Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Charpy Impact, Notched | 3.70 J/cm² @Temperature 23.0 °C |
17.6 ft-lb/in² @Temperature 73.4 °F |
|
Plastcom SLOVAMID 6 HI/1 TLS PA6, improved strength FeaturesPA 6 with the content of thermoplastic kaoutchouc. Impacted, for mouldings with high toughness either at minus temperatures, suitable for external use, eg. ski shoes, sports and safety helme.. |
|||
Charpy Impact, Notched | 3.70 J/cm² @Temperature 23.0 °C |
17.6 ft-lb/in² @Temperature 73.4 °F |
conditioned; ISO 179-1eA |
Lanxess Durethan® BKV 230 DUS008 000000 Nylon 6, 30% Glass Fiber PA 6, 30% glass fiber, injection molding, impact modified, heat-ageing stabilizedInformation provided by LANXESS. |
|||
Charpy Impact, Notched | 3.70 J/cm² @Temperature 23.0 °C |
17.6 ft-lb/in² @Temperature 73.4 °F |
ISO 179-1/1eA |
Styron Magnumâ„¢ 3904 Acrylonitrile Butadiene Styrene (ABS) MAGNUMâ„¢ 3904 is a resin with super-high impact. It is used in a wide range of technical applications. The mass (continuous process) ABS technology of Dow ensures an ABS resin that combines ex.. |
|||
Charpy Impact, Notched | 3.70 J/cm² @Temperature 23.0 °C |
17.6 ft-lb/in² @Temperature 73.4 °F |
Injection Molded; ISO 179/1eA |
Styron MAGNUMâ„¢ 3904 Acrylonitrile Butadiene Styrene (ABS) Resin Overview: MAGNUMâ„¢ 3904 is a resin with super-high impact. It is used in a wide range of technical applications. It can be processed by injection molding, extrusion or thermoforming. The mass (c.. |
|||
Charpy Impact, Notched | 3.70 J/cm² @Temperature 23.0 °C |
17.6 ft-lb/in² @Temperature 73.4 °F |
Injection Molded; ISO 179/1eA |
Styron MAGNUMâ„¢ 3904 Smooth Acrylonitrile Butadiene Styrene (ABS) Resin Overview: MAGNUMâ„¢ 3904 is an extrusion/thermoforming resin developed for high impact and other technical applications. The mass (continuous process) ABS technology of Styron ensures an ABS tech.. |
|||
Charpy Impact, Notched | 3.70 J/cm² @Temperature 23.0 °C |
17.6 ft-lb/in² @Temperature 73.4 °F |
|
BASF Ultramid® Structure B3WG10 LF High-Performance Long-Glass Fiber Reinforced Polyamide |
|||
Charpy Impact, Notched | 3.70 J/cm² @Temperature 23.0 °C |
17.6 ft-lb/in² @Temperature 73.4 °F |
ISO 179/1eA |
DSM Arnitel® PM650 General Purpose Grade Copolyester Elastomer (North America) Product description: Arnitel® combines the advantages of engineering thermoplastics, being easy to process with excellent mechanical properties, at the same time with the flexibility of rubbers.Arn.. |
|||
Charpy Impact, Notched | 3.70 J/cm² @Temperature 23.0 °C |
17.6 ft-lb/in² @Temperature 73.4 °F |
ISO 179/1eA |
DSM Arnitel® PM650 Polyether Ester Elastomer (European and Asian Grade) Product description: Arnitel® combines the advantages of engineering thermoplastics, being easy to process with excellent mechanical properties, at the same time with the flexibility of rubbers.Arn.. |