Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Charpy Impact Unnotched | 2.20 J/cm² | 10.5 ft-lb/in² | ISO 179 |
PolyOne OnForce™ LFT SF-40LCF/000 Black Polyphenylene Sulfide (PPS) PolyOne's Long Fiber Thermoplastic (LFT) compounds are formulated for demanding applications which require high stiffness and good impact such as metal replacement or other structural applications. .. |
|||
Charpy Impact Unnotched | 2.20 - 7.00 J/cm² | 10.5 - 33.3 ft-lb/in² | Average value: 5.51 J/cm² Grade Count:17 |
Overview of materials for Polybutylene Terephthalate (PBT), 50% Glass Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Polybutylene Terephthalate (PBT), 50% Glass Fiber Filled". Specific grades with glass content between 45.. |
|||
Charpy Impact Unnotched | 2.20 J/cm² @Temperature -40.0 °C |
10.5 ft-lb/in² @Temperature -40.0 °F |
DIN 53453 |
Nilit FRIANYL A63 CV10 Nylon 6.6 for injection molding, 10% carbon fiber reinforced Nylon 6.6 for injection molding (good conductive and electrostatic properties).Information provided by Frisetta Polymer, which merged into Nilit Plastics |
|||
Charpy Impact Unnotched | 2.20 J/cm² @Temperature -40.0 °C |
10.5 ft-lb/in² @Temperature -40.0 °F |
DIN 53453 |
Nilit FRIANYL A63 CV-CU 0550 Nylon 6.6 for injection molding, 5% carbon fiber reinforced, 50% copper filled Nylon 6.6 for injection moldingInformation provided by Frisetta Polymer, which merged into Nilit Plastics |
|||
Charpy Impact Unnotched | 2.20 J/cm² - NB @Temperature -30.0 - -20.0 °C |
10.5 ft-lb/in² - NB @Temperature -22.0 - -4.00 °F |
Average value: 2.85 J/cm² Grade Count:56 |
Overview of materials for Polycarbonate/Polybutylene Terephthalate (PBT) Blend, Unreinforced This property data is a summary of similar materials in the MatWeb database for the category "Polycarbonate/Polybutylene Terephthalate (PBT) Blend, Unreinforced". Each property range of values repor.. |
|||
Charpy Impact Unnotched | 2.20 - 5.50 J/cm² @Temperature -30.0 - -30.0 °C |
10.5 - 26.2 ft-lb/in² @Temperature -22.0 - -22.0 °F |
Average value: 3.64 J/cm² Grade Count:5 |
Overview of materials for Polycarbonate/Polybutylene Terephthalate (PBT) Blend, Glass Filled This property data is a summary of similar materials in the MatWeb database for the category "Polycarbonate/Polybutylene Terephthalate (PBT) Blend, Glass Filled". Each property range of values repor.. |
|||
Charpy Impact Unnotched | 2.20 - 3.00 J/cm² @Temperature -30.0 - 30.0 °C |
10.5 - 14.3 ft-lb/in² @Temperature -22.0 - 86.0 °F |
Average value: 2.52 J/cm² Grade Count:6 |
Overview of materials for Liquid Crystal Polymer (LCP), 30% Glass Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Liquid Crystal Polymer (LCP), 30% Glass Fiber Filled". Specific grades with glass content between 25% an.. |
|||
Charpy Impact Unnotched | 2.20 - 9.00 J/cm² @Temperature -40.0 - -30.0 °C |
10.5 - 42.8 ft-lb/in² @Temperature -40.0 - -22.0 °F |
Average value: 4.59 J/cm² Grade Count:16 |
Overview of materials for Nylon 66, 10% Carbon Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66, 10% Carbon Fiber Filled". Specific grades with carbon fiber content between 5% and 14% are inc.. |
|||
Charpy Impact Unnotched | 2.20 J/cm² | 10.5 ft-lb/in² | flatwise; ISO 179 1fU |
Lehmann & Voss LUVOCOM® 1105-7760 PEEK, with carbon fiber, PTFE, lubricant modified, high viscosity Applications: Automotive industry, textile machinery, medical- and precision engineering, aircraft industry.Strong, stiff parts; low thermal coefficient of expansion.Dynamic stressed parts at high m.. |
|||
Charpy Impact Unnotched | 2.20 J/cm² | 10.5 ft-lb/in² | edgewise; ISO 179 1eU |
Lehmann & Voss LUVOCOM® 19-7816 Polyamide 46, with carbon fiber, lubricant modified Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.Improved friction and wear behaviour. Emergency running property.Strong, stiff parts.Electrical.. |
|||
Charpy Impact Unnotched | 2.20 J/cm² | 10.5 ft-lb/in² | edgewise; ISO 179 1eU |
