Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Charpy Impact Unnotched | 0.800 - 1.20 J/cm² @Temperature 23.0 °C |
3.81 - 5.71 ft-lb/in² @Temperature 73.4 °F |
Injection and Compression; ISO 179/ 1eU |
Raschig Group 3505 Epoxy Glass-fiber reinforced epoxy molding compound. Good mechanical strength, very good electrical isolation properties and dimensional stability even at high temperatures. This product meets the allowed.. |
|||
Charpy Impact Unnotched | 0.800 - 1.10 J/cm² | 3.81 - 5.23 ft-lb/in² | Injection; ISO 179/1eU |
Raschig Group RALUPOL® 4802 UP Polyester Glass-fiber reinforced polyester molding compound. Low mold shrinkage and post-shrinkage, good electrical values, excellent heat resistance, outstanding pourability. This product meets the allowed u.. |
|||
Charpy Impact Unnotched | 0.800 J/cm² | 3.81 ft-lb/in² | ISO Data |
Americas Styrenics Styron® 685P Polystyrene
(discontinued **) STYRON® 685P general purpose polystyrene resin is a high heat resin with good strength, moldability/processability, and excellent clarity. This resin is typically used in consumer electronic applic.. |
|||
Charpy Impact Unnotched | 0.800 J/cm² | 3.81 ft-lb/in² | ISO 179/1eU |
Total Lacqrene® 1070 Crystal Polystyrene
(discontinued **) Description: LACQRENE® 1070 is a very high molecular weight polystyrene used in extrusion. It is particularly designed for the production of foam sheet, where the very high molecular weight gives .. |
|||
Charpy Impact Unnotched | 0.800 - 30.0 J/cm² | 3.81 - 143 ft-lb/in² | Average value: 6.23 J/cm² Grade Count:6 |
Overview of materials for Acrylonitrile Butadiene Styrene (ABS), 20% Glass Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Acrylonitrile Butadiene Styrene (ABS), 20% Glass Fiber Filled". Specific grades with glass content betwe.. |
|||
Charpy Impact Unnotched | 0.800 J/cm² @Temperature -30.0 °C |
3.81 ft-lb/in² @Temperature -22.0 °F |
|
Ineos ABS Lustran® 1460, Injection Grade
(discontinued **) Injection molding grade, increased heat and impact resistance, medium gloss.Information provided by Bayer.LANXESS was spun-off from Bayer in early 2005. Business renamed Ineos ABS after INEOS acqui.. |
|||
Charpy Impact Unnotched | 0.800 - 1.00 J/cm² | 3.81 - 4.76 ft-lb/in² | Compression; ISO 179/1eU |
Raschig Group RESINOL® 87120 EPF Phenolic Glass-fiber reinforced phenolic molding compound. Excellent heat resistance, low mould shrinkage and post-shrinkage, good chemical resistance and very good mechanical properties. This product meets .. |
|||
Charpy Impact Unnotched | 0.800 - 999.9 J/cm² @Temperature -30.0 - -20.0 °C |
3.81 - 4759 ft-lb/in² @Temperature -22.0 - -4.00 °F |
Average value: 0.800 J/cm² Grade Count:2 |
Overview of materials for Polycarbonate, Glass Fiber Filled, Flame Retardant This property data is a summary of similar materials in the MatWeb database for the category "Polycarbonate, Glass Fiber Filled, Flame Retardant". Each property range of values reported is minimum a.. |
|||
Charpy Impact Unnotched | 0.800 - 3.00 J/cm² | 3.81 - 14.3 ft-lb/in² | Average value: 2.27 J/cm² Grade Count:3 |
Overview of materials for Polytetrafluoroethylene (PTFE), Mica Filled This property data is a summary of similar materials in the MatWeb database for the category "Polytetrafluoroethylene (PTFE), Mica Filled". Each property range of values reported is minimum and maxi.. |
|||
Charpy Impact Unnotched | 0.800 J/cm² @Temperature 23.0 °C |
3.81 ft-lb/in² @Temperature 73.4 °F |
