Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Charpy Impact, Notched | 1.60 J/cm² @Temperature 23.0 °C |
7.61 ft-lb/in² @Temperature 73.4 °F |
STN EN ISO 179 |
Plastcom SLOVAMID® 6/6T GF 35 TS PA6/6T reinforced with glass fiber, improved heat resistance PA 6/6T for injection molding, reinforced with 35% of glass fiber, for moldings with high strength and toughness used in the automotive, electrical, engineering and consumer-goods industry, improved.. |
|||
Charpy Impact, Notched | 1.60 J/cm² @Temperature 23.0 °C |
7.61 ft-lb/in² @Temperature 73.4 °F |
V-notch Edgew 80*10*4 sp=62mm; ISO 179/1eA |
SABIC Innovative Plastics Cycolac® GPM5500 ABS (Europe-Africa-Middle East) CYCOLAC GPM5500 is a multi purpose injection moulding grade, providing a favourable balance of engineering properties. CYCOLAC GPM5500 has a wide processing window. It is recommended for application.. |
|||
Charpy Impact, Notched | 1.60 J/cm² @Temperature 23.0 °C |
7.61 ft-lb/in² @Temperature 73.4 °F |
ISO 179 |
Polykemi AB POLYabs N20 ABS Information provided by Polykemi AB |
|||
Charpy Impact, Notched | 1.60 J/cm² @Temperature 23.0 °C |
7.61 ft-lb/in² @Temperature 73.4 °F |
ISO 179 |
Polykemi AB SCANAMID 66 A43^E F14 Nylon 66, Glass Fiber Reinforced, Modified Information provided by Polykemi AB |
|||
Charpy Impact, Notched | 1.60 J/cm² @Temperature -20.0 °C |
7.61 ft-lb/in² @Temperature -4.00 °F |
|
Plastcom SLOVAMID 6 HI/1 TLS PA6, improved strength FeaturesPA 6 with the content of thermoplastic kaoutchouc. Impacted, for mouldings with high toughness either at minus temperatures, suitable for external use, eg. ski shoes, sports and safety helme.. |
|||
Charpy Impact, Notched | 1.60 J/cm² @Temperature 23.0 °C |
7.61 ft-lb/in² @Temperature 73.4 °F |
|
Plastcom SLOVAMID 6 NG GF 15 HI PA6, 15% glass fibre, improved strength FeaturesPA 6 for injection moulding, chemically strengthened with 15% glass fibre. Application: impacted mouldings and mouldings with high strength applied in automotive, electrical, engineering and.. |
|||
Charpy Impact, Notched | 1.60 J/cm² @Temperature 23.0 °C |
7.61 ft-lb/in² @Temperature 73.4 °F |
ISO 179 |
Polykemi AB POLYabs F20 ABS Information provided by Polykemi AB |
|||
Charpy Impact, Notched | 1.60 J/cm² @Temperature 23.0 °C |
7.61 ft-lb/in² @Temperature 73.4 °F |
ISO 179 |
Polykemi AB POLYabs F20 UV4 ABS, UV-stabilized Information provided by Polykemi AB |
|||
Charpy Impact, Notched | 1.60 J/cm² @Temperature -30.0 °C |
7.61 ft-lb/in² @Temperature -22.0 °F |
V-notch Edgew 80*10*3 sp=62mm; ISO 179/1eA |
SABIC Innovative Plastics Lexan® ML3021A PC (Europe-Africa-Middle East) LEXAN ML3021A is a high viscosity, UV stabilised grade especially designed for injection blow moulding and profile extrusion.This data was supplied by SABIC-IP for the Europe-Africa-Middle East regi.. |
|||
Charpy Impact, Notched | 1.60 J/cm² @Temperature 23.0 °C |
7.61 ft-lb/in² @Temperature 73.4 °F |
DAM; ISO 179/1eA |
DuPont Performance Polymers Zytel® 73G30HSL BK416 Nylon 6
(Unverified Data**) Zytel® 73G30HSL BK416 is a 30% glass fiber reinforced, heat stabilized, lubricated, black polyamide 6 resin for injection molding.Information provided by DuPont Performance Polymers |
|||
Charpy Impact, Notched | 1.60 J/cm² @Temperature 23.0 °C |
7.61 ft-lb/in² @Temperature 73.4 °F |
ISO 179 |
