Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Charpy Impact Unnotched | 1.80 - 2.10 J/cm² | 8.57 - 9.99 ft-lb/in² | ISO 11542-2 |
Okulen® 1000 PE-UHMW, Colored OKULEN® 1000 is an ultra high molecular low pressure polyethylene with a molecular weight of < 3.5 g/mol. It has great wear resistance, high impact strength, and excellent sliding properties ideal .. |
|||
Charpy Impact Unnotched | 1.80 J/cm² | 8.57 ft-lb/in² | DIN 53453 |
Nilit FRIANYL A63 CU90 Nylon 6.6 for injection molding, 90% copper filled Nylon 6.6 for injection moldingInformation provided by Frisetta Polymer, which merged into Nilit Plastics |
|||
Charpy Impact Unnotched | 1.80 J/cm² @Temperature -40.0 °C |
8.57 ft-lb/in² @Temperature -40.0 °F |
DIN 53453 |
Nilit RECONYL A SG30 Recycled nylon 6.6 for injection molding, 30% mineral filled Recycled nylon 6.6 for injection molding (available only in black).Information provided by Frisetta Polymer, which merged into Nilit Plastics |
|||
Charpy Impact Unnotched | 1.80 - 4.00 J/cm² @Temperature -30.0 - 30.0 °C |
8.57 - 19.0 ft-lb/in² @Temperature -22.0 - 86.0 °F |
Average value: 2.45 J/cm² Grade Count:4 |
Overview of materials for Liquid Crystal Polymer (LCP), 40% Glass Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Liquid Crystal Polymer (LCP), 40% Glass Fiber Filled". Specific grades with glass content between 35% an.. |
|||
Charpy Impact Unnotched | 1.80 J/cm² | 8.57 ft-lb/in² | edgewise; ISO 179 1eU |
Lehmann & Voss LUVOCOM® 1700-8019 PPO, with glass fiber and PTFE, low-warpage Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.Strong, stiff parts; low thermal coefficient of expansion.Improved friction and wear behaviour... |
|||
Charpy Impact Unnotched | 1.80 J/cm² | 8.57 ft-lb/in² | edgewise; ISO 179 1eU |
Lehmann & Voss LUVOCOM® 80-7388 Polyacetal-copolymer, with carbon fiber and PTFE Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.Electrically conductive, suitable for continuous discharging of statically generated electricit.. |
|||
Charpy Impact Unnotched | 1.80 J/cm² | 8.57 ft-lb/in² | ISO 179/1eU |
Lucite International Diakon® LG156 Acrylic Bead Polymer, High Transparency PMMA beads offer an exceptional transmission level of 92.5%, an increase of +0.5% in light transmission vs. granular grades - ideal for medical diagnostic devices.Information provided by Lucite Inte.. |
|||
Charpy Impact Unnotched | 1.80 J/cm² | 8.57 ft-lb/in² | |
LATI Larton K/20 PPS, 20% Carbon Fiber Reinforced Polyphenylene Sulfide (PPS) based compound. Carbon fiber. Very good chemical resistance. Very good thermal properties. Low smoke density and low toxicity index.Availability: Africa & Middle East; As.. |
|||
Charpy Impact Unnotched | 1.80 J/cm² | 8.57 ft-lb/in² | edgewise; ISO 179 1eU |
Lehmann & Voss LUVOCOM® 1200-7899 ABS, with steel fiber Applications: Office communication.Electrically conductive, suitable for continuous discharging of statically generated electricity.Isotropic shrinkage characteristics.Information provided by Lehman.. |
|||
Charpy Impact Unnotched | 1.80 J/cm² | 8.57 ft-lb/in² | flatwise; ISO 179 1fU |
Lehmann & Voss LUVOCOM® 1301-7575 PPS, linear, with glass fiber Applications: Automotive industry, textile-and office machinery, medical- and precision engineering.Strong, stiff parts.High continuous use and heat distortion temperature. Non flammable.High chemic.. |
|||
Charpy Impact Unnotched | 1.80 J/cm² | 8.57 ft-lb/in² | ISO 179 |
Chi Mei Kibisan® PN-107 L125 SAN High Clarity |
|||
Charpy Impact Unnotched | 1.80 - 3.00 J/cm² | 8.57 - 14.3 ft-lb/in² | ISO 179 |
Bulk Molding Compounds tetra-DUR F 4401 Bulk Molding Compound UL-licensed, general purpose productTypical Applications - Requiring mechanical strength, abrasion resistance, dimensional stability, electrical insulation, electrostatic dissipation (explosion prot.. |
