Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Charpy Impact, Notched | 0.150 J/cm² @Temperature -20.0 °C |
0.714 ft-lb/in² @Temperature -4.00 °F |
STN EN ISO 179 |
Plastcom PLASTALEN® PH 51 T 40 Polypropylene reinforced with mineral filler Modified homopolymer PP for injection molding with the content of 40% mineral filler. General application. Delivered in black color.Information Provided by Plastcom spol. s r.o. |
|||
Charpy Impact, Notched | 0.150 J/cm² @Temperature 23.0 °C |
0.714 ft-lb/in² @Temperature 73.4 °F |
STN EN ISO 179 |
Plastcom PLASTAMID® 6 BT N 26 B PA6 Basic type PA 6 for compounding, for general use. Use: automotive, engineering, electrical and consumer-goods industry. Delivered in the natural mode and in the full RAL color scale.Information Prov.. |
|||
Charpy Impact, Notched | 0.150 J/cm² @Temperature -20.0 °C |
0.714 ft-lb/in² @Temperature -4.00 °F |
STN EN ISO 179 |
Plastcom PLASTAMID® 6 BT N 26 B/IM PA6 Basic type PA 6 for injection molding, for general use. Use: automotive, engineering, electrical and consumer-goods industry - electrical tools, fasteners, clamps, hobby tools. Delivered in the natu.. |
|||
Charpy Impact, Notched | 0.150 J/cm² @Temperature 23.0 °C |
0.714 ft-lb/in² @Temperature 73.4 °F |
STN EN ISO 179 |
Plastcom PLASTAMID® 6 BT N 29 B/IM PA6 Basic type PA 6 for injection molding, for general use. Use: automotive, engineering, electrical and consumer-goods industry - electrical tools, fasteners, clamps, hobby tools. Delivered in the natu.. |
|||
Charpy Impact, Notched | 0.150 J/cm² @Temperature 23.0 °C |
0.714 ft-lb/in² @Temperature 73.4 °F |
STN EN ISO 179 |
Plastcom PLASTAMID® 6 BT PA6 Basic type PA 6 for compounding, modified for general use. Use: automotive, engineering, electrical and consumer-goods industry. Delivered in the natural mode and in the full RAL color scale.Informa.. |
|||
Charpy Impact, Notched | 0.150 J/cm² @Temperature -20.0 °C |
0.714 ft-lb/in² @Temperature -4.00 °F |
|
Plastcom SLOVALEN PC 51 C 20 PP, 20% mineral filling FeaturesModified homopolymer and copolymer PP for injection moulding with the contenct of 20% microground, chemically modified talc. Increased strength, rigidity and thermal application up to 100°C.. |
|||
Charpy Impact, Notched | 0.150 J/cm² @Temperature -20.0 °C |
0.714 ft-lb/in² @Temperature -4.00 °F |
|
Plastcom SLOVALEN PH 22 T 40 PP, 40% mineral filling FeaturesModified homopolymer PP for injection moulding with the content of 40% microground, floated, chemically modified talc. Special designed for automotive light housings. Delivered in natural mo.. |
|||
Charpy Impact, Notched | 0.150 J/cm² @Temperature -20.0 °C |
0.714 ft-lb/in² @Temperature -4.00 °F |
|
Plastcom SLOVALEN PH 52 T 20 PP, 20% mineral filling FeaturesModified homopolymer PP for injection moulding with the content of 20% mineral filling. Increased rigidity, strength and thermal use up to 130°C depending on the talc conte nt. Decreased sh.. |
|||
Charpy Impact, Notched | 0.150 J/cm² @Temperature 23.0 °C |
0.714 ft-lb/in² @Temperature 73.4 °F |
|
Plastcom SLOVALEN PH 61 B 70 PP, 70% mineral filling FeaturesModified PP for injection moulding with the content of 70% of barium sulphate. Increased density. Decreased shrinkage.Used for production of vertical blind weights. Delivered in natural mode.. |
|||
Charpy Impact, Notched | 0.150 J/cm² @Temperature -20.0 °C |
0.714 ft-lb/in² @Temperature -4.00 °F |
|
