Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Charpy Impact Unnotched | 3.30 J/cm² | 15.7 ft-lb/in² | DIN 53453 |
Nilit FRIANYL A63 GV20 Nylon 6.6 for injection molding, 20% glass fiber reinforced Nylon 6.6 for injection moldingInformation provided by Frisetta Polymer, which merged into Nilit Plastics |
|||
Charpy Impact Unnotched | 3.30 J/cm² @Temperature -40.0 °C |
15.7 ft-lb/in² @Temperature -40.0 °F |
DIN 53453 |
Nilit FRIANYL B63 H-GV15 Nylon 6 for injection molding, 15% glass fiber reinforced Nylon 6 for injection molding, heat stabilized.Information provided by Frisetta Polymer, which merged into Nilit Plastics |
|||
Charpy Impact Unnotched | 3.30 J/cm² | 15.7 ft-lb/in² | DIN 53453 |
Nilit FRIANYL B63 MG30 Nylon 6 for injection molding, 30% mineral filled Nylon 6 for injection molding.Information provided by Frisetta Polymer, which merged into Nilit Plastics |
|||
Charpy Impact Unnotched | 3.30 J/cm² | 15.7 ft-lb/in² | ISO 179/1eU |
Nilit FRIANYL B63 W-KV10 Nylon 6 for injection molding, 10% glass ball reinforced Nylon 6 for injection molding, heat stabilized.Information provided by Frisetta Polymer, which merged into Nilit Plastics |
|||
Charpy Impact Unnotched | 3.30 J/cm² - NB | 15.7 ft-lb/in² - NB | Average value: 3.65 J/cm² Grade Count:52 |
Overview of materials for Polycarbonate/Polybutylene Terephthalate (PBT) Blend, Unreinforced This property data is a summary of similar materials in the MatWeb database for the category "Polycarbonate/Polybutylene Terephthalate (PBT) Blend, Unreinforced". Each property range of values repor.. |
|||
Charpy Impact Unnotched | 3.30 J/cm² - NB @Temperature -40.0 - 30.0 °C |
15.7 ft-lb/in² - NB @Temperature -40.0 - 86.0 °F |
Average value: 7.76 J/cm² Grade Count:77 |
Overview of materials for Nylon 6, 40% Glass Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Nylon 6, 40% Glass Fiber Filled". Specific grades with glass content between 35% and 44% are included. E.. |
|||
Charpy Impact Unnotched | 3.30 J/cm² | 15.7 ft-lb/in² | edgewise; ISO 179 1eU |
Lehmann & Voss LUVOCOM® 1105-7776 PEEK, with carbon fiber, lubricant modified Applications: Automotive industry, textile machinery, medical- and precision engineering, aircraft industry.Strong, stiff parts.Low warpage, isotropic shrinkage characteristics.Emergency running pro.. |
|||
Charpy Impact Unnotched | 3.30 J/cm² | 15.7 ft-lb/in² | flatwise; ISO 179 1fU |
Lehmann & Voss LUVOCOM® 80-8284 Polyacetal-copolymer, with carbon fiber Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.Electrically conductive, suitable for continuous discharging of statically generated electricit.. |
|||
Charpy Impact Unnotched | 3.30 J/cm² | 15.7 ft-lb/in² | edgewise; ISO 179 1eU |
Lehmann & Voss LUVOCOM® 1104-7598 Polyether ketone, with carbon fiber, PTFE, lubricant modified Applications: Automotive industry, mechanical- and precision engineering.Improved strength and stiffnes at elevated temperatures.Improved fatigue properties.Thermic, mechanic and chemical highly str.. |
|||
Charpy Impact Unnotched | 3.30 J/cm² @Temperature -30.0 °C |
15.7 ft-lb/in² @Temperature -22.0 °F |
ISO 179/2C |
SABIC Innovative Plastics Valox® 4012G PBT (Europe-Africa-Middle East) VALOX 4012G is a 10% glass fibre reinforced PBT injection moulding resin with excellent mechanical properties. Applications: connectors. This grade is a 4012 with improved cycle time and ductility. |
|||
Charpy Impact Unnotched | 3.30 J/cm² @Temperature -30.0 °C |
15.7 ft-lb/in² @Temperature -22.0 °F |
Edgew 80*10*4 sp=62mm; ISO 179/1eU |
SABIC Innovative Plastics Valox® 7062HP PBT ENDURAN 7062HP is a 38% mineral filled & FDA compliance injection moulding resin. |
|||
Charpy Impact Unnotched | 3.30 J/cm² @Temperature -30.0 °C |
15.7 ft-lb/in² @Temperature -22.0 °F |
ISO 179/2C |
SABIC Innovative Plastics Valox® ENH4550 PBT 25% GF reinforced, Non-Brominated & Non-Chlorinated Flame Retardant, PBT resin. |
|||
Charpy Impact Unnotched | 3.30 J/cm² | 15.7 ft-lb/in² | Edgew 80*10*4 sp=62mm; ISO 179/1eU |
