Mechanical Properties Metric English Comments
Charpy Impact, Notched 0.120 J/cm²

@Temperature -20.0 °C
0.571 ft-lb/in²

@Temperature -4.00 °F
STN EN ISO 179
Plastcom PLASTALEN® PH 91 SDU Polypropylene
Modified homopolymer PP for injection molding. General use in all industry branches. Delivered in natural mode and in full RAL color.Information Provided by Plastcom spol. s r.o.
Charpy Impact, Notched 0.120 J/cm²

@Temperature -20.0 °C
0.571 ft-lb/in²

@Temperature -4.00 °F
STN EN ISO 179
Plastcom PLASTALEN® PQ 81 T 10 Polypropylene reinforced with mineral filler
Modified PP for injection molding with the content of 10% mineral filler, impact modified. Delivered in black color.Information Provided by Plastcom spol. s r.o.
Charpy Impact, Notched 0.120 J/cm²

@Temperature -20.0 °C
0.571 ft-lb/in²

@Temperature -4.00 °F
Plastcom SLOVALEN PH 51 T 60 PP, 60% mineral filling
FeaturesModified homopolymer PP for injection moulding with the content of 60% microground, floated, chemically modified talc. General application in all industry. Delivered in natural mode and in t..
Charpy Impact, Notched 0.120 - 0.180 J/cm²

@Temperature 23.0 °C
0.571 - 0.857 ft-lb/in²

@Temperature 73.4 °F
Compression; ISO 179/ 1eA
Raschig Group MELOPLAS® 150 MF
Wood flour-reinforced MF molding compound in dark colors. High surface hardness, high mechanical strength, good electrical properties. Self-extinguishing (V-O/1,6 according to UL 94), UL-listed. Fr..
Charpy Impact, Notched 0.120 - 0.180 J/cm²

@Temperature 23.0 °C
0.571 - 0.857 ft-lb/in²

@Temperature 73.4 °F
Compression; ISO 179/ 1eA
Raschig Group MELOPLAS® 152 MF
Cellulose-reinforced MF molding compound in white and colored shades. Very good electrical properties, high surface hardness, good abrasion- and UV-stability, very good resistance to chemicals - al..
Charpy Impact, Notched 0.120 - 0.180 J/cm²

@Temperature 23.0 °C
0.571 - 0.857 ft-lb/in²

@Temperature 73.4 °F
Compression; ISO 179/ 1eA
Raschig Group MELOPLAS® 181 MF
Cellulose-reinforced, phenol-modified MF molding compound (MPF) in white and colored shades. High surface hardness, good electrical properties, good mechanical strength, high UV and heat resistanc..
Charpy Impact, Notched 0.120 - 0.180 J/cm²

@Temperature 23.0 °C
0.571 - 0.857 ft-lb/in²

@Temperature 73.4 °F
Compression; ISO 179/ 1eA
Raschig Group MELOPLAS® 181.5 MF
Cellulose-reinforced, phenol-modified MF molding compound (MPF) in white and colored shades. Very good electrical properties, high surface hardness, good mechanical strength, high UV and heat resis..
Charpy Impact, Notched 0.120 - 0.180 J/cm²

@Temperature 23.0 °C
0.571 - 0.857 ft-lb/in²

@Temperature 73.4 °F
Compression; ISO 179/ 1eA
Raschig Group MELOPLAS® 182 MF
Wood flour-reinforced and inorganically filled, phenol-modified MF molding compound (MPF) in dark colors. Improved dimensional stability and electrical properties as compared with MP 180, high surf..
Charpy Impact, Notched 0.120 - 0.180 J/cm²

@Temperature 23.0 °C
0.571 - 0.857 ft-lb/in²

@Temperature 73.4 °F
Compression; ISO 179/ 1eA
Raschig Group MELOPLAS® 183 MF
Cellulose-reinforced and inorganically filled, phenol-modified MF molding compound (MPF) in white and colored shades. Improved dimensional stability and electrical properties as compared with MP 18..
Charpy Impact, Notched 0.120 J/cm²

@Temperature -30.0 °C
0.571 ft-lb/in²

@Temperature -22.0 °F
ISO 179/1eA
Inno-Comp INNOPOL® CS 1-3000 B DEL Polypropylene Homopolymer
INNOPOL® CS 1-3000 B DEL is developed for producing injection molded automotive components.All information provided by INNO-COMP.
Charpy Impact, Notched 0.120 J/cm²

@Temperature -30.0 °C
0.571 ft-lb/in²

@Temperature -22.0 °F
ISO 179/1eA
Inno-Comp INNOPOL® CS 1-3000 N DEL Polypropylene Homopolymer
INNOPOL® CS 1-3000 N DEL is developed for producing injection molded automotive components.All information provided by INNO-COMP.
Charpy Impact, Notched 0.120 J/cm²

@Temperature -20.0 °C
0.571 ft-lb/in²

@Temperature -4.00 °F
ISO 179/1eA
Borealis Borcoat™ MA115E Syntactic Polypropylene for Steel Pipe Coating
Borcoat™ MA115E is a highly filled polypropylene compound and is self colored. Applications: Borcoat™ MA115E is recommended as heavy weight coating for special applications used in steel pipe coa..
Charpy Impact, Notched 0.120 J/cm²

