Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Charpy Impact, Notched | 3.50 J/cm² @Temperature 23.0 °C |
16.7 ft-lb/in² @Temperature 73.4 °F |
|
Plastcom SLOVALEN PQ 81 T 30 PP, 30% mineral filling FeaturesModified PP for injection moulding with the content of 30% mineral filling. Increased rigidity, strength and thermal use up to 130°C depending on the talc content. Decreased shrinkage. Gene.. |
|||
Charpy Impact, Notched | 3.50 J/cm² @Temperature 23.0 °C |
16.7 ft-lb/in² @Temperature 73.4 °F |
ISO 179 |
PolyOne OnFlex™ BIO 5170D-E0010 Thermoplastic Elastomer (TPE) OnFlex™ BIO 5100 series thermoplastic elastomer compounds are glass reinforced thermoplastic polyurethane compounds made from renewable natural sources. These compounds contain at least 20% renewab.. |
|||
Charpy Impact, Notched | 3.50 J/cm² @Temperature 23.0 °C |
16.7 ft-lb/in² @Temperature 73.4 °F |
ISO 179 |
Polykemi AB POLYblend 65V PC/ABS-Blend, Flame Retardant Information provided by Polykemi AB |
|||
Charpy Impact, Notched | 3.50 J/cm² @Temperature -30.0 °C |
16.7 ft-lb/in² @Temperature -22.0 °F |
V-notch Edgew 80*10*3 sp=62mm; ISO 179/1eA |
SABIC Innovative Plastics Cycoloy® CP8930 PC+ABS (Europe-Africa-Middle East) High heat, PC/ABS for automotive electro plating applications, excellent balance in flow/impactThis data was supplied by SABIC-IP for the Europe-Africa-Middle East region. |
|||
Charpy Impact, Notched | 3.50 J/cm² @Temperature 23.0 °C |
16.7 ft-lb/in² @Temperature 73.4 °F |
V-notch Edgew 80*10*3 sp=62mm; ISO 179/1eA |
SABIC Innovative Plastics Cycoloy® LG9000 PC+ABS (Europe-Africa-Middle East) CYCOLOY LG9000 is a low gloss PC+ABS injection moulding grade. LG9000 combines good impact / heat and UV resistance with a low gloss surface appearence. It is suitable for automotive interior applic.. |
|||
Charpy Impact, Notched | 3.50 J/cm² @Temperature -20.0 °C |
16.7 ft-lb/in² @Temperature -4.00 °F |
ISO 179 |
Polykemi AB SCANTEC PC S60R Polycarbonate Information provided by Polykemi AB |
|||
Charpy Impact, Notched | 3.50 J/cm² @Temperature 23.0 °C |
16.7 ft-lb/in² @Temperature 73.4 °F |
ISO 179/2C |
SABIC Innovative Plastics Lexan® FXE101R PC (Europe-Africa-Middle East) Transparent PC. ILLUMINATE special effects (fluorescent/edge glow colors). For thicker sections without sinks. Internal mold release.This data was supplied by SABIC-IP for the Europe-Africa-Middl.. |
|||
Charpy Impact, Notched | 3.50 J/cm² @Temperature 23.0 °C |
16.7 ft-lb/in² @Temperature 73.4 °F |
ISO 179/1eA |
Inno-Comp INNOPOL® CS 2-3110 TO BU 10% Talc Filled Polypropylene Copolymer INNOPOL® CS 2-3110 TO BU is a 10% talc-filled, black colored and UV stabilized compound based on polypropylene block-copolymer.INNOPOL® CS 2-3110 TO BU is developed for producing injection mol.. |
|||
Charpy Impact, Notched | 3.50 J/cm² @Temperature 23.0 °C |
16.7 ft-lb/in² @Temperature 73.4 °F |
Conditioned; ISO 179/1eA |
Lanxess Durethan® BKV 140 H2.0 900051 Copolyamide, 40% Glass Fiber CoPA, injection molding grade, 40% glass fibers, elastomer-modified, electroplateable, higher notched impact strength and also higher energy absorption under biaxial impact load than BKV 40, even in.. |
|||
Charpy Impact, Notched | 3.50 J/cm² @Temperature 23.0 °C |
