Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Izod Impact, Notched | 6.94 J/cm | 13.0 ft-lb/in | ASTM D256 |
Nylene® Naxel™ PC1210 Polycarbonate Description: Naxel™ PC1210 is a 6 melt, general purpose polycarbonate. Information provided by Custom Resins. ALM, Nylene Canada, and Custom Resins are all operting companies of Polymeric Resources.. |
|||
Izod Impact, Notched | 6.94 J/cm | 13.0 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics Cycoloy® C3650 PC+ABS Flame retardant PC/ABS blend using non-brominated and non-chlorinated flame retardant systems, offering high impact and excellent extrusion and thermoforming characteristics. Halogen free according .. |
|||
Izod Impact, Notched | 6.94 J/cm | 13.0 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics Lexan® 121 PC UL rated HB as of 10/97. 200 series recommended when V-2 rating required. Nonhalogenated. 17.5 MFR, for small intricate parts. |
|||
Izod Impact, Notched | 6.94 J/cm | 13.0 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics Lexan® 121R PC UL rated HB as of 10/97. 200 series recommended when V-2 rating required. Nonhalogenated. 17.5 MFR, for small, intricate parts. Internal mold release. |
|||
Izod Impact, Notched | 6.94 J/cm | 13.0 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics Lexan® 121R PC (Asia Pacific) Nonhalogenated. 17.5 MFR, for small, intricate parts. Internal mold release. |
|||
Izod Impact, Notched | 6.94 J/cm | 13.0 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics Lexan® 123R PC UL rated HB as of 10/97. 200 series recommended when V-2 rating required. Nonhalogenated. 17.5 MFR, for small, intricate parts. UV stabilized. Internal mold release. |
|||
Izod Impact, Notched | 6.94 J/cm | 13.0 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics Lexan® 124 PC (Asia Pacific) 17.5 MFR, for small, intricate parts. FDA food contact compliant in limited colors. Effective January 15th, 2007 this grade is no longer supported with biocompatibility information and should not .. |
|||
Izod Impact, Notched | 6.94 J/cm @Temperature 22.8 °C |
13.0 ft-lb/in @Temperature 73.0 °F |
ASTM D256 |
Polymer Resources PC-FD3 Polycarbonate, FDA-compliant Feedstocks, High Flow, Gamma Resistant Polycarbonate, FDA-compliant Feedstocks, High Flow, Gamma ResistantProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test sampl.. |
|||
Izod Impact, Notched | 6.94 J/cm @Temperature -30.0 °C |
13.0 ft-lb/in @Temperature -22.0 °F |
ASTM D256 |
SABIC Innovative Plastics Lexan® EM1210 PC (Asia Pacific) Automotive interiors. Excellent heat/impact resistance and outstanding property retention over wide temperature range/severe automotive conditions |
|||
Izod Impact, Notched | 6.94 J/cm @Temperature 22.8 °C |
13.0 ft-lb/in @Temperature 73.0 °F |
ASTM D256 |
Polymer Resources PC-GP3-D-[color]-5 Polycarbonate, FDA-compliant Feedstocks, High Flow Polycarbonate, FDA-compliant Feedstocks, High FlowProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Information pr.. |
|||
Izod Impact, Notched | 6.94 J/cm @Temperature -30.0 °C |
13.0 ft-lb/in @Temperature -22.0 °F |
ASTM D256 |
SABIC Innovative Plastics Lexan® EXL6414 PC PC-Siloxane copolymer with excellent processability. Impact modified, medium flow, extreme low temp. ductility. |
|||
Izod Impact, Notched | 6.94 J/cm | 13.0 ft-lb/in | 73°F, 0.125 in; ASTM D256 |
Ravago Manufacturing Americas Hybrid B3030U Polycarbonate + PBT Alloy Entec's proprietary products include a full range of compounds in the Nylon 6/6, Nylon 6, ABS, PBT, Polycarbonate, PC/ABS, PC/ASA, PC/PBT, and PPO/PPE resin families.Information provided by Rava.. |
|||
Izod Impact, Notched | 6.94 J/cm | 13.0 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics Lexan® HP2JP PC (Asia Pacific) Med/high flow polycarbonate. For medical devices and pharmaceutical applications. Healthcare management of change, biocompatible (ISO10993 or USP Class VI). EtO and steam sterilizable. Contains m.. |
|||
Izod Impact, Notched | 6.94 J/cm | 13.0 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics Lexan® HP2NR PC (Europe-Africa-Middle East) Med/high flow polycarbonate. For medical devices and pharmaceutical applications. Healthcare management of change, biocompatible (ISO10993 or USP Class VI). EtO and steam sterilizable. Contains no.. |