LG Chemical HT-700 ABS, High Strength, High Scratch Resistance Information Provided by LG Chem |
|||
Charpy Impact, Notched | 1.60 J/cm² @Temperature 23.0 °C |
7.61 ft-lb/in² @Temperature 73.4 °F |
ISO 179-1eA |
Ineos ABS Lustran® M205FC ABS Pellets, Injection Molding Grade Injection Molding grade for medical applications (e.g. inhalers, roller clamps, spikes, etc.)/ Biocompatible with up to 30 days human contact duration according to USP Class VI and ISO 10993-1. Food.. |
|||
Charpy Impact, Notched | 1.60 J/cm² @Temperature 23.0 °C |
7.61 ft-lb/in² @Temperature 73.4 °F |
ISO 179 |
LG Chemical NS-161 ABS, Antistatic, High Strength Information Provided by LG Chem |
|||
Charpy Impact, Notched | 1.60 J/cm² @Temperature -30.0 °C |
7.61 ft-lb/in² @Temperature -22.0 °F |
ISO 179 |
LG Chemical SH-610 ABS, Extrusion, High Impact Information Provided by LG Chem |
|||
Charpy Impact, Notched | 1.60 J/cm² @Temperature 23.0 °C |
7.61 ft-lb/in² @Temperature 73.4 °F |
ISO 179/1eA |
Styron MAGNUM™ 3325 SLG Acrylonitrile Butadiene Styrene (ABS) Resin Overview: Super Low Gloss, Medium Heat, Medium Impact ABS resin for injection molded automotive interior trim applications Magnum 3325 SLG can achieve 60° Gardner gloss levels below 2.0 with low .. |
|||
Charpy Impact, Notched | 1.60 J/cm² @Temperature -30.0 °C |
7.61 ft-lb/in² @Temperature -22.0 °F |
ISO 179/1eA |
Solvay TECHNYL® C 536XT PA6, DRY Description: TECHNYL® C 536XT is an unreinforced polyamide 6, high viscosity, for extrusion blow molding. This product is available in natural color.Benefits: The product offers a good processing.. |
|||
Charpy Impact, Notched | 1.60 J/cm² @Temperature 23.0 °C |
7.61 ft-lb/in² @Temperature 73.4 °F |
ISO 179/1eA |
Suzhou Hipro Polymers Hiprolon® 70 MC HLS G30 Nylon 610, 30% glass fiber filled Hiprolon® 70 MC HLS G30 polyamide 6.10 compound reinforced with 30% chopped glass fiber for injection molding. Features: high heat resistance, dimension stability, impact resistance, good flow ab.. |
|||
Charpy Impact, Notched | 1.60 J/cm² @Temperature -30.0 °C |
7.61 ft-lb/in² @Temperature -22.0 °F |
ISO 179/1eA |
Sax Polymers SAXATEC 4307 Acrylonitrile Styrene Acrylate SAXATEC 4307 is a high impact resistant, high viscosity and weatherable ASA injection molding grade, characterized by high mechanical strength and good processabilityInformation provided by SAX Poly.. |
|||
Charpy Impact, Notched | 1.60 J/cm² @Thickness 3.00 mm, Temperature -30.0 °C |
7.61 ft-lb/in² @Thickness 0.118 in, Temperature -22.0 °F |
complete break; ISO 7391/b.o. ISO 179-1eA |
Covestro Makrolon® 2405 MAS056 Polycarbonate Main characteristics:• High toughness• Good heat resistance• Glass-like transparency, optical quality• High dimensional accuracy and stabilityGrade characteristics:• General purpose• Low.. |
|||
Charpy Impact, Notched | 1.60 J/cm² @Thickness 3.00 mm, Temperature -30.0 °C |
7.61 ft-lb/in² @Thickness 0.118 in, Temperature -22.0 °F |
complete break; ISO 7391/b.o. ISO 179-1eA |
Covestro Makrolon® 3158 Polycarbonate Main characteristics:• High toughness• Good heat resistance• Glass-like transparency, optical quality• High dimensional accuracy and stabilityGrade characteristics:• Medical devices - bioc.. |
|||
Charpy Impact, Notched | 1.60 J/cm² @Temperature -30.0 °C |
7.61 ft-lb/in² @Temperature -22.0 °F |
ISO 179/1eA |