ISO 179-1/2 eU |
Hexion Bakelite™ PF 31.5 Phenolic Formaldehyde Resin, Improved Electrical Properties
(discontinued **) Phenolic molding compound, mainly organically filled, electrically high grade, standardized molding compound.Application areas: Parts for electrical and telecommunications technology, car electronic.. |
|||
Charpy Impact Unnotched | 0.800 J/cm² @Temperature 23.0 °C |
3.81 ft-lb/in² @Temperature 73.4 °F |
ISO 179-1/2 eU |
Hexion Bakelite™ PF 84 Phenolic Formaldehyde Resin, Special Preparation Cylindrical Pellets, High Mechanical Strength
& Phenolic molding compound, organically filled, reinforced with cotton fibers, increased notched impact strength, standardized molding compound.Application areas: Contact support power switch, moldin.. |
|||
Charpy Impact Unnotched | 0.800 J/cm² @Temperature 23.0 °C |
3.81 ft-lb/in² @Temperature 73.4 °F |
ISO 179-1/2 eU |
Hexion Bakelite™ PF 4109 Phenolic Formaldehyde Resin, Improved Electrical Properties, Ammonia Free, Resistant to High Temperatures, Low Shrinkage, High Arc Resistance, UL Listed, Acetic Acid Free Phenolic molding compound, inorganically filled, glass fiber reinforced, ammonia and acetic acid free, electrically high grade, high temperature stability, low shrinkage, high mechanical strength, U.. |
|||
Charpy Impact Unnotched | 0.800 J/cm² | 3.81 ft-lb/in² | |
LATI Latamid 12 H 90FE03 PA 12, Heat Stabilized Polyamide 12 (PA12) based compound. Heat stabilized. Magnetizable filler. Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInformation provided by Lati Industria.. |
|||
Charpy Impact Unnotched | 0.800 J/cm² | 3.81 ft-lb/in² | |
LATI Laticonther 87/28 GR/50 PC, 50% Graphite Reinforced High thermal conductivity product based on Polycarbonate (PC). Graphite.Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInformation provided by Lati Industria T.. |
|||
Charpy Impact Unnotched | 0.800 J/cm² | 3.81 ft-lb/in² | |
LATI Latishield 36/AR-08A G/17-V0E ABS, Steel/Glass Fiber Reinforced, Flame Retardant EMI shielding product based on Acrylonitrile-Butadiene-Styrene copolymer (ABS). Steel fibers. Glass fibers. UL94 V-0 classified, with brominated flame retardants, PBB/PBDE free. Availability: Africa.. |
|||
Charpy Impact Unnotched | 0.800 J/cm² | 3.81 ft-lb/in² | ISO 179 |
Styrolution PS 153A GPPS Styrolution PS 153A is an antistatic modified, general purpose polystyrene grade with a good flow characteristic.AntistaticGood flow characteristicsInformation provided by Styrolution |
|||
Charpy Impact Unnotched | 0.800 J/cm² | 3.81 ft-lb/in² | ISO 179 |
Styrolution PS 153F GPPS Styrolution PS 153F is general purpose polystyrene with high heat resistance and good flow properties. Styrolution PS 153F is free of internal lubricants, e.g. zinc stearate.Free of internal lubrica.. |
|||
Charpy Impact Unnotched | 0.800 J/cm² | 3.81 ft-lb/in² | ISO 179/1eU |
Total PSC 1540(EU) Crystal Polystyrene 1540 is an easy flowing crystal polystyrene designed for extrusion or injection applications. In extrusion, it improves extruder output and thermoforming cycle times when mixed with a high impact p.. |
|||
Charpy Impact Unnotched | 0.800 - 1.00 J/cm² | 3.81 - 4.76 ft-lb/in² | ISO 179 |
Vyncolit 2723 W Novolac Phenolic Mineral and organic filled phenolic molding compound with excellent mechanical, thermal and dielectric properties. I2/FO classified under NF F 16-101 (Fire & Smoke classification).USES: Circuit bre.. |
|||
Charpy Impact Unnotched | 0.800 J/cm² @Temperature -30.0 °C |