16.7 ft-lb/in² @Temperature 73.4 °F |
cond.; ISO 179-1eA |
Lanxess Durethan® BKV 215 000000 Nylon 6-Copolymer, Glass Fiber Reinforced, Impact Modified PA 6-Copolymer, 15% glass fibers, injection molding impact modifiedInformation provided by LANXESS. |
|||
Charpy Impact, Notched | 3.50 J/cm² @Temperature 23.0 °C |
16.7 ft-lb/in² @Temperature 73.4 °F |
Conditioned; ISO 179/1eA |
Lanxess Durethan® BKV 215 H2.0 901510 Copolyamide, 15% Glass Fiber CoPA, injection molding grade, 15% glass fibers, elastomer-modified, higher impact and notched impact strength and also higher energy absorption under biaxial impact load than BKV 115, conditioning .. |
|||
Charpy Impact, Notched | 3.50 J/cm² @Temperature 23.0 °C |
16.7 ft-lb/in² @Temperature 73.4 °F |
Conditioned; ISO 179-1eA |
Lanxess Durethan® BKV 215 H3.0 000000 Nylon 6-Copolymer, 15% Glass Fibers PA 6-Copolymer, 15% glass fibers, injection molding, impact modified |
|||
Charpy Impact, Notched | 3.50 J/cm² @Temperature 23.0 °C |
16.7 ft-lb/in² @Temperature 73.4 °F |
ISO 179/1eA |
Styrolution Terluran® SP-6 ABS Description: High impact grade, suitable for extrusion.Information provided by STYROLUTION, which is a joint venture between BASF and INEOS |
|||
Charpy Impact, Notched | 3.50 J/cm² @Temperature 12.0 °C |
16.7 ft-lb/in² @Temperature 53.6 °F |
ISO 179/1eA |
Styron CALIBREâ„¢ 301-10 Polycarbonate Resin Overview: CALIBREâ„¢ 300-10 polycarbonate resins offer exceptional impact resistance, heat distortion resistance and optical clarity as well as high melt strength for blow molding and sheet appli.. |
|||
Charpy Impact, Notched | 3.50 J/cm² @Temperature 23.0 °C |
16.7 ft-lb/in² @Temperature 73.4 °F |
ISO R179 |
Styron Pulse® A35-105 PC/ABS PULSE™ A35-105 engineering resins give exceptional impact strength even at low temperatures and have high heat distortion temperature.Information provided by DowThis product line was spun off f.. |
|||
Charpy Impact, Notched | 3.50 J/cm² @Temperature 23.0 °C |
16.7 ft-lb/in² @Temperature 73.4 °F |
ISO 179/1eA |
Borealis Daplen™ EE108U Polypropylene TPO Compound Daplen™ EE108U is a 10% mineral filled elastomer modified polypropylene compound intended for injection molding. This material has an excellent balance between impact strength and stiffness, gives.. |
|||
Charpy Impact, Notched | 3.50 J/cm² @Temperature 23.0 °C |
16.7 ft-lb/in² @Temperature 73.4 °F |
ISO 179/1eA |
DSM Akulon® F223-D (Cond.) Low/Medium Viscosity Nylon 6 (North America) Description: The Akulon portfolio is engineered for optimum performance to suit different processing techniques and end use markets.Unfilled Extrusion ResinsAkulon resins are available with melt vis.. |
|||
Charpy Impact, Notched | 3.50 J/cm² @Temperature 23.0 °C |
16.7 ft-lb/in² @Temperature 73.4 °F |
ISO 179/1eA |
DSM Akulon® F223-D Nylon 6 (European and Asian Grade) (Cond) The Akulon® product portfolio is engineered for optimum performance to suit different processing techniques and end use markets. Akulon Nylon 6 is used for extrusion applications including barrier .. |
|||
Charpy Impact, Notched | 3.50 J/cm² @Temperature 23.0 °C |
16.7 ft-lb/in² @Temperature 73.4 °F |
cond; ISO 179/1eA |
DSM Akulon® K125/A PA6 Low Viscosity |
|||
Charpy Impact, Notched | 3.50 J/cm² @Temperature 23.0 °C |