|||
Izod Impact, Notched | 6.94 J/cm | 13.0 ft-lb/in | natural, tints; ASTM D256 |
SABIC Innovative Plastics Lexan® HPS2R PC Med/high flow polycarbonate. For medical devices and pharmaceutical applications. Healthcare management of change, biocompatible (ISO10993 or USP Class VI). EtO, steam, e-beam and gamma sterilizable.. |
|||
Izod Impact, Notched | 6.94 J/cm | 13.0 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics Lexan® LI1813R PC Low-viscosity multi-purpose PC having low levels of ionics species. Internal mold release and UV-stabilized. |
|||
Izod Impact, Notched | 6.94 J/cm | 13.0 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics Lexan® LI1911R PC Low-viscosity multi-purpose PC having low levels of ionics species. Internal mold release. |
|||
Izod Impact, Notched | 6.94 J/cm | 13.0 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics Lexan® HP2NR PC (Asia Pacific) Med/high flow polycarbonate. For medical devices and pharmaceutical applications. Healthcare management of change, biocompatible (ISO10993 or USP Class VI). EtO and steam sterilizable. Contains no.. |
|||
Izod Impact, Notched | 6.94 J/cm | 13.0 ft-lb/in | ASTM D256 |
Premix Premi-Glas® 2200-22 Fiberglass Reinforced SMC
(discontinued **) Description: Premi-Glas® 2200-22 is a fiberglass reinforced thermoset Sheet Molding Compound similar to the Premi-Glas® 2200-22 CR-SX product. Unlike the -CR-SX version, this product carries no UL.. |
|||
Izod Impact, Notched | 6.94 J/cm @Temperature 22.8 °C |
13.0 ft-lb/in @Temperature 73.0 °F |
ASTM D256 |
LTL Color Compounds ColorFast® PC150 Polycarbonate 15 melt high flow polycarbonateAll information provided by LTL Color Compounders, Inc. |
|||
Izod Impact, Notched | 6.94 J/cm @Temperature 0.000 °C |
13.0 ft-lb/in @Temperature 32.0 °F |
ASTM D256 |
SABIC Innovative Plastics Xenoy® 1102 PBT+PC (Asia Pacific) Unreinforced PC/polyester alloy. Excellent low temperatue impact/chemical resistance to automotive fluids. |
|||
Izod Impact, Notched | 6.94 J/cm | 13.0 ft-lb/in | 73°F, 0.125 in.; ASTM D256 |
Star Plastics PC721HFR Molding Grade PC High Flow with Release Information provided by Star Plastics, Inc. |
|||
Izod Impact, Notched | 6.94 J/cm | 13.0 ft-lb/in | 73°F; ASTM D256 |
Styron EMERGEâ„¢ 4410-11 MFR Polycarbonate EMERGEâ„¢ PC 4410-11 advanced resin is a high impact polycarbonate resin designed for Information Technology Equipment and Injection Molding Applications.Information provided by DowThis product l.. |
|||
Izod Impact, Notched | 6.94 J/cm | 13.0 ft-lb/in | ASTM D256 |
Styron EMERGEâ„¢ 4850-10 Polycarbonate EMERGEâ„¢ 4850-10 advanced resin provides superior ignition resistance and ultraviolet light resistance in opaque applications. It has an f1 rating by Underwriters Laboratories Inc. Physical pr.. |
|||
Izod Impact, Notched | 6.94 J/cm | 13.0 ft-lb/in | ASTM D256 |
Styron EMERGEâ„¢ 4800-19 Polycarbonate EMERGEâ„¢ 4800-19 advanced resin provides superior ignition resistance in opaque, injection molding applications. Physical properties and process-ability are outstanding for this class of polyca.. |
|||
Izod Impact, Notched | 6.94 J/cm | 13.0 ft-lb/in | ASTM D256 |
Clariant Renol PCSP0016BL-201 Polycarbonate/Polyester Alloy Data provided by Clariant Masterbatches |
|||
Izod Impact, Notched | 6.94 J/cm | 13.0 ft-lb/in | ASTM D256 |
Nylene® Naxel™ PC40CV Polycarbonate Description: Naxel™ PC40CV is a 17 melt, virgin, general purpose polycarbonate. Information provided by Custom Resins. ALM, Nylene Canada, and Custom Resins are all operting companies of Polymeric .. |
|||
Izod Impact, Notched | 6.94 J/cm @Temperature 23.0 °C |
13.0 ft-lb/in @Temperature 73.4 °F |
ASTM D 256 |
SABIC Innovative Plastics Lexan® SFX123RU PC SFX123RU is a transparent SecurFX grade with improved flow, mold release and UV stabilizer. This grade is for security applications and contains proprietary authentication technology.This data was s.. |
|||
Izod Impact, Notched | 6.94 J/cm @Temperature 23.0 °C |
13.0 ft-lb/in @Temperature 73.4 °F |
ASTM D 256 |
SABIC Innovative Plastics Lexan® SFX123RU PC (Asia Pacific) SFX123RU is a transparent SecurFX grade with improved flow, mold release and UV stabilizer. This grade is for security applications and contains proprietary authentication technology.This data was s.. |