Mechanical Properties Metric English Comments
Flexural Yield Strength 82.0 MPa

@Temperature 163 °C
11900 psi

@Temperature 325 °F
Wet (Immersion at 170°F for 7 days)
Hexcel® HexPly® 954-2A Curing Cyanate Resin
HexPly® 954-2A is a 350°F (177°C) curing toughened cyanate resin with low moisture absorption, and excellent microcracking resistance. HexPly® 954-2A is formulated for autoclave or press molding..