
Izod Impact, Notched 3.50 J/cm

@Thickness 3.20 mm
6.56 ft-lb/in

@Thickness 0.126 in
ASTM D256
SABIC Innovative Plastics ULTEM 2110EPR PEI (Asia Pacific)
10% Glass fiber filled, high flow Polyetherimide (Tg 217C) with internal mold release and enhanced electroplatability. ECO Conforming, UL94 V0 and 5VA listing.
Izod Impact, Notched 3.50 J/cm
6.56 ft-lb/in
ASTM D256
Solvay Specialty Polymers Ixef® BXT 2000-0203 Polyarylamide (PARA)
Ixef® BXT 2000-0203 resin was developed specifically for extrusion and blow-molding processes. Unlike grades targeted for injection molding, Ixef® BXT 2000-0203 resin can be successfully extru..
Izod Impact, Notched 3.50 J/cm
6.56 ft-lb/in
ASTM D256
SPS Guang Zhou POPTREEâ„¢ 6001 Flame-retarded Polyethylene
Characteristic: Low density, superior melt flow index, high notched impact strengthApplications: X'mas decorative productInformation Provided by SPS (Guang Zhou) Ltd.
Izod Impact, Notched 3.50 J/cm

@Temperature 23.0 °C
6.56 ft-lb/in

@Temperature 73.4 °F
ASTM-D256
Polyram PlusTek RA845 Nylon 6.6, Impact Modified
Improved impact polyamide 6.6 for good resistance to low temp for injection molding applicationsInformation provided by Polyram Ram On Ind.
Izod Impact, Notched 3.50 J/cm

@Temperature 23.0 °C
6.56 ft-lb/in

@Temperature 73.4 °F
ASTM-D256
Polyram Polytron P50B03 Copolymer Polypropylene, Chemically Coupled 50% Long Glass Fiber
A CHEMICALLY COUPLED 50% LONG GLASS FIBER REINFORCED BLACK POLYPROPYLENE HEAT STABILIZED FOR INJECTION MOLDING APPLICATION.These products have significantly improved impact performance characteristi..
Izod Impact, Notched 3.50 J/cm

@Temperature 23.0 °C
6.56 ft-lb/in

@Temperature 73.4 °F
ASTM-D256
Polyram RamLloy PBB520 PC/ABS alloy, Flame Retardant
Flame retardant PC/ABS alloy for injection molding applicationsInformation provided by Polyram Ram On Ind.
Izod Impact, Notched 3.50 J/cm
6.56 ft-lb/in
ASTM-D256
Braskem GP100OR HDPE High Density Extrusion Polyethylene
GP100OR is a high-density polyethylene compound specially developed for the manufacturing of extruded pipes for gas distribution. It is produced with bimodal technology and has high molar mass. It s..
Izod Impact, Notched 3.50 J/cm
6.56 ft-lb/in
ASTM D256
Sumitomo Bakelite North America FS-80-P-1 Long-Glass Reinforced Diallyl Phthalate
Isophthalate DAP Resin Isomer. Used for critical, high-performance military and commercial electrical components where long-term reliability is demanded.Meets the requirements of ASTM D5948 Type GI..
Copyright © lookpolymers.com All Rights Reserved