Lehmann & Voss LUVOCOM® 20-8112 Polyphthalamide, with carbon fiber, lubricant modified Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.Strong, stiff parts.Dynamic stressed parts at high movement velocity.Improved friction and wear.. |
|||
Charpy Impact Unnotched | 2.20 J/cm² | 10.5 ft-lb/in² | ISO 179/1eU |
Lucite International Diakon® Frost 952 70 Acrylic Polymer Information provided by Lucite International |
|||
Charpy Impact Unnotched | 2.20 J/cm² | 10.5 ft-lb/in² | edgewise; ISO 179 1eU |
Lehmann & Voss LUVOCOM® 19-7745 Polyamide 46, with PTFE, improved wear resistance Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.Isotropic shrinkage characteristics.Good friction and wear behaviour especially at increased te.. |
|||
Charpy Impact Unnotched | 2.20 J/cm² @Temperature -30.0 °C |
10.5 ft-lb/in² @Temperature -22.0 °F |
ISO 179 |
Lehmann & Voss LUVOCOM® 50/GF/20/TF/20/BK 100 Polycarbonate, with glass fiber and PTFE Applications: Data processing machinery, precision engineering, film and photo industry, sporting and leisure goods, medical enineering.High-strength and high-stiff parts; low coefficient of expansi.. |
|||
Charpy Impact Unnotched | 2.20 J/cm² | 10.5 ft-lb/in² | Edgew 80*10*4 sp=62mm; ISO 179/1eU |
SABIC Innovative Plastics LNP STAT-KON EX03319C PEI (Asia Pacific) LNP* Stat-Kon* EX03319C is a polyetherimide compound reinforced with carbon fiber for good stiffness, dimension stability and has extremely high level of cleanliness for the most demanding applicati.. |
|||
Charpy Impact Unnotched | 2.20 J/cm² @Temperature -30.0 °C |
10.5 ft-lb/in² @Temperature -22.0 °F |
Edgew 80*10*4 sp=62mm; ISO 179/1eU |
SABIC Innovative Plastics Xenoy® 6370 PBT+PC (Europe-Africa-Middle East) XENOY 6370 is an impact modified semi-crystalline thermoplastic. blend with 30% glass fibre reinforcement offering toughness and ductility. |
|||
Charpy Impact Unnotched | 2.20 J/cm² | 10.5 ft-lb/in² | ISO 179-1 |
Unitika A1025GO PA6, Flame Retardant, Dry Information provided by Unitika Ltd. |
|||
Charpy Impact Unnotched | 2.20 J/cm² | 10.5 ft-lb/in² | Conditioned; ISO 179/IeU |
Addiplast Addilene H 490 M10F Flame Retardant Polypropylene, 10% Mineral Filled Flame retardant, mineral filled, with halogensInformation provided by Addiplast. |
|||
Charpy Impact Unnotched | 2.20 J/cm² | 10.5 ft-lb/in² | Conditioned; ISO 179/IeU |
Addiplast Addinyl B2H G30 Flame Retardant Nylon 6, 30% Glass Bead Flame retardant, 30% glass bead filled, with halogensInformation provided by Addiplast. |
|||
Charpy Impact Unnotched | 2.20 J/cm² | 10.5 ft-lb/in² | ISO 179/IeU |
Addiplast Addilene H 442 M30 Polypropylene Homopolymer High heat resistance, detergent stabilizedInformation provided by Addiplast. |
|||
Charpy Impact Unnotched | 2.20 - 3.50 J/cm² @Temperature -40.0 - -30.0 °C |
10.5 - 16.7 ft-lb/in² @Temperature -40.0 - -22.0 °F |
Average value: 2.85 J/cm² Grade Count:2 |
Overview of materials for Polyethylene Terephthalate (PET), Glass/Mineral Reinforced This property data is a summary of similar materials in the MatWeb database for the category "Polyethylene Terephthalate (PET), Glass/Mineral Reinforced". Each property range of values reported is m.. |
|||
Charpy Impact Unnotched | 2.20 J/cm² | 10.5 ft-lb/in² | ISO 179/1eU |
Lucite International Diakon® ST15G8 Toughened Acrylic Polymer The Diakon® impact PMMA series offer the best combination of impact, chemical and heat resistance and provide rigidity and surface hardness. The grades in the Diakon® series can be processed by in.. |
|||
Charpy Impact Unnotched | 2.20 - 1000 J/cm² | 10.5 - 4760 ft-lb/in² | Average value: 4.15 J/cm² Grade Count:7 |
Overview of materials for Polybutylene Terephthalate (PBT), Glass Filled, Impact Modified This property data is a summary of similar materials in the MatWeb database for the category "Polybutylene Terephthalate (PBT), Glass Filled, Impact Modified". Each property range of values reported.. |