Polymer Property : Charpy Impact, Notched = 0.619 ft-lb/in² Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Charpy Impact, Notched 0.130 J/cm²

@Temperature -20.0 °C
0.619 ft-lb/in²

@Temperature -4.00 °F
STN EN ISO 179
Plastcom PLASTALEN® PH 52 T 20 003/1M Polypropylene reinforced with 20% mineral filler
PP homopolymer for injection molding with the content of 20 % mineral filler, heat stabilized. Application in automotive industry. Delivered in black grade.Information Provided by Plastcom spol. s r..
Charpy Impact, Notched 0.130 - 0.200 J/cm²

@Temperature 23.0 °C
0.619 - 0.952 ft-lb/in²

@Temperature 73.4 °F
Injection; ISO 179/ 1eA
Raschig Group MELOPLAS® 150 MF
Wood flour-reinforced MF molding compound in dark colors. High surface hardness, high mechanical strength, good electrical properties. Self-extinguishing (V-O/1,6 according to UL 94), UL-listed. Fr..
Charpy Impact, Notched 0.130 - 0.200 J/cm²

@Temperature 23.0 °C
0.619 - 0.952 ft-lb/in²

@Temperature 73.4 °F
Injection; ISO 179/ 1eA
Raschig Group MELOPLAS® 182 MF
Wood flour-reinforced and inorganically filled, phenol-modified MF molding compound (MPF) in dark colors. Improved dimensional stability and electrical properties as compared with MP 180, high surf..
Charpy Impact, Notched 0.130 - 0.200 J/cm²

@Temperature 23.0 °C
0.619 - 0.952 ft-lb/in²

@Temperature 73.4 °F
Injection; ISO 179/ 1eA
Raschig Group MELOPLAS® 183 MF
Cellulose-reinforced and inorganically filled, phenol-modified MF molding compound (MPF) in white and colored shades. Improved dimensional stability and electrical properties as compared with MP 18..
Charpy Impact, Notched 0.130 J/cm²

@Temperature -20.0 °C
0.619 ft-lb/in²

@Temperature -4.00 °F
STN EN ISO 179
Plastcom PLASTALEN® PH 52 T 20 Polypropylene reinforced with mineral filler
PP homopolymer for injection molding with the content of 20 % mineral filler, heat stabilized. Application in automotive industry. Delivered in black grade.Information Provided by Plastcom spol. s r..
Charpy Impact, Notched 0.130 J/cm²

@Temperature -20.0 °C
0.619 ft-lb/in²

@Temperature -4.00 °F
ISO 179/1eA
Inno-Comp INNOPOL® CS 1-1120 AN 20% Talc-Filled Polypropylene Homopolymer
INNOPOL® CS 1-1120 AN is a 20% talc-filled polypropylene homopolymer compound /PP-H TD20 (ISO 1043)/. This grade is available in natural and custom colored form.INNOPOL® CS 1-1120 AN is develo..
Charpy Impact, Notched 0.130 J/cm²

@Temperature 23.0 °C
0.619 ft-lb/in²

@Temperature 73.4 °F
ISO 179
Unipetrol PE HD LITEN® BB 85 HDPE
Made for blow molding, extrusion, and pipe applications.Information provided by Unipetrol RPA
Charpy Impact, Notched 0.130 J/cm²

@Temperature 23.0 °C
0.619 ft-lb/in²

@Temperature 73.4 °F
ISO 179
Unipetrol PE HD LITEN® FB 85 HDPE
Made for tubular film applications.Information provided by Unipetrol RPA
Charpy Impact, Notched 0.130 J/cm²

@Temperature -20.0 °C
0.619 ft-lb/in²

@Temperature -4.00 °F
ISO 179
Unipetrol PP MONSTEN® MT 825 Polypropylene Random Copolymer
Made for injection molding applications. Antistatic and transparent stabilization. Random copolymer.Information provided by Unipetrol RPA
Charpy Impact, Notched 0.130 J/cm²

@Temperature -20.0 °C
0.619 ft-lb/in²

@Temperature -4.00 °F
ISO 179
Unipetrol PP MONSTEN® MT 935 Polypropylene Random Copolymer
Made for injection molding applications. Antistatic and transparent stabilization. Random copolymer.Information provided by Unipetrol RPA
Charpy Impact, Notched 0.130 J/cm²

@Temperature -20.0 °C
0.619 ft-lb/in²

@Temperature -4.00 °F
ISO 179
Unipetrol PP MONSTEN® MT 950 Polypropylene Random Copolymer
Made for injection molding applications. Antistatic and transparent stabilization. Random copolymer.Information provided by Unipetrol RPA