Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Izod Impact, Unnotched | 8.52 J/cm | 16.0 ft-lb/in | ASTM D4812 |
SABIC Innovative Plastics Lexan® HFD4413 PC Lexan* HFD4413 is a 30% glass filled, injection moldable grade designed for high flow and superior surface appearance. Internal mold release. |
|||
Izod Impact, Unnotched | 8.54 J/cm @Thickness 3.17 mm |
16.0 ft-lb/in @Thickness 0.125 in |
ASTM D256 |
Techmer ES Luriblend® PA6/10 GF30 TS15 30% Glass Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber, 30% Filler by WeightAdditive: Heat Stabilizer and PTFE+ Silicone LubricantFeatures: Lubricated, Heat Stabilizer and Good W.. |
|||
Izod Impact, Unnotched | 8.54 J/cm @Thickness 3.17 mm |
16.0 ft-lb/in @Thickness 0.125 in |
ASTM D256 |
Techmer ES Luriblend® PP GF20 CC GL2 BK 20% Glass Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber, 20% Filler by WeightAdditive: Graphite Powder Lubricant(2%)Features: Chemically Coupled and LubricatedAppearance: BlackInf.. |
|||
Izod Impact, Unnotched | 8.54 J/cm | 16.0 ft-lb/in | ASTM D4812 |
SABIC Innovative Plastics LNP THERMOCOMP LF003 PEEK (Asia Pacific) LNP* Thermocomp* LF003 is a compound based on Polyetheretherketone resin containing Glass Fiber. |
|||
Izod Impact, Unnotched | 8.54 J/cm @Temperature 23.0 °C |
16.0 ft-lb/in @Temperature 73.4 °F |
ASTM D 4812 |
SABIC Innovative Plastics Ultem ATX153R PEI+PCE (Europe-Africa-Middle East) 30% Glass fiber filled, high flow Polyetherimide blend with internal mold release. ECO Conforming, UL94 V0 and 5VA listing.This data was supplied by SABIC-IP for the Europe-Africa-Middle East regio.. |
|||
Izod Impact, Unnotched | 8.54 J/cm | 16.0 ft-lb/in | ASTM D4812 |
SABIC Innovative Plastics LNP THERMOCOMP PF006S PA 6 LNP THERMOCOMP* PF006S is a compound based on Nylon 6 resin containing 30% Glass Fiber. Added features of this material include: Heat Stabilized. |
|||
Izod Impact, Unnotched | 8.54 J/cm | 16.0 ft-lb/in | ASTM D4812 |
SABIC Innovative Plastics LNP VERTON MX02795 PP LNP* VERTON* MX02795 is a compound based on Polypropylene resin containing Proprietary Fillers. Added features of this material include: Heat Stabilized, UV Stabilized, Structural. |
|||
Izod Impact, Unnotched | 8.55 J/cm | 16.0 ft-lb/in | ASTM D256A |
Total PPH 3925WZ Polypropylene, Injection Molding Grade Easy flow injection molding homopolymerNucleation - FINA 3925WZ is nucleated to provide fast cycle time and improve contact clarity.Antistat - FINA 3925WZ contains an antistat that will help protect.. |
|||
Izod Impact, Unnotched | 8.54 J/cm | 16.0 ft-lb/in | ASTM D4812 |
A. Schulman SCHULAMID® 6 GF15H 15% Glass Fiber Reinforced, Heat Impact Nylon 6 Information provided by A. Schulman. |
|||
Izod Impact, Unnotched | 8.54 J/cm | 16.0 ft-lb/in | ASTM D4812 |
A. Schulman SCHULAMID® 6 GF15H 15% Glass Fiber Reinforced, Heat Impact Nylon 6 Information provided by A. Schulman. |
|||
Izod Impact, Unnotched | 8.54 J/cm | 16.0 ft-lb/in | ASTM D4812 |
Asahi Kasei Thermylene® P6-30FG-0708 30% Glass Fiber Reinforced, High Impact Information provided by Asahi Thermofil |
|||
Izod Impact, Unnotched | 8.54 J/cm | 16.0 ft-lb/in | ASTM D4812 |
A. Schulman ComAlloy® E-14961 30% Glass Fiber Reinforced Polycarbonate Information provided by A. Schulman.The ComAlloy product line has been integrated into the A Schulman product line. |