|||
Charpy Impact Unnotched | 1.80 - 3.00 J/cm² | 8.57 - 14.3 ft-lb/in² | ISO 179 |
Bulk Molding Compounds tetra-DUR L 4305 Bulk Molding Compound UL-licensed. Anchor wave-isolation.Typical Applications - Requiring mechanical strength, abrasion resistance, dimensional stability, electrical insulation, electrostatic dissipation (explosion prote.. |
|||
Charpy Impact Unnotched | 1.80 - 8.50 J/cm² | 8.57 - 40.5 ft-lb/in² | Average value: 4.46 J/cm² Grade Count:77 |
Overview of materials for Polyetheretherketone, Glass Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Polyetheretherketone, Glass Fiber Filled". Each property range of values reported is minimum and maximum.. |
|||
Charpy Impact Unnotched | 1.80 J/cm² @Temperature -30.0 °C |
8.57 ft-lb/in² @Temperature -22.0 °F |
|
BASF Novolen® 3300 MC Polypropylene Data was collected by ISO methods and provided by BASF. |
|||
Charpy Impact Unnotched | 1.80 - 4.80 J/cm² | 8.57 - 22.8 ft-lb/in² | Average value: 2.77 J/cm² Grade Count:6 |
Overview of materials for Polyphenylene Ether, 30% Glass Filled This property data is a summary of similar materials in the MatWeb database for the category "Polyphenylene Ether, 30% Glass Filled". Specific grades with glass content between 25% and 34% are inclu.. |
|||
Charpy Impact Unnotched | 1.80 J/cm² @Temperature 23.0 °C |
8.57 ft-lb/in² @Temperature 73.4 °F |
ISO 179/1eU |
Styrolution Luran® 368 R Crystal Clear Transparent 77851 SAN Description: General-purpose grade with well-balanced properties, suitable for injection molding and extrusion. Especially for applications where highest transparency and low natural color is requir.. |
|||
Charpy Impact Unnotched | 1.80 J/cm² | 8.57 ft-lb/in² | ISO 179 |
Styrolution Luran® 368 R SAN General-purpose grade with well-balanced properties intended for both injection molding and extrusion.Information provided by STYROLUTION, which is a joint venture between BASF and INEOS. |
|||
Charpy Impact Unnotched | 1.80 J/cm² @Temperature -30.0 °C |
8.57 ft-lb/in² @Temperature -22.0 °F |
ISO 179 |
Styrolution Luran® 368 R SAN General-purpose grade with well-balanced properties intended for both injection molding and extrusion.Information provided by STYROLUTION, which is a joint venture between BASF and INEOS. |
|||
Charpy Impact Unnotched | 1.80 - 2.60 J/cm² | 8.57 - 12.4 ft-lb/in² | Average value: 2.00 J/cm² Grade Count:6 |
Overview of materials for Acrylic, Optical Grade, Molded This property data is a summary of similar materials in the MatWeb database for the category "Acrylic, Optical Grade, Molded". Each property range of values reported is minimum and maximum values of.. |
|||
Charpy Impact Unnotched | 1.80 - 8.20 J/cm² @Temperature -30.0 - -20.0 °C |
8.57 - 39.0 ft-lb/in² @Temperature -22.0 - -4.00 °F |
Average value: 5.75 J/cm² Grade Count:14 |
Overview of materials for Polypropylene, Long Glass Fiber 50% This property data is a summary of similar materials in the MatWeb database for the category "Polypropylene, Long Glass Fiber 50%". Specific grades with glass content between 45% and 54% are include.. |
|||
Charpy Impact Unnotched | 1.80 - 7.80 J/cm² | 8.57 - 37.1 ft-lb/in² | Average value: 4.03 J/cm² Grade Count:4 |
Overview of materials for Polypropylene, Glass/Mineral Reinforced This property data is a summary of similar materials in the MatWeb database for the category "Polypropylene, Glass/Mineral Reinforced". Each property range of values reported is minimum and maximum .. |
|||
Charpy Impact Unnotched | >= 1.80 J/cm² | >= 8.57 ft-lb/in² | ISO 179 |
Bulk Molding Compounds tetra-DUR N 4203 Bulk Molding Compound Highest dimensional stability under temp. Low profile.Typical Applications - Requiring mechanical strength, abrasion resistance, dimensional stability, electrical insulation, electrostatic dissipat.. |