Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Izod Impact, Unnotched | 6.94 J/cm @Thickness 3.17 mm |
13.0 ft-lb/in @Thickness 0.125 in |
ASTM D256 |
Niche Polymer PCM18BK PC Information provided by Niche Polymer |
|||
Izod Impact, Unnotched | 6.94 J/cm | 13.0 ft-lb/in | ASTM D256 |
Polymer Resources TPSF-GP1 PBT, 30% Glass Reinforced Structural Foam Grade Process: Foam MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples. Foam grades tested with foamed parts with a 10% weight reduction rel.. |
|||
Izod Impact, Unnotched | 6.94 J/cm @Thickness 3.18 mm |
13.0 ft-lb/in @Thickness 0.125 in |
ASTM D256 |
LNP Thermocomp® EF-1004 BK8-115 Polyetherimide, Glass Fiber Reinforcement
(discontinued **) Forms: PelletsProcessing Method: Injection MoldingInformation provided by LNP, a GE Plastics Company.This data sheet is labeled Discontinued; however many LNP grades are still active under new names.. |
|||
Izod Impact, Unnotched | 6.94 J/cm | 13.0 ft-lb/in | ASTM D4812 |
Solvay Specialty Polymers Supradel® HTS-2420 High Temperature Sulfone Resin
(discontinued **) SUPRADEL HTS-2420 is a 20% glass-fiber reinforced high-temperature, high-performance, amorphous, sulfone polymer. With a glass transition temperature of 245°C and a heat deflection temperature of 2.. |
|||
Izod Impact, Unnotched | 6.96 J/cm @Temperature 23.0 °C |
13.0 ft-lb/in @Temperature 73.4 °F |
ASTM D 4812 |
SABIC Innovative Plastics LNP Lubricomp ML002S PP LNP* Lubricomp* ML002S is a compound based on Polypropylene containing PTFE. Characteristics of this grade are: Heat Stabilized and Internally Lubricated.This data was supplied by SABIC-IP for the.. |
|||
Izod Impact, Unnotched | 6.94 J/cm @Thickness 3.17 mm |
13.0 ft-lb/in @Thickness 0.125 in |
ASTM D256 |
Techmer ES HiFill® HDPE GF25 CC 25% Glass Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 25% Filler by WeightFeatures: Chemically CoupledInformation provided by TP Composites, Inc. |
|||
Izod Impact, Unnotched | 6.94 J/cm | 13.0 ft-lb/in | ASTM D4812 |
A. Schulman POLYFLAM™ E-14526-31 30% Glass Reinforced Chemically Coupled Polypropylene DescriptionPolyfort® E-14526-31 is a 30% glass reinforced chemically coupled polypropylene black. Information provided by A. Schulman. |
|||
Izod Impact, Unnotched | 6.94 J/cm | 13.0 ft-lb/in | ASTM D256 |
Adell ZR-37 33% Glass Reinforced Nylon/Olefin Alloy Data provided by Adell Plastics, Inc. |
|||
Izod Impact, Unnotched | 6.94 J/cm | 13.0 ft-lb/in | ASTM D4812 |
Asahi Kasei Thermylene® P-20FG-1714 20% Glass Fiber Reinforced, Medium Impact Information provided by Asahi Thermofil |
|||
Izod Impact, Unnotched | 6.94 J/cm | 13.0 ft-lb/in | ASTM D4812 |
Asahi Kasei Thermylene® P6-30FG-0632 30% Glass Fiber Reinforced, Heat Stabilized Information provided by Asahi Thermofil |