Mechanical Properties Metric English Comments
Charpy Impact, Notched 15.0 J/cm²

@Temperature 23.0 °C
71.4 ft-lb/in²

@Temperature 73.4 °F
Radici Radilon® CST 38FL (cond.) Nylon 6/66
Radilon® CS is a range of polyamide 6/66 copolymers obtained through the polymerization of caprolactam and hexamethylendiamine salt with adipic acid.Information provided by Radici group.
Charpy Impact, Notched 15.0 J/cm²

@Temperature 23.0 °C
71.4 ft-lb/in²

@Temperature 73.4 °F
Conditioned; ISO 179/1eA
Lanxess Durethan® DP BC 500 H2.0 901510 Nylon 6
PA 6, extrusion and blow molding grade, non-reinforced, elastomer-modified, high viscosity, good heat-ageing resistance
Charpy Impact, Notched >= 15.0 J/cm²

@Temperature 23.0 °C
>= 71.4 ft-lb/in²

@Temperature 73.4 °F
ISO 179-1
Total Lumicene® mPE M 4041 UV Metallocene Polyethylene, Rotomolding
Lumicene® mPE M 4041 UV is a new generation metallocene medium density polyethylene with hexene as comonomer.Lumicene® mPE M 4041 UV is intended for the manufacture of rotomolded items.Lumicene® ..
Charpy Impact, Notched >= 15.0 J/cm²

@Temperature -30.0 °C
>= 71.4 ft-lb/in²

@Temperature -22.0 °F
ISO 179-1
Total Lumicene® mPE M 4041 UV Metallocene Polyethylene, Rotomolding
Lumicene® mPE M 4041 UV is a new generation metallocene medium density polyethylene with hexene as comonomer.Lumicene® mPE M 4041 UV is intended for the manufacture of rotomolded items.Lumicene® ..
Charpy Impact, Notched 15.0 J/cm²

@Temperature 23.0 °C
71.4 ft-lb/in²

@Temperature 73.4 °F
50%RH; ISO 179/1eA
DuPont Performance Polymers Zytel® BM7300THS BK317 Nylon 6  (Unverified Data**)
Zytel® BM7300THS is an unreinforced, heat stabilized, lubricated, toughened polyamide 6 for blow molding.Information provided by DuPont Performance Polymers
Charpy Impact, Notched 15.0 J/cm²

@# of Cycles 2.00 ,
Temperature -101 °C
71.4 ft-lb/in²

@# of Cycles 2.00 ,
Temperature -150 °F
Transverse
AK Steel NITRONIC® 19-D Duplex Stainless Steel
AK Steel NITRONIC® 19D is a stainless steel with a mixed ferrite and austenite structure. This alloy provides high yield strength (65 ksi minimum {448 MPa}), good drawing and welding characteristi..