16.7 ft-lb/in² @Temperature 73.4 °F |
ISO 179/1eA |
DSM Akulon® K222-D (Cond.) Low Viscosity Nylon 6 (North America) Description: The Akulon portfolio is engineered for optimum performance to suit different processing techniques and end use markets.Unfilled Extrusion ResinsAkulon resins are available with melt vis.. |
|||
Charpy Impact, Notched | 3.50 J/cm² @Temperature 23.0 °C |
16.7 ft-lb/in² @Temperature 73.4 °F |
ISO 179/1eA |
DSM Akulon® K224-PG8 (Cond.) 40% Glass Reinforced, Impact Modified Nylon 6 (North America) Description: The Akulon portfolio is engineered for optimum performance to suit different processing techniques and end use markets.Unfilled Extrusion ResinsAkulon resins are available with melt vis.. |
|||
Charpy Impact, Notched | 3.50 J/cm² @Temperature 23.0 °C |
16.7 ft-lb/in² @Temperature 73.4 °F |
ISO 179/1eA |
DSM Akulon® K224-PG8 Impact Modified Nylon 6-40% Glass Reinforced (European Grade) (Cond) The Akulon® product portfolio is engineered for optimum performance to suit different processing techniques and end use markets. Akulon Nylon 6 is used for extrusion applications including barrier .. |
|||
Charpy Impact, Notched | 3.50 J/cm² @Temperature 23.0 °C |
16.7 ft-lb/in² @Temperature 73.4 °F |
cond; ISO 179/1eA |
DSM Stanyl® TW341-N PA46 Heat Stabilized, Lubricated |
|||
Charpy Impact, Notched | 3.50 J/cm² @Temperature 23.0 °C |
16.7 ft-lb/in² @Temperature 73.4 °F |
ISO 179/eA |
Eurotec® Tecomid® NA40 NL IL PA 6.6 impact modified Excellent stiffness/toughness balanceHigh mechanical strengthVery good thermal stabilityExcellent flammability characteristicsGood electrical propertiesHigh wear resistance and low frictionVery good.. |
|||
Charpy Impact, Notched | 3.50 J/cm² @Temperature -30.0 °C |
16.7 ft-lb/in² @Temperature -22.0 °F |
ISO 179 |
Ascend Performance Materials Vydyne® 41H NT Nylon 66, Impact Modified, DAM Vydyne® 41H NT is general-purpose, impact-modified PA66 resin. Available in natural, it is heat-stabilized for improved resistance to elevated temperatures. The heat stabilization package for Vydyn.. |
|||
Charpy Impact, Notched | 3.50 J/cm² @Temperature -30.0 °C |
16.7 ft-lb/in² @Temperature -22.0 °F |
ISO 179 |
Ascend Performance Materials Vydyne® 41H Nylon 66, Impact Modified, DAM Vydyne® 41H is a general-purpose, impact-modified PA66 resin. Available in natural, it is heat-stabilized for improved resistance to elevated temperatures. The heat stabilization package for Vydyne.. |
|||
Charpy Impact, Notched | 3.50 J/cm² @Temperature 23.0 °C |
16.7 ft-lb/in² @Temperature 73.4 °F |
ISO 179/1eA |
Ascend Performance Materials Vydyne® 65A Nylon 66, General Purpose, intermediate viscosity, Conditioned Vydyne® 65A is a medium-viscosity, heat-stabilized PA66 resin suitable for injection-molding extrusion and compounding applications. It is available in natural color only. Vydyne 65A resin offers h.. |
|||
Charpy Impact, Notched | 3.50 J/cm² @Temperature 23.0 °C |
16.7 ft-lb/in² @Temperature 73.4 °F |
ISO 179 |
Polykemi AB POLYfill PPHC EP1001F Polypropylene Information provided by Polykemi AB |
|||
Charpy Impact, Notched | 3.50 J/cm² @Temperature 23.0 °C |
16.7 ft-lb/in² @Temperature 73.4 °F |
cond; ISO 179/1eA |
DSM Stanyl® TE300 PA46 Heat Stabilized |