Plastcom SLOVALEN PH 76 T 20 FRD 5 PP, 20% mineral filling, flame retardant FeaturesModified homopolymer PP for injection moulding, with the content of 20% microground chemically modified talc, retarded with halogen flame retardant Application - electrical industry - termin.. |
|||
Charpy Impact, Notched | 0.150 J/cm² @Temperature -20.0 °C |
0.714 ft-lb/in² @Temperature -4.00 °F |
STN EN ISO 179 |
Plastcom SLOVAMID 6 GF 25 FRA 5 Polyamide 6, 25% Glass Fiber, Halogen Flame Retardant FeaturesPA 6 for injection moulding, chemically reinforced with 25% glass fiber, with halogen flame retardant. Main features: flammability in accordance with UL 94 V0 at 1.6mm, glow wire at 960°C,.. |
|||
Charpy Impact, Notched | 0.150 J/cm² @Temperature -20.0 °C |
0.714 ft-lb/in² @Temperature -4.00 °F |
STN EN ISO 179 |
Plastcom SLOVAMID 66 BT Polyamide 66 FeaturesModified for general use, with excellent manufacturing properties, characterized by high strength and toughness also at low temperatures. Use in automotive, electrical, engineering and cons.. |
|||
Charpy Impact, Notched | 0.150 J/cm² @Temperature -20.0 °C |
0.714 ft-lb/in² @Temperature -4.00 °F |
|
Plastcom SLOVAMID 66 FRC 2 PA66, basic type FeaturesModified for general use, with excellent manufacturing properties, characterized by high strength and toughness also at minus temperatures. Used in automotive, electrical, engineering and co.. |
|||
Charpy Impact, Notched | 0.150 J/cm² @Temperature -20.0 °C |
0.714 ft-lb/in² @Temperature -4.00 °F |
|
Plastcom SLOVAMID 66 OB PA66, optically brightened FeaturesPA 66 for injection moulding, optical brightened, for mouldings with high surface brightness, with increased toughness and modulus of elasticity in tension in comparison with the basic type... |
|||
Charpy Impact, Notched | 0.150 J/cm² @Temperature -20.0 °C |
0.714 ft-lb/in² @Temperature -4.00 °F |
ISO 179 |
Polykemi AB POLYfill PPH T15040CR Polypropylene Homopolymer, Mineral Reinforced Information provided by Polykemi AB |
|||
Charpy Impact, Notched | 0.150 J/cm² @Temperature -20.0 °C |
0.714 ft-lb/in² @Temperature -4.00 °F |
ISO 179 |
Polykemi AB SCANCOMP PP BN140 T5 Polypropylene Information provided by Polykemi AB |
|||
Charpy Impact, Notched | 0.150 - 0.250 J/cm² @Temperature 23.0 °C |
0.714 - 1.19 ft-lb/in² @Temperature 73.4 °F |
Injection; ISO 179/ 1eA |
Raschig Group 4552 Silicone Glass fiber reinforced silicone molding compound. Excellent thermal stability - up to +/- 300°C continuously, excellent electrical properties, good mechanical strength, very good dimensional stabi.. |
|||
Charpy Impact, Notched | 0.150 - 0.250 J/cm² @Temperature 23.0 °C |
0.714 - 1.19 ft-lb/in² @Temperature 73.4 °F |
Compression; ISO 179/ 1eA |
Raschig Group AMPLA® 2000 melamine-modified polyester Halogen-free, organically and inorganically filled melamine-modified Polyester molding compound. Low post-shrinkage, very good electrical values, high heat resistance, very good sliding behavior, ve.. |
|||
Charpy Impact, Notched | 0.150 - 0.200 J/cm² @Temperature 23.0 °C |
0.714 - 0.952 ft-lb/in² @Temperature 73.4 °F |
Injection; ISO 179/ 1eA |
Raschig Group MELOPLAS® 152.7 MF Cellulose-reinforced MF molding compound in white and colored shades. High surface hardness, very good UV stability, very good resistance to chemicals also to foodstuff ingredients, physiologically.. |
|||
Charpy Impact, Notched | 0.150 J/cm² @Temperature 23.0 °C |
0.714 ft-lb/in² @Temperature 73.4 °F |
STN EN ISO 179 |
Plastcom SLOVAMID 6 BT LS Polyamide 6, UV Stabilized FeaturesPA 6 for injection moulding with the content of UV stabilizer predetermines products for external use, eg. seats for sport stadiums, covers of electrical appliances. Delivered in natural an.. |