DSM Arnitel® PL581 58 Shore D, Injection Grade Copolyester Elastomer (North America) Product description: Arnitel® combines the advantages of engineering thermoplastics, being easy to process with excellent mechanical properties, at the same time with the flexibility of rubbers.Arn.. |
|||
Charpy Impact, Notched | 1.60 J/cm² @Temperature 23.0 °C |
7.61 ft-lb/in² @Temperature 73.4 °F |
ISO 179/1eA |
DSM Stanyl® TW241F10 Nylon 46-50% Glass Reinforced (European Grade) (Dry) Stanyl is a high performance polyamide providing good performance and value across a broad range of automotive and electronic applications. Stanyl offers:Highest mechanical properties at high temper.. |
|||
Charpy Impact, Notched | 1.60 J/cm² @Temperature -30.0 °C |
7.61 ft-lb/in² @Temperature -22.0 °F |
ISO 179/eA |
Eurotec® Tecomid® NA40 GR50 NL PA 6.6 50% glass fiber reinforced Excellent stiffness/toughness balanceHigh mechanical strengthVery good thermal stabilityExcellent flammability characteristicsGood electrical propertiesHigh wear resistance and low frictionVery good.. |
|||
Charpy Impact, Notched | 1.60 J/cm² @Temperature -30.0 °C |
7.61 ft-lb/in² @Temperature -22.0 °F |
ISO 179/eA |
Eurotec® Tecomid® NB40 GR40 NL PA 6 40% glass fiber reinforced Excellent stiffness/toughness balanceHigh mechanical strengthVery good thermal stabilityExcellent flammability characteristicsGood electrical propertiesHigh wear resistance and low frictionVery good.. |
|||
Charpy Impact, Notched | 1.60 J/cm² @Temperature -30.0 °C |
7.61 ft-lb/in² @Temperature -22.0 °F |
ISO 179 |
Arkema Group Pebax® Rnew 72R53 SP 01 Polyether Block Amide (PEBA) Polyether block amide Pebax® 72R53 SP 01 is a thermoplastic elastomer made of flexible polyether and rigid polyamide based on renewable resources. This SP grade has been developed to be heat and UV.. |
|||
Charpy Impact, Notched | 1.60 J/cm² @Temperature -30.0 °C |
7.61 ft-lb/in² @Temperature -22.0 °F |
|
Akro-Plastic Akromid® A3 GF 50 (2423) PA 6.6 Dry, 50% Glass Filled AKROMID® A (Polyamide 6.6) is an engineering compound, characterized by high mechanical strength, stiffness and thermal resistance. Furthermore, this polyamide offers high toughness at low temperat.. |
|||
Charpy Impact, Notched | 1.60 J/cm² @Temperature 23.0 °C |
7.61 ft-lb/in² @Temperature 73.4 °F |
ISO 179/1eA |
DSM Akulon® K224-HPG3 Impact Modified Nylon 6-15% Glass Reinforced (European Grade) (Dry) The Akulon® product portfolio is engineered for optimum performance to suit different processing techniques and end use markets. Akulon Nylon 6 is used for extrusion applications including barrier .. |
|||
Charpy Impact, Notched | 1.60 J/cm² @Temperature -30.0 °C |
7.61 ft-lb/in² @Temperature -22.0 °F |
ISO 179/1eA |
Sax Polymers SAXAMID 236F6Q32 Nylon 6.6, 30% Glass Fiber SAXAMID 236F6Q32 is a impact-modified polyamide 6.6 injection-molding-grade reinforced with 30% glass fibers and very good flow properties. It is suitable for applications requiring toughness in com.. |
|||
Charpy Impact, Notched | 1.60 J/cm² @Temperature -30.0 °C |
7.61 ft-lb/in² @Temperature -22.0 °F |
ISO 179/1eA |
DSM Arnitel® PM581 Polyether Ester Elastomer (European and Asian Grade) Product description: Arnitel® combines the advantages of engineering thermoplastics, being easy to process with excellent mechanical properties, at the same time with the flexibility of rubbers.Arn.. |