3.81 ft-lb/in² @Temperature -22.0 °F |
|
Covestro Apec® HT KU 1-9350 High-Heat Polycarbonate Transparent and opaque shades possible.Applications: Medical sector: superheated steam sterilization.Information provided by Bayer.As of 1 September 2015, Bayer MaterialScience was separated from Ba.. |
|||
Charpy Impact Unnotched | 0.800 J/cm² @Temperature -30.0 °C |
3.81 ft-lb/in² @Temperature -22.0 °F |
|
Covestro Apec® HT KU 1-9353 High-Heat Polycarbonate, UV-Stabilized Transparent and opaque shades possible, UV-stabilized.Applications: Lighting, automotive and household goods, light covers.Information provided by Bayer.As of 1 September 2015, Bayer MaterialScience.. |
|||
Charpy Impact Unnotched | 0.800 J/cm² @Temperature -30.0 °C |
3.81 ft-lb/in² @Temperature -22.0 °F |
|
BASF Procom® D 1012 Polypropylene Data was collected by ISO methods and provided by BASF. |
|||
Charpy Impact Unnotched | 0.800 - 1.10 J/cm² | 3.81 - 5.24 ft-lb/in² | ISO 179 |
Vyncolit X682 Novolac Phenolic Glass fiber, glass bead and graphite filled phenolic molding compound with excellent mechanical properties and a low coefficient of friction.USES: Water pump seals and self-lubricating bearings.Info.. |
|||
Charpy Impact Unnotched | 0.800 J/cm² | 3.81 ft-lb/in² | ISO 179/1eU |
Total Lacqrene® 1160(AS) Crystal Polystyrene
(discontinued **) LACQRENE® 1160 is a high resistance, high molecular weight crystal polystyrene mainly for the extrusion industry. It is particularly useful in the production of thick sheet by direct gassing, wher.. |
|||
Charpy Impact Unnotched | 0.800 - 1.10 J/cm² | 3.81 - 5.23 ft-lb/in² | Injection; ISO 179/1eU |
Raschig Group 5567 DAP Diallyl Phthalate (DAP), Cast, Mineral Filler Glass-fiber reinforced diallyl phthalate molding compound free from halogens. Good mechanical strength together with retention of high electrical isolation properties under hot humid conditions, exc.. |
|||
Charpy Impact Unnotched | 0.800 J/cm² | 3.81 ft-lb/in² | edgewise; ISO 179 1eU |
Lehmann & Voss LUVOCOM® 1105-8165 PEEK, with carbon fiber, lubricant modified Applications: Automotive industry, textile machinery, medical- and precision engineering, aircraft industry.Strong, stiff parts.Chemical and hydrolysis resistance parts, non flammable.Electrically c.. |
|||
Charpy Impact Unnotched | 0.800 J/cm² - NB | 3.81 ft-lb/in² - NB | Average value: 10.6 J/cm² Grade Count:198 |
Overview of materials for Nylon 6, Unreinforced This property data is a summary of similar materials in the MatWeb database for the category "Nylon 6, Unreinforced". Each property range of values reported is minimum and maximum values of appropri.. |
|||
Charpy Impact Unnotched | 0.800 J/cm² - NB | 3.81 ft-lb/in² - NB | Average value: 4.14 J/cm² Grade Count:84 |
Overview of materials for Polypropylene Copolymer This property data is a summary of similar materials in the MatWeb database for the category "Polypropylene Copolymer". Each property range of values reported is minimum and maximum values of approp.. |
|||
Charpy Impact Unnotched | 0.800 - 0.800 J/cm² @Temperature -20.0 - -20.0 °C |
3.81 - 3.81 ft-lb/in² @Temperature -4.00 - -4.00 °F |
Average value: 0.800 J/cm² Grade Count:1 |
Overview of materials for Polypropylene with 40% Mica Filler This property data is a summary of similar materials in the MatWeb database for the category "Polypropylene with 40% Mica Filler". Specific grades with primary filler content between 35% and 44% are.. |