SABIC Innovative Plastics LNP THERMOCOMP D451 PC (Asia Pacific) LNP* Thermocomp* D451 (or EXTC8141) is a compound based on Polycarbonate resin containing Glass Fiber, Flame Retardant. Added features of this material include: High modulus, good flatness, good duc.. |
|||
Charpy Impact Unnotched | 3.30 J/cm² | 15.7 ft-lb/in² | Edgew 80*10*4 sp=62mm; ISO 179/1eU |
SABIC Innovative Plastics LNP THERMOCOMP EXTC8141 PC (Asia Pacific) LNP* Thermocomp* EXTC8141 is a compound based on Polycarbonate resin containing Glass Fiber, Flame Retardant. Added features of this material include: High modulus, good flatness, good ductility, No.. |
|||
Charpy Impact Unnotched | 3.30 J/cm² @Temperature -30.0 °C |
15.7 ft-lb/in² @Temperature -22.0 °F |
Edgew 80*10*4 sp=62mm; ISO 179/1eU |
SABIC Innovative Plastics Valox® 7062HP PBT (Asia Pacific) ENDURAN 7062HP is a 38% mineral filled & FDA compliance injection moulding resin. |
|||
Charpy Impact Unnotched | 3.30 J/cm² @Temperature -30.0 °C |
15.7 ft-lb/in² @Temperature -22.0 °F |
Edgew 80*10*4 sp=62mm; ISO 179/1eU |
SABIC Innovative Plastics Valox® 7062HP PBT (Europe-Africa-Middle East) ENDURAN 7062HP is a 38% mineral filled & FDA compliance injection moulding resin. |
|||
Charpy Impact Unnotched | 3.30 J/cm² @Temperature -30.0 °C |
15.7 ft-lb/in² @Temperature -22.0 °F |
Edgew 80*10*4 sp=62mm; ISO 179/1eU |
SABIC Innovative Plastics NORYL GFN1 PPE+PS PPE+PS blend. 10% Glass reinforced. NSF 61 listing in several colors (restrictions apply). FDA compliance (restrictions apply). Low water absorption. Hydrolytic stability. Dimensional stability. Sui.. |
|||
Charpy Impact Unnotched | 3.30 J/cm² @Temperature -40.0 °C |
15.7 ft-lb/in² @Temperature -40.0 °F |
ISO 179/1eU |
Borealis Daplen™ MD206U Polypropylene Compound 20% Mineral Filled Daplen MD206U is a 20% mineral filled polypropylene compound intended for injection molding. MD206U has been developed especially for automotive interior parts that require excellent balance betwee.. |
|||
Charpy Impact Unnotched | >= 3.30 J/cm² | >= 15.7 ft-lb/in² | Parallel to laminations; IEC 1212-2 5.5.2 |
Hippe EP GC 201 Woven Glass Cloth Reinforced Epoxy Resin - Sheet Used in mechanical, electrical and electronic applications. Extremely high mechanical strength at moderate temperature. Very good stability of electrical properties under high humidity.Information.. |
|||
Charpy Impact Unnotched | >= 3.30 J/cm² | >= 15.7 ft-lb/in² | Parallel to laminations; IEC 1212-2 5.5.2 |
Hippe EP GC 202 Woven Glass Cloth Reinforced Epoxy Resin - Sheet Used in mechanical, electrical and electronic applications. Extremely high mechanical strength at moderate temperature. Very good stability of electrical properties under high humidity. Flame ret.. |
|||
Charpy Impact Unnotched | >= 3.30 J/cm² | >= 15.7 ft-lb/in² | Parallel to laminations; IEC 1212-2 5.5.2 |
Hippe EP GC 203 Woven Glass Cloth Reinforced Epoxy Resin - Sheet Used in mechanical, electrical and electronic applications. Extremely high mechanical strength at moderate temperature. Very good stability of electrical properties under high humidity. High mech.. |
|||
Charpy Impact Unnotched | >= 3.30 J/cm² | >= 15.7 ft-lb/in² | Parallel to laminations; IEC 1212-2 5.5.2 |
Hippe EP GC 204 Woven Glass Cloth Reinforced Epoxy Resin - Sheet Used in mechanical, electrical and electronic applications. Extremely high mechanical strength at moderate temperature. Very good stability of electrical properties under high humidity. High mech.. |
|||
Charpy Impact Unnotched | 3.30 J/cm² @Temperature -30.0 °C |
15.7 ft-lb/in² @Temperature -22.0 °F |
ISO 179 |
BASF Ultradur S 4090 G4 LS High Speed BK15077 20% Glass Filled PBT |
|||
Charpy Impact Unnotched | 3.30 J/cm² | 15.7 ft-lb/in² | ISO 179/2C |
SABIC Innovative Plastics Valox® VX4510 PBT (Europe-Africa-Middle East) VALOX VX4510 is a flame retarded, 10% glassfiber reinforced injection moulding PBT resin. |
|||
Charpy Impact Unnotched | 3.30 J/cm² | 15.7 ft-lb/in² | ISO 179/1eU |
Lucite International Elvakon® 4451 Super Low Gloss Acrylic Capstock Coextrusion grade developed to provide high aesthetic control, outstanding weatherability and impact and scratch resistance, the Elvakon® series enables protection of substrates with a durable prot.. |