Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Charpy Impact Unnotched | 5.50 J/cm² | 26.2 ft-lb/in² | DIN 53453 |
Nilit FRIANYL A63 GV35 Nylon 6.6 for injection molding, 35% glass fiber reinforced Nylon 6.6 for injection moldingInformation provided by Frisetta Polymer, which merged into Nilit Plastics |
|||
Charpy Impact Unnotched | 5.50 J/cm² | 26.2 ft-lb/in² | DIN 53453 |
Nilit FRIANYL B63 HS-GV15 Nylon 6 for injection molding, 15% glass fiber reinforced Nylon 6 for injection molding, high impact modified.Information provided by Frisetta Polymer, which merged into Nilit Plastics |
|||
Charpy Impact Unnotched | 5.50 J/cm² @Temperature 23.0 °C |
26.2 ft-lb/in² @Temperature 73.4 °F |
ISO 179/1eU |
PolyOne Bergamid™ A700 G25 HW UF Polyamide 66 (Nylon 66) Information provided by PolyOne |
|||
Charpy Impact Unnotched | 5.50 J/cm² | 26.2 ft-lb/in² | ISO 179 |
Shell Carilon® DB6F5G40 Polyketone, Flame-Retarded (V-0), 20% Glass-Reinforced Injection Molding Grade
(disco Shell announced in Feb. 2000 that the Carilon product line is being discontinued. CARILON Polymer DB6F5G40 is a flame-retarded, 20 percent glass-fiber-reinforced, injection molding grade with mecha.. |
|||
Charpy Impact Unnotched | 5.50 J/cm² | 26.2 ft-lb/in² | DIN 53453 |
Nilit FRIANYL B63 H-GV30 Nylon 6 for injection molding, 30% glass fiber reinforced Nylon 6 for injection molding, heat stabilized.Information provided by Frisetta Polymer, which merged into Nilit Plastics |
|||
Charpy Impact Unnotched | 5.50 J/cm² | 26.2 ft-lb/in² | DIN 53453 |
Nilit FRIANYL B63 HS-GV30 Nylon 6 for injection molding, 30% glass fiber reinforced Nylon 6 for injection molding, high impact modified.Information provided by Frisetta Polymer, which merged into Nilit Plastics |
|||
Charpy Impact Unnotched | 5.50 J/cm² | 26.2 ft-lb/in² | edgewise; ISO 179 1eU |
Lehmann & Voss LUVOCOM® 1105-8354 PEEK, with carbon fiber Applications: Automotive industry, textile machinery, medical- and precision engineering, aircraft industry.High-strength and high-stiff parts; low coefficient of expansion.Dynamic stressed parts at.. |
|||
Charpy Impact Unnotched | 5.50 J/cm² | 26.2 ft-lb/in² | edgewise; ISO 179 1eU |
Lehmann & Voss LUVOCOM® 19-7276 Polyamide 46, with carbon fiber and PTFE Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.High-strength and high-stiff parts; low coefficient of expansion.Reduced moment of inertia comp.. |
|||
Charpy Impact Unnotched | 5.50 J/cm² | 26.2 ft-lb/in² | edgewise; ISO 179 1eU |
Lehmann & Voss LUVOCOM® 20-7094 Polyphthalamide, with carbon fiber and PTFE Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.High-strength and high-stiff parts; low coefficient of expansion.Low influence from moisture an.. |
|||
Charpy Impact Unnotched | 5.50 J/cm² @Temperature 23.0 °C |
26.2 ft-lb/in² @Temperature 73.4 °F |
ISO 179/1eU |
Lanxess Pocan® T 3150 XF 000000 PBT + PET, 55% Glass Fiber PBT+PET, 55% glass fibers, injection molding, improved flowability, low tendency to warp, increased temperature peak load, increased strength and increased modulus |
|||
Charpy Impact Unnotched | 5.50 J/cm² | 26.2 ft-lb/in² | edgewise; ISO 179 1eU |
Lehmann & Voss LUVOCOM® 1105-8001 PEEK, with glass spheres Applications: Automotive industry, textile machinery, medical- and precision engineering, aircraft industry.Reduced moment of inertia compared with metal parts.Chemical and hydrolysis resistance par.. |
|||
Charpy Impact Unnotched | 5.50 J/cm² | 26.2 ft-lb/in² | ISO 179/2C |
SABIC Innovative Plastics Valox® 420 PBT (Europe-Africa-Middle East) VALOX 420 is a 30% glass fiber reinforced PBT injection moulding resin with excellent mechanical and thermal properties. Applications: appliance handles, spotlights, electric motors. |
|||
Charpy Impact Unnotched | 5.50 J/cm² | 26.2 ft-lb/in² | ISO 179/2C |
SABIC Innovative Plastics Valox® VX5022 PBT (Europe-Africa-Middle East) VALOX VX5022 is a 20% glass fibre reinforced PBT+PC blend with low warpage characteristics. This grade is 5021 with reduced warpage. |
|||
Charpy Impact Unnotched | 5.50 J/cm² | 26.2 ft-lb/in² | Injection Molded; ISO 179/1fU |
Styron DLGF9411.00 Polypropylene Overview: DLGF 9400.00 is a 40% long glass fiber reinforced grade with good flow properties. The glass fibers (12 mm length) are coupled to the polypropylene matrix resulting in high stiffness and s.. |