@Temperature -20.0 °C
0.571 ft-lb/in²

@Temperature -4.00 °F
ISO 179/1eA
Borealis MD441U Polypropylene Compound, Mineral Filled
MD441U is a 40% mineral filled polypropylene compound intended for injection molding. This material has excellent balanced mechanical properties and a medium melt flow rate. Applications: air cond..
Charpy Impact, Notched 0.120 J/cm²

@Temperature -20.0 °C
0.571 ft-lb/in²

@Temperature -4.00 °F
ISO 179/1eA
Borealis MG302Al Polypropylene Compound, Mineral Filled
MG302AI is a 30% mineral filled polypropylene compound intended for injection and back injection molding. This material has an excellent balance between impact strength and stiffness and high melt ..
Charpy Impact, Notched 0.120 J/cm²

@Temperature -20.0 °C
0.571 ft-lb/in²

@Temperature -4.00 °F
ISO 179/1eA
Borealis PS65T20 Polypropylene Compound, Mineral Filled
PS65T20 is a 20% mineral filled polypropylene compound intended for injection and back injection molding. This material has excellent balanced mechanical properties and high melt flow rate. Applic..
Charpy Impact, Notched 0.120 J/cm²

@Temperature 23.0 °C
0.571 ft-lb/in²

@Temperature 73.4 °F
ISO 179
Unipetrol PE HD LITEN® BB 10 HDPE
Made for blow molding, extrusion, and pipe applications.Information provided by Unipetrol RPA
Charpy Impact, Notched 0.120 J/cm²

@Temperature 23.0 °C
0.571 ft-lb/in²

@Temperature 73.4 °F
ISO 179
Unipetrol PE HD LITEN® BB 29 HDPE
Made for blow molding, extrusion, and pipe applications.Information provided by Unipetrol RPA
Charpy Impact, Notched 0.120 J/cm²

@Temperature 23.0 °C
0.571 ft-lb/in²

@Temperature 73.4 °F
ISO 179
Unipetrol PE HD LITEN® BB 38 HDPE
Made for blow molding, extrusion, and pipe applications.Information provided by Unipetrol RPA
Charpy Impact, Notched 0.120 J/cm²

@Temperature 23.0 °C
0.571 ft-lb/in²

@Temperature 73.4 °F
ISO 179
Unipetrol PE HD LITEN® FB 10 HDPE
Made for tubular film applications.Information provided by Unipetrol RPA
Charpy Impact, Notched 0.120 J/cm²

@Temperature 23.0 °C
0.571 ft-lb/in²

@Temperature 73.4 °F
ISO 179
Unipetrol PE HD LITEN® FB 29 HDPE
Made for tubular film applications.Information provided by Unipetrol RPA
Charpy Impact, Notched 0.120 J/cm²

@Temperature 23.0 °C
0.571 ft-lb/in²

@Temperature 73.4 °F
ISO 179
Unipetrol PE HD LITEN® PL 10 HDPE
Pipe applications.Information provided by Unipetrol RPA
Charpy Impact, Notched 0.120 J/cm²

@Temperature 23.0 °C
0.571 ft-lb/in²

@Temperature 73.4 °F
ISO 179
Unipetrol PE HD LITEN® TB 38 HDPE
Made for tape applications.Information provided by Unipetrol RPA
Charpy Impact, Notched 0.120 J/cm²

@Temperature 23.0 °C
0.571 ft-lb/in²

@Temperature 73.4 °F
ISO 179
Unipetrol PE HD LITEN® VL 10 HDPE
Extrusion and pipe applications.Information provided by Unipetrol RPA
Charpy Impact, Notched 0.120 J/cm²

@Temperature -20.0 °C
0.571 ft-lb/in²

@Temperature -4.00 °F
ISO 179/1eA
Borealis ME212U Polypropylene Compound, Mineral Filled
ME212U is a 20% mineral filled polypropylene compound intended for injection molding. This material has excellent balanced mechanical properties and is easy to process. Applications: air ducts, air..
Charpy Impact, Notched 0.120 J/cm²

@Temperature -20.0 °C
0.571 ft-lb/in²

@Temperature -4.00 °F
ISO 179/1eA
Borealis MS64T20 Polypropylene Compound, Mineral Filled
MS64T20 is a 20% mineral filled polypropylene compound intended for injection molding. This material has excellent balanced mechanical properties and is easy to process. Applications: automotive p..
Charpy Impact, Notched 0.120 - 0.180 J/cm²

@Temperature 23.0 °C
0.571 - 0.857 ft-lb/in²

@Temperature 73.4 °F
Compression; ISO 179/ 1eA
Raschig Group MELOPLAS® 180 MF
Wood flour-reinforced, phenol-modified MF molding compound (MPF) in dark colors. High surface hardness, good mechanical strength and electrical properties, good heat resistance. Self-extinguishing ..
Charpy Impact, Notched 0.120 J/cm²

@Temperature -20.0 °C
0.571 ft-lb/in²

@Temperature -4.00 °F
ISO 179/1eA
Borealis MD231U Polypropylene Compound, Mineral Filled
MD231U is a 20 % mineral filled polypropylene compound intended for injection molding. This material has excellent balanced mechanical properties and a medium melt flow rate. Applications: Air duc..