|||
Charpy Impact, Notched | 0.150 J/cm² @Temperature -20.0 °C |
0.714 ft-lb/in² @Temperature -4.00 °F |
STN EN ISO 179 |
Plastcom SLOVAMID 6 BT LS Polyamide 6, UV Stabilized FeaturesPA 6 for injection moulding with the content of UV stabilizer predetermines products for external use, eg. seats for sport stadiums, covers of electrical appliances. Delivered in natural an.. |
|||
Charpy Impact, Notched | 0.150 J/cm² @Temperature -20.0 °C |
0.714 ft-lb/in² @Temperature -4.00 °F |
|
Plastcom SLOVAMID 6 GF 25 FRA 5 LS PA6, 25% glass fibre, flame retardant FeaturesPA 6 for injection moulding, chemically reinforced with 25% glass fibre, with halogen flame retardant. Main features: flammability in accordance with UL 94 V0 at 1.6 mm, glow wire at 960°C,.. |
|||
Charpy Impact, Notched | 0.150 J/cm² @Temperature -40.0 °C |
0.714 ft-lb/in² @Temperature -40.0 °F |
ISO 179 |
Polykemi AB POLYfill PP HIP8040 VT2 Polypropylene, Mineral Reinforced, Heat Resistant Information provided by Polykemi AB |
|||
Charpy Impact, Notched | 0.150 J/cm² @Temperature -30.0 °C |
0.714 ft-lb/in² @Temperature -22.0 °F |
ISO 179/1eA |
Inno-Comp INNOPOL® CS 1-2140 BLH 40% Talc-Filled Polypropylene Homopolymer INNOPOL® CS 1-2140 BLH is recommended especially for producing products, where high stiffness, low shrinkage, long term heat stability and excellent processability are required.All information pr.. |
|||
Charpy Impact, Notched | 0.150 J/cm² @Temperature -30.0 °C |
0.714 ft-lb/in² @Temperature -22.0 °F |
ISO 179/1eA |
Inno-Comp INNOPOL® CS 2-3120 BPLU 9H0017 20% Talc-Filled, UV Stabilized Polypropylene Block-Copolymer INNOPOL® CS 2-3120 BPLU 9H0017 is a 20% talc filled, UV stabilized compound based on polypropylene block-copolymer.INNOPOL® CS 2-3120 BPLU 9H0017 is developed for producing injection molded au.. |
|||
Charpy Impact, Notched | 0.150 J/cm² @Temperature 23.0 °C |
0.714 ft-lb/in² @Temperature 73.4 °F |
|
LATI Latene® 7-V2 PP Homopolymer, Flame Retardant Polypropylene homopolymer (PPh) based compound. UL94 V-2 classified, with brominated flame retardants, PBB/PBDE free. Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North A.. |
|||
Charpy Impact, Notched | 0.150 J/cm² @Temperature 23.0 °C |
0.714 ft-lb/in² @Temperature 73.4 °F |
|
LATI Latene® 7 TR-V2 PP Homopolymer, Mineral Reinforced, Flame Retardant Polypropylene homopolymer (PPh) based compound. Mineral filler. UL94 V-2 classified, with brominated flame retardants, PBB/PBDE free. Good surface appearance.Availability: Africa & Middle East; Asia.. |
|||
Charpy Impact, Notched | 0.150 J/cm² @Temperature 23.0 °C |
0.714 ft-lb/in² @Temperature 73.4 °F |
|
LATI Latene® 7H2-V2HF PP Homopolymer, Heat Stabilized, Flame Retardant Polypropylene homopolymer (PPh) based compound. Heat stabilized. UL94 V-2 classified, halogens-based flame retardants free.Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; No.. |
|||
Charpy Impact, Notched | 0.150 J/cm² @Temperature -20.0 °C |
0.714 ft-lb/in² @Temperature -4.00 °F |
ISO 179/1eA |
Borealis Borcom™ WG140AI Polypropylene Borcom™ WG140AI is a polypropylene microcomposite intended for injection molding. This material has an excellent balance between impact strength and stiffness, high melt flow rate and gives a good.. |
|||
Charpy Impact, Notched | 0.150 J/cm² @Temperature -20.0 °C |
0.714 ft-lb/in² @Temperature -4.00 °F |
ISO 179 |
Polykemi AB POLYfill PPH T20040 Polypropylene Homopolymer, Mineral Reinforced Information provided by Polykemi AB |