|||
Charpy Impact Unnotched | 5.50 J/cm² | 26.2 ft-lb/in² | ISO 179/1eU |
Solvay TECHNYL® A 218 MZ15 V 25 PA66, 25/15% glass/mineral fiber, Conditioned Description: TECHNYL® A 218 MZ15 V25 is a polyamide 66, reinforced with 25% of glass fiber and 15% of mineral filler, heat stabilized, for injection molding. This product is available in black co.. |
|||
Charpy Impact Unnotched | 5.50 J/cm² @Temperature -20.0 °C |
26.2 ft-lb/in² @Temperature -4.00 °F |
ISO 179/1eU |
Borealis Nepol™ GB402HP 40% Long Glass Fiber Reinforced Polypropylene Nepol GB402HP is a 40% long glass fiber reinforced polypropylene grade, produced using Borealis ` propriety and exclusive, patented Nepol technology intended for injection molding and extrusion. Th.. |
|||
Charpy Impact Unnotched | 5.50 J/cm² @Temperature -20.0 °C |
26.2 ft-lb/in² @Temperature -4.00 °F |
ISO 179/1eU |
Borealis Daplen™ EG102AI Polypropylene Compound 15% Mineral Filled Daplen EF102AI is a 15% mineral filled polypropylene compound intended injection molding. EG102AI is an easy flow grade, specially developed for the car industry. Daplen EF102AI has been developed.. |
|||
Charpy Impact Unnotched | 5.50 J/cm² @Temperature 30.0 °C |
26.2 ft-lb/in² @Temperature 86.0 °F |
conditioned; ISO 179/1eU |
EMS-Grivory Grivory® AS LF 20 PA66-Z20 Product description: Grilon AS LF 20 is a heat stabilized, normal viscosity PA 66 injection molding grade with 20% lubricant (PTFE + silicon oil). Grilon AS LF 20 has the following important propert.. |
|||
Charpy Impact Unnotched | 5.50 J/cm² @Temperature -30.0 °C |
26.2 ft-lb/in² @Temperature -22.0 °F |
ISO 179/1eU |
DuPont Performance Polymers Crastin® SK603 NC010 Polybutylene Terephthalate (PBT)
(Unverified Data**) 20% Glass Reinforced Polybutylene Terephthalate Crastin SK603 NC010 is a 20% glass fiber reinforced lubricated polybutylene terephthalate resin for injection molding.Information provided by DuPont P.. |
|||
Charpy Impact Unnotched | 5.50 J/cm² | 26.2 ft-lb/in² | 50%RH; ISO 179/1eU |
DuPont Performance Polymers Minlon® 10B140 NC010 Nylon 66
(Unverified Data**) 40% Mineral Reinforced Polyamide 66Minlon 10B140 NC010 is a 40% mineral reinforced polyamide 66 for injection molding. It has very low warpage.Information provided by DuPont Performance Polymers |
|||
Charpy Impact Unnotched | 5.50 J/cm² | 26.2 ft-lb/in² | conditioned; ISO 179/1eU |
EMS-Grivory Grivory® HT2C-3X black 9833 PA6T/66-CF30 Product description: Grivory HT2C-3X black 9833 us a 30% carbon-fiber reinforced engineering thermoplastic material based on a semi-crystalline, partially aromatic copolyamide. Acc to ISO: PA 6T/66... |
|||
Charpy Impact Unnotched | 5.50 J/cm² | 26.2 ft-lb/in² | dry; ISO 179/1eU |
EMS-Grivory Grivory® XE 4216 black 9233 PA6T/66-GF30 Product description: Grivory XE 4216 black 9233 is a high heat stabilized, 30% glass fiber reinforced, semicrystalline, thermoplastic engineering material for injection molding. Polymer designation .. |
|||
Charpy Impact Unnotched | 5.50 J/cm² | 26.2 ft-lb/in² | ISO 179/IeU |
Addiplast Addinyl A2 V30 Nylon 66, 30% Glass Filled Glass fiber reinforced, high strengthInformation provided by Addiplast. |
|||
Charpy Impact Unnotched | 5.50 J/cm² | 26.2 ft-lb/in² | |
BASF Procom® GC30S 401 Polypropylene Uses: Electrical appliance housings (e.g. drills), components requiring high impact and temperature resistance, furniture frames.Data was collected by ISO methods and provided by BASF. |
|||
Charpy Impact Unnotched | 5.50 J/cm² | 26.2 ft-lb/in² | ISO 179 |
BASF Ultramid® 1403-2 NF3001 13% Glass Filled PA66 (Dry) Ultramid 1403-2 NF3001 is a 13% glass reinforced, heat stabilized injection molding PA6/6. |
|||
Charpy Impact Unnotched | 5.50 J/cm² | 26.2 ft-lb/in² | Conditioned; ISO 179/IeU |
Addiplast Addinyl C2 V15 Nylon 66/6, 15% Glass Filled Glass fiber reinforced, high strengthInformation provided by Addiplast. |
|||
Charpy Impact Unnotched | 5.50 J/cm² @Temperature -30.0 °C |
26.2 ft-lb/in² @Temperature -22.0 °F |
50%RH; ISO 179/1eU |
DuPont Performance Polymers Zytel® 105F BK010 Nylon 66
(Unverified Data**) Unreinforced UV Stabilized Polyamide 66 Zytel 105F BK010 is a lubricated fast cycling weather resistant PA 66 resin. Zytel 105F BK010 contains finely dispersed carbon black.Information provided by D.. |