Izod Impact, Unnotched 10.0 J/cm
18.7 ft-lb/in
ASTM D256
NYCOA 5033 HST 33% Glass-Fiber Reinforced, Heat Stabilized, Translucent Nylon 66 Resin
NYCOA 5033 HST is a 33% glass fiber reinforced, heat stabilized, translucent Nylon 66 resin used for injection molding. It has been specifically formulated for see through storage tanks for automoti..
Izod Impact, Unnotched 10.0 J/cm
18.7 ft-lb/in
ASTM D4812
Premix Premi-Glas® 1200-25 Fiberglass Reinforced Thermoset SMC
Premi-Glas® 1200-25 is a fiberglass reinforced thermoset sheet molding compound for general purpose applications requiring thermal stability and stiffness.Key features and benefits are:Excellent st..
Izod Impact, Unnotched 10.0 J/cm
18.7 ft-lb/in
ASTM D4812
Premix Premi-Glas® 1200H-25 Fiberglass Reinforced Thermoset SMC
Premi-Glas® 1200H-25 is a fiberglass reinforced thermoset sheet molding compound for general purpose and HVAC applications requiring thermal stability and stiffness.Key features and benefits are:Go..
Izod Impact, Unnotched 10.0 J/cm
18.7 ft-lb/in
ASTM D4812
Premix Premi-Glas® 1240-25 Fiberglass Reinforced Thermoset Thick Molding Compound
Premi-Glas® 1240-25 is a fiberglass reinforced thermoset Thick Molding Compound for general purpose applications requiring thermal stability and stiffness.Key features and benefits are:Excellent st..
Izod Impact, Unnotched 10.0 J/cm
18.7 ft-lb/in
ASTM D4812
Premix Premi-Glas® 2200-25 CR-SX Fiberglass Reinforced SMC
Description: Premi-Glas® 2200-25 CR-SX is a fiberglass reinforced thermoset Sheet Molding Compound formulated for excellent electrical properties and fire retardance; it also has very good thermal ..
Izod Impact, Unnotched 10.0 J/cm
18.7 ft-lb/in
ASTM D4812
Premix Premi-Glas® 2203-25 CR-SX Fiberglass Reinforced SMC
Description: Premi-Glas® 2203-25 CR-SX is a fiberglass reinforced thermoset Sheet Molding Compound formulated for excellent electrical properties and fire retardance; it also has very good thermal ..
Izod Impact, Unnotched 10.0 J/cm
18.7 ft-lb/in
ASTM D4812
Premix Premi-Glas® 2203-25 CR-SX-HT Fiberglass Reinforced Thermoset SMC
Premi-Glas® 2203-25 CR-SX-HT is a fiberglass reinforced thermoset sheet molding compound for electrical and flame retardant applications.Key features and benefits are:Enhanced product for higher UL..
Izod Impact, Unnotched 10.0 J/cm
18.7 ft-lb/in
ASTM D4812
Premix Premi-Glas® 2204-25 CR-SX Fiberglass Reinforced SMC
Description: Premi-Glas® 2204-25 CR-SX is a fiberglass reinforced thermoset Sheet Molding Compound formulated for excellent electrical properties and fire retardance; it also has very good thermal ..
Izod Impact, Unnotched 10.0 J/cm
18.7 ft-lb/in
ASTM D4812
Premix Premi-Glas® 2205-25 CR-SX Fiberglass Reinforced SMC
Description: Premi-Glas® 2205-25 CR-SX is a fiberglass reinforced thermoset Sheet Molding Compound formulated for excellent electrical properties and fire retardance; it also has very good thermal ..
Izod Impact, Unnotched 10.0 J/cm
18.7 ft-lb/in
ASTM D4812
Premix Premi-Glas® 2243-24 CR-SX Fiberglass Reinforced Thermoset Thick Molding Compound
Premi-Glas® 2243-24 CR-SX is a fiberglass reinforced thermoset thick molding compound for electrical and flame retardant applications.Key features and benefits are:TMC compounding process preserves..
Izod Impact, Unnotched 10.0 J/cm
18.7 ft-lb/in
ASTM D4812
Premix Premi-Glas® 3200-25 Fiberglass Reinforced SMC
Description: Premi-Glas® 3200-25 is a fiberglass reinforced thermoset Sheet Molding Compound formulated for excellent electrical properties and fire retardance; it also has very good thermal and di..
Izod Impact, Unnotched 10.0 J/cm
18.7 ft-lb/in
ASTM D4812
SABIC Innovative Plastics LNP LUBRICOMP SFP36 PA12
LNP* LUBRICOMP* SFP36 is a compound based on Nylon 12 resin containing 30% Glass Fiber 15% PTFE/Silicone. Added feature of this grade is: Wear Resistant.
Izod Impact, Unnotched 10.0 J/cm
18.7 ft-lb/in
ASTM D256
Solvay Specialty Polymers Amodel® AS-1133 HS Polyphthalamide (PPA), 33% Glass Fiber (Dry)
Amodel® AS-1133 HS is a 33% glass reinforced, heat stabilized polyphthalamide (PPA) resin that provides excellent structural integrity in molded parts, even those with wall thicknesses greater th..
Izod Impact, Unnotched 10.0 J/cm
18.7 ft-lb/in
ASTM D256
Solvay Specialty Polymers AvaSpire® AV-621 GF30 Polyaryletherketone (PAEK), 30% Glass Fiber
AvaSpire® AV-621 GF30 is a 30% glass fiber reinforced version of AvaSpire® AV-621. This formulation offers better dimensional stability and lower warpage than 30% glass reinforced PEEK. This r..
Izod Impact, Unnotched 10.0 J/cm
18.7 ft-lb/in
ASTM D256
Solvay Specialty Polymers KetaSpire® KT-820 GF13 Polyetheretherketone (PEEK), 13% Glass Fiber
KetaSpire® KT-820 is a low flow, 13% glass fiber reinforced grade of polyetheretherketone (PEEK). The glass fiber content is optimized to provide a balance of strength and stiffness with toughnes..
Izod Impact, Unnotched 10.0 J/cm
18.7 ft-lb/in
ASTM D256
Ineos Nova Zylar® 631 Clear Impact Modified Acrylic Copolymer  (discontinued **)
Features:Outstanding practical toughness and ductilityStyrenic processing advantagesExcellent property retention after ETO and gamma sterilizationUSP Class VI compliantCustom colors and enhancement ..
Izod Impact, Unnotched 10.0 J/cm
18.7 ft-lb/in
ASTM D4812
SABIC Innovative Plastics LNP THERMOCOMP RF007SXN PA 66
LNP* THERMOCOMP* RF007SXN is a Hydro-Stable, 35% Glass Fiber reinforced compound based on Nylon 66. Added features of this grade include: Heat Stabilized